Method of Recovering the Fibrous Fraction of Glass/Epoxy Composites
Source abstract
Abstract
This study reports the method of recovery of glass fibers from glass/epoxy composites through the solvent method. It is possible to decompose epoxy resin with a yield of more than 99 wt% soluble products in a nitric acid solution (8 M) at 90 C for 5 h. The decomposition rate of epoxy resin increases with an increase in temperature and concentration of acid solution. The glass fibers can be recovered with very little contamination and they have a tensile strength reduction of 3.5% under decomposition conditions of T = 70°C, t = 250 h, C = 6 M and α= 6 g/100 mL. These fibers can be used as reinforcement to prepare new composites. The interlaminar shear strength (ILSS) of recovered short fiber-reinforced composites produce strength reductions of only 2.5% compared with pristine composites.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Fiber-reinforced polymer composites · Mechanical Behavior of Composites · Natural Fiber Reinforced Composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Applied Chemistry Harbin Institute of Technology, Harbin 150001, P.R. China,
Department of Applied Chemistry Harbin Institute of Technology, Harbin 150001, P.R. China
References (11)
Show source-provided references
1. Ralph, J. · Plastics Engineering · 1991 · 47 · 13
2. 10.1016/S0011-2275(97)00127-610.1016/S0011-2275(97)00127-6 ↗
3. 10.1002/pc.1046810.1002/pc.10468 ↗
4. 10.1023/A:100432920962310.1023/A:1004329209623 ↗
5. 10.1002/app.1995.07057111610.1002/app.1995.070571116 ↗
6. 10.2472/jsms.44.42810.2472/jsms.44.428 ↗
7. 10.1016/S0165-2370(00)00122-410.1016/S0165-2370(00)00122-4 ↗
8. Jutte, R. B. · Plastics Engineering · 1991 · 47 · 13
9. 10.1002/app.2099010.1002/app.20990 ↗
10. 10.1016/S0266-3538(99)00154-210.1016/S0266-3538(99)00154-2 ↗
11. Liu, Y. Y. · Journal of Harbin Institute of Technology · 2005 · 37 · 470