Influence of electrospun nanofibers on the interlaminar properties of unidirectional epoxy resin/glass fiber composite laminates
Source abstract
Abstract
Nylon 6,6 nanofibers were interleaved in the mid-plane of glass fiber/epoxy matrix composite laminates for Mode I and II fracture mechanic tests. The present study investigates the effect of the nanofibers on the laminates’ mechanical response. Results showed that Nylon 6,6 nanofibers improved specimen’s fracture mechanic behavior: the initial energy release rates G IC and G IIC increased 62% and 109%, respectively, when nanofibrous interlayer was used. Scanning electron microscope micrographs showed that nanofiber bridging mechanism enhances performances of the nanomodified specimens, still able to link the layers when the matrix is broken.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Fiber-reinforced polymer composites · Electrospun Nanofibers in Biomedical Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Industrial Engineering, University of Bologna, Bologna, Italy
Design, Manufacture, and Engineering Management Department, University of Strathclyde, Glasgow, UK
References (34)
Show source-provided references
1. Sridharan S · 2008
2. 10.1016/j.compscitech.2005.05.00810.1016/j.compscitech.2005.05.008 ↗
3. 10.1016/j.compscitech.2005.07.03810.1016/j.compscitech.2005.07.038 ↗
4. 10.1016/j.compscitech.2012.05.01210.1016/j.compscitech.2012.05.012 ↗
5. 10.1016/S0263-8223(98)00036-110.1016/S0263-8223(98)00036-1 ↗
6. 10.2514/3.1015210.2514/3.10152 ↗
7. 10.1016/S1359-835X(04)00180-010.1016/S1359-835X(04)00180-0 ↗
8. 10.1016/S0261-3069(00)00030-310.1016/S0261-3069(00)00030-3 ↗
9. 10.1002/pat.183710.1002/pat.1837 ↗
10. Dzenis YA and Reneker DH. Delamination resistant composites prepared by small diameter fiber reinforcement at ply interfaces. Patent US 6265333, USA, 2001.
11. 10.1016/j.compstruct.2011.08.01910.1016/j.compstruct.2011.08.019 ↗
12. 10.1016/j.msea.2006.07.06410.1016/j.msea.2006.07.064 ↗
13. 10.1007/BF0232005110.1007/BF02320051 ↗
14. 10.1016/j.ijsolstr.2005.05.01710.1016/j.ijsolstr.2005.05.017 ↗
15. 10.1016/j.compositesa.2006.05.00410.1016/j.compositesa.2006.05.004 ↗
16. Macander AB · ASTM STP · 1986 · 893 · 422
17. 10.1016/j.compscitech.2011.11.01010.1016/j.compscitech.2011.11.010 ↗
18. 10.1016/j.compositesb.2014.12.01510.1016/j.compositesb.2014.12.015 ↗
19. 10.1016/j.compscitech.2010.06.01910.1016/j.compscitech.2010.06.019 ↗
20. 10.1016/j.compscitech.2007.07.01010.1016/j.compscitech.2007.07.010 ↗
21. 10.3390/ma411196710.3390/ma4111967 ↗
22. 10.2514/1.4179110.2514/1.41791 ↗
23. 10.1002/pc.2264310.1002/pc.22643 ↗
24. 10.1016/j.compstruct.2013.07.02110.1016/j.compstruct.2013.07.021 ↗
25. 10.1016/j.compositesa.2005.09.01010.1016/j.compositesa.2005.09.010 ↗
26. 10.1016/j.compstruct.2013.10.03910.1016/j.compstruct.2013.10.039 ↗
27. Palazzetti R. Flexural behaviour of carbon and glass fiber composite laminates reinforced with nylon 6,6 electrospun nanofibers. J Comp Mater . Epub ahead of print. DOI: 10.1177/0021998314565410.10.1177/0021998314565410 ↗
28. Alessi S, Di Filippo M, Dispenza C, et al. Effects of nylon 6,6 nanofibrous mats on thermal properties and delamination behavior of high performance CFRP laminates. Polym Compos . Epub ahead of print 2014. DOI: 10.1002/pc.10.1002/pc.23035 ↗
29. ASTM D5528 2008. Standard test method for mode I interlaminar fracture toughness of unidirectional fiber-reinforced polymer matrix composites.
30. European Structural Integrity Society · 1993
31. ASTM D7264 2007. Standard test method for flexural properties of polymer matrix composite materials.
32. 10.1016/j.compscitech.2009.01.03410.1016/j.compscitech.2009.01.034 ↗
33. 10.1016/j.compositesb.2013.07.00410.1016/j.compositesb.2013.07.004 ↗
34. Giuliese G, Palazzetti R, Moroni F, et al. Cohesive zone modelling of delamination response of a composite laminate with interleaved nylon 6,6 nanofibers. Compos Part B 2015. Epub ahead of print. DOI: 10.1016/j.compositesb.2015.03.087.10.1016/j.compositesb.2015.03.087 ↗