journal article·2011-07

Effects of types of fillers and filler loading on the properties of silicone rubber composites

S.M. Kong, M. Mariatti, J.J.C. Busfield

Publisher page

Abstract

In this study, the effects of loading levels of nano BN, nano SN and synthetic ND particles on the thermal and mechanical properties of silicone rubber were investigated. Nanoparticle-filled silicone rubber composites were prepared by cast molding process. In general, incorporation of thermally conductive nanoparticles to the silicone rubber matrix improved the thermal conductivity of the composites. BN particles have the most pronounced effect on the thermal conductivity in comparison to SN and ND particles at any given loading level. TGA studies revealed that the thermal stability of the SN/silicone rubber system increased as the filler loading level increased; however, BN and ND facilitated the thermal degradation of the silicone rubber nanocomposites. For tensile test, it is observed that the addition of nanoparticles generally increased the tensile strength of silicone rubber composites compared to the neat silicone rubber. However, for BN system, the tensile strength of the composites decreased when more than 1.5 vol.% of BN is loaded in the system. The reduction was caused by the existence of voids and agglomerations in the BN/silicone rubber system. In general, tensile modulus and strain at break of nanocomposites increased with the incorporation of nanoparticles into silicone rubber matrix.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Thermal properties of materials · High voltage insulation and dielectric phenomena · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials and Mineral Resources Engineering, Universiti Sains Malaysia, Penang, Malaysia.

Department of Materials, Queen Mary, University of London, London, United Kingdom.

References (24)

Show source-provided references
1. 10.1016/S0040-6031(02)00065-510.1016/S0040-6031(02)00065-5 ↗
2. 10.1016/j.carbon.2006.12.00710.1016/j.carbon.2006.12.007 ↗
3. 10.1016/S1359-4311(00)00034-X10.1016/S1359-4311(00)00034-X ↗
4. 10.1177/002199830708618410.1177/0021998307086184 ↗
5. 10.1002/pc.2029610.1002/pc.20296 ↗
6. 10.1016/j.tca.2004.12.02410.1016/j.tca.2004.12.024 ↗
7. 10.1002/pc.2027610.1002/pc.20276 ↗
8. 10.1002/polb.2151910.1002/polb.21519 ↗
9. 10.1016/S0026-2692(02)00191-X10.1016/S0026-2692(02)00191-X ↗
10. Noll W · 1968
11. Chojnowski J · 1993 · 193
12. Han Z, Wood JW, Herman H, Zhang C and Stevens GC. Thermal properties of composites filled with different fillers. In: IEEE International Symposium on Electrical Insulation, ISEI 2008 (Conference Record), Vancouver, BC, 9–12 June 2008, pp. 497–501.10.1109/ELINSL.2008.4570381 ↗
13. 10.1016/j.tca.2009.10.02010.1016/j.tca.2009.10.020 ↗
14. 10.1016/j.compositesa.2009.04.00510.1016/j.compositesa.2009.04.005 ↗
15. 10.1016/j.compscitech.2009.12.02310.1016/j.compscitech.2009.12.023 ↗
16. 10.1016/S1359-835X(01)00023-910.1016/S1359-835X(01)00023-9 ↗
17. Kochetov R, Andritsch A, Lafont U, Morshuis PHF, Picken SJ and Smit, JJ. Thermal behavior of epoxy resin filled with high thermal conductivity nanopowders. In: IEEE International Symposium on Electrical Insulation, ISEI 2009 (Conference Record), Montreal, QC, 31 May–3 June 2009, pp. 524–528.10.1109/EIC.2009.5166402 ↗
18. Liang Q, Xiu Y, Lin W, Moon KS and Wong CP. Epoxy/h-BN composites for thermally conductive underfill material. In: Electronic Components and Technology Conference, ECTC 2009 , San Diego, CA, 26–29 May 2009, pp. 437–440.10.1109/ECTC.2009.5074050 ↗
19. 10.1002/pc.2029610.1002/pc.20296 ↗
20. 10.1016/S0735-1933(98)00059-110.1016/S0735-1933(98)00059-1 ↗
21. 10.1016/j.tca.2010.02.00210.1016/j.tca.2010.02.002 ↗
22. 10.1016/j.polymdegradstab.2004.07.01110.1016/j.polymdegradstab.2004.07.011 ↗
23. 10.1007/s10854-009-9991-310.1007/s10854-009-9991-3 ↗
24. Farhang F · Iran Polym J · 2009 · 18 · 149