Investigation of the mixed-mode delamination in polymer-matrix composites using acoustic emission technique
Source abstract
Abstract
This paper is a novel application of acoustic emission (AE) technique to investigate the actual occurring modes of delamination damage (i.e. mode I, mode II and the combination of these pure modes) in glass/epoxy composites. AE parameters and mechanical information associated with some novel methodologies were used to develop new AE-based approaches for studying delamination damage. The inter-laminar fracture energy for the initiation of delamination, Gc, was also measured using the novel introduced methods and standard methodologies. The results indicate that different interface lay-ups and different GII/GT modal ratio values indicate different AE signals and mechanical behaviors. Scanning electron microscope was also used to observe the induced damage mechanisms. It was found that the presented methods of employing AEs to characterize delamination damage and to obtain Gc were successful, especially in mode II and mixed-mode conditions where unstable crack growth and difficult crack growth monitoring prohibit a rigorous measurement of Gc. The results of this study could lead to improve automatic techniques for health monitoring of the real composite structures.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Mechanical Behavior of Composites · Ultrasonics and Acoustic Wave Propagation · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Non-destructive Testing Lab, Department of Mechanical Engineering, Amirkabir University of Technology, Tehran, Iran
References (27)
Show source-provided references
1. 10.1016/B0-08-042993-9/00073-510.1016/B0-08-042993-9/00073-5 ↗
2. Sridharan S · 2008
3. 10.1016/S0266-3538(98)00063-310.1016/S0266-3538(98)00063-3 ↗
4. 10.1533/9781845694821.2.21710.1533/9781845694821.2.217 ↗
5. 10.1016/j.compstruc.2007.02.01510.1016/j.compstruc.2007.02.015 ↗
6. Minak G · 2008 · 165
7. 10.1177/002199830934955310.1177/0021998309349553 ↗
8. Definitions of terms relating to acoustic emission. ASTM E610-98A, 1991.
9. 10.1002/pc.1021510.1002/pc.10215 ↗
10. 10.1016/S0266-3538(02)00087-810.1016/S0266-3538(02)00087-8 ↗
11. 10.1177/073168441141514010.1177/0731684411415140 ↗
12. 10.1016/j.matdes.2010.08.04810.1016/j.matdes.2010.08.048 ↗
13. 10.1115/1.150484810.1115/1.1504848 ↗
14. 10.1016/S0263-8223(99)00126-910.1016/S0263-8223(99)00126-9 ↗
15. 10.1016/j.compositesa.2006.04.01310.1016/j.compositesa.2006.04.013 ↗
16. 10.1016/0266-3538(94)90171-610.1016/0266-3538(94)90171-6 ↗
17. 10.1016/j.compositesa.2006.09.00110.1016/j.compositesa.2006.09.001 ↗
18. 10.1016/S0266-3538(02)00255-510.1016/S0266-3538(02)00255-5 ↗
19. 10.1016/j.compscitech.2006.03.03210.1016/j.compscitech.2006.03.032 ↗
20. 10.1177/073168441244225710.1177/0731684412442257 ↗
21. 10.1016/0266-3538(96)00005-X10.1016/0266-3538(96)00005-X ↗
22. 10.1177/147592171246999410.1177/1475921712469994 ↗
23. Ducept F, Gamby D and Davies P. A mixed-mode failure criterion derived from tests on symmetric and asymmetric specimens, Compos Sci Technol ; 59: 609–619.10.1016/S0266-3538(98)00105-5 ↗
24. Standard test method for mixed mode I–mode II interlaminar fracture toughness of unidirectional fiber reinforced polymer matrix composites. ASTM D 6671/D 6671M – 03, 2004.
25. 10.1016/S0008-6223(01)00021-510.1016/S0008-6223(01)00021-5 ↗
26. 10.1016/j.compscitech.2004.01.00810.1016/j.compscitech.2004.01.008 ↗
27. 10.1016/j.compositesb.2010.09.02110.1016/j.compositesb.2010.09.021 ↗