Fatigue Crack Growth Behavior of Filament Wound Composite Pipes in Corrosive Environment
Source abstract
Abstract
The stress corrosion crack growth behavior of ±45°, ±55°, and ±75° filament wound composite pipes with surface crack subjected to 0.6 M HCl acid under alternating internal pressure was investigated. E-glass/epoxy pipes consist of six layers with stacking sequences of (+45/-45) 3 , (+55/-55) 3 , and (+75/-75) 3 . Dilute (0.6M) HCl acid was applied to the surface crack region by a corrosion cell mounted on the outer surface of the pipe. The specimens were tested at room temperature and exposed to open-ended fatigue tests in which the pipes can deform freely in the axial direction. The tests were performed in accordance with the ASTM D-2992 standard. The surface notches with different a/t and a/c forms were cut on the outer surface of the pipe parallel to the pipe axis. The internal pressure was generated by conventional hydraulic oil for fatigue loading. The low cycle tests were applied with 0.42 Hz frequency and R = 0.05 stress ratio. After the corrosion fatigue test, the fracture surfaces were examined and observed damage mechanisms discussed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Structural Integrity and Reliability Analysis · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Selçuk University, Department of Mechanical Engineering, 42075, Kampüs/Konya, Turkey,
Selçuk University, Department of Mechanical Engineering, 42075, Kampüs/Konya, Turkey
References (34)
Show source-provided references
1. 10.1016/S0266-3538(96)00158-310.1016/S0266-3538(96)00158-3 ↗
2. 10.1016/S1359-8368(00)00037-810.1016/S1359-8368(00)00037-8 ↗
3. 10.1016/S0266-3538(01)00084-710.1016/S0266-3538(01)00084-7 ↗
4. 10.1016/j.compscitech.2004.10.00210.1016/j.compscitech.2004.10.002 ↗
5. Samanci, A. · Composite Structures · 2007 · 8 · 207
6. 10.1016/j.compositesa.2006.04.01110.1016/j.compositesa.2006.04.011 ↗
7. Frost, S.R.
8. 10.1016/0956-7143(94)90058-210.1016/0956-7143(94)90058-2 ↗
9. Frost, S.R.
10. 10.1016/0266-3538(94)90029-910.1016/0266-3538(94)90029-9 ↗
11. 10.1016/S0266-3538(00)00215-310.1016/S0266-3538(00)00215-3 ↗
12. 10.1007/BF0102834010.1007/BF01028340 ↗
13. 10.1016/0010-4361(83)90014-910.1016/0010-4361(83)90014-9 ↗
14. 10.1007/BF0072147110.1007/BF00721471 ↗
15. 10.1016/0010-4361(84)90727-410.1016/0010-4361(84)90727-4 ↗
16. 10.1016/S0263-8223(01)00061-710.1016/S0263-8223(01)00061-7 ↗
17. 10.1016/0010-4361(80)90378-X10.1016/0010-4361(80)90378-X ↗
18. 10.1007/BF0055499610.1007/BF00554996 ↗
19. 10.1016/0266-3538(87)90002-910.1016/0266-3538(87)90002-9 ↗
20. 10.1016/S0266-3538(00)00244-X10.1016/S0266-3538(00)00244-X ↗
21. 10.1016/S1359-8368(00)00036-610.1016/S1359-8368(00)00036-6 ↗
22. Jones, F.R. · 1999
23. 10.1016/j.compscitech.2004.01.01710.1016/j.compscitech.2004.01.017 ↗
24. 10.1007/BF0058628910.1007/BF00586289 ↗
25. 10.1016/0010-4361(81)90498-510.1016/0010-4361(81)90498-5 ↗
26. Standard Practice for Obtaining Hydrostatic or Pressure Design Basis for ‘Fiberglass’ (Glass-Fiber-Reinforced Thermosetting Resin) Pipe and Fittings. American Society for Testing Materials (ASTM) Designation: D2992-91.
27. 10.1016/S0266-3538(01)00008-210.1016/S0266-3538(01)00008-2 ↗
28. Newman, J.C. · 1979
29. 10.1016/0266-3538(92)90087-J10.1016/0266-3538(92)90087-J ↗
30. 10.1016/B978-1-4832-8370-8.50049-810.1016/B978-1-4832-8370-8.50049-8 ↗
31. 10.1016/0010-4361(83)90141-610.1016/0010-4361(83)90141-6 ↗
32. 10.1179/mst.1985.1.3.17710.1179/mst.1985.1.3.177 ↗
33. 10.1179/msc.1980.14.8-9.44110.1179/msc.1980.14.8-9.441 ↗
34. Collins, H.H. · Materials and Applications · 1978 · 3 · 6