journal article·2010-12

Investigation into the effect of drilling parameters on delamination in drilling GFRP

Erol Kilickap

Publisher page

Abstract

The purpose of this article is to investigate the influence of the cutting parameters, such as cutting speed and feed rate, and point angle on delamination and surface roughness produced when drilling a glass fiber-reinforced plastic composite. All tests were run without coolant at cutting speeds of 5, 10, 15, 20, and 25 m/min and feed rates of 0.1, 0.2, 0.3, and 0.4 mm/rev and point angle of 118° and 135°. The damage generated associated with drilling GFRP composites was observed, both at the entrance and the exit during the drilling process. It was observed that the delamination on drilled holes increased with increasing cutting speed and feed rate. The best results of the delamination are obtained at lower cutting speed and feed rates. For minimum damage on drilled holes, glass fiber-reinforced plastic composite must be drilled at a lower feed rate. It is shown that the point angle of drill is an important parameter on delamination and surface roughness.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced machining processes and optimization · Advanced Machining and Optimization Techniques · Erosion and Abrasive Machining

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering, Dicle University, Turkey,

References (21)

Show source-provided references
1. Wallenberger FT, Watson JC and Li H. Glass fibers. In: Miracle DB and Donaldson SL (eds) ASM handbook. Vol. 21, Composites, USA: ASM International, 2002, pp.27-34.10.31399/asm.hb.v21.a0003353 ↗
2. Blaga A. Glass fibre-reinforced polyester composites. http://irc.nrc-cnrc.gc.ca/pubs/cbd/cbd205_e.html , (2005, accessed November 2008), pp.1-6.
3. 10.1016/S0266-3538(01)00196-810.1016/S0266-3538(01)00196-8 ↗
4. 10.1016/j.ijmecsci.2007.01.00110.1016/j.ijmecsci.2007.01.001 ↗
5. 10.1016/j.jmatprotec.2004.04.17310.1016/j.jmatprotec.2004.04.173 ↗
6. 10.1016/j.compstruct.2005.09.03910.1016/j.compstruct.2005.09.039 ↗
7. 10.1016/j.msea.2007.03.02310.1016/j.msea.2007.03.023 ↗
8. 10.1016/S0263-8223(03)00180-610.1016/S0263-8223(03)00180-6 ↗
9. 10.1016/j.compositesa.2006.01.02010.1016/j.compositesa.2006.01.020 ↗
10. 10.1016/j.ijmachtools.2007.10.01510.1016/j.ijmachtools.2007.10.015 ↗
11. 10.1016/S0261-3069(03)00062-110.1016/S0261-3069(03)00062-1 ↗
12. 10.1016/S0924-0136(03)00812-410.1016/S0924-0136(03)00812-4 ↗
13. 10.1016/j.matdes.2007.01.01610.1016/j.matdes.2007.01.016 ↗
14. 10.1016/j.ijmachtools.2005.05.02310.1016/j.ijmachtools.2005.05.023 ↗
15. 10.1016/j.compstruct.2005.09.03910.1016/j.compstruct.2005.09.039 ↗
16. 10.1016/j.compscitech.2006.10.00910.1016/j.compscitech.2006.10.009 ↗
17. 10.1016/j.compscitech.2006.05.00310.1016/j.compscitech.2006.05.003 ↗
18. Marques AT
19. Altintas Y. · 2000
20. Trent EM · 1991
21. Field M. · 1999