journal article·2006-01

Effect of Loading and Surface Modification of MWCNTs on the Fracture Behavior of Epoxy Nanocomposites

S. Ganguli, H. Aglan, P. Dennig, G. Irvin

Publisher page

Abstract

Nanocomposites consisting of multiwalled carbon nanotubes (MWCNTs) and a bifunctional epoxy resin are manufactured by a unique dispersion technique. The effect of loading and surface modification of the MWCNTs on the mechanical properties and fracture behavior of the nanocomposites is studied. Both a scanning electron microscope (SEM) and an atomic force microscope (AFM) are used to identify the mechanisms by which the nanocomposites acquired their fracture resistance. At 0.1 wt% loading, both ball-milled and acid-treated MWCNT composites perform better than the neat resin. An increase of 40% in the fracture toughness has been achieved at 0.15 wt% loading with ball-milled MWCNTs. An increase of 80% in the fracture toughness has been achieved at 0.15 wt% loading in the acid-treated MWCNT nanocomposites. The AFM images of the MWCNT nanocomposites reveal that the MWCNTs are well dispersed in both the systems. A better dispersion of MWCNTs has been achieved with acid treatment than with ball milling. The SEM images of the fractured surfaces reveal a tremendous increase in the number of fracture surface features associated with the acid-treated MWCNT nanocomposites, in comparison with the ball-milled MWCNT nanocomposites and the neat resin.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Carbon Nanotubes in Composites · Polymer Nanocomposites and Properties · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering, Tuskegee University, Tuskegee, AL 36088, USA

Department of Mechanical Engineering, Tuskegee University, Tuskegee, AL 36088, USA,

Ahwahnee Technology, Inc., San Jose, CA 95138, USA

Eastman Kodak Company, Rochester, NY 14650, USA

References (23)

Show source-provided references
1. 10.1177/009524430504592710.1177/0095244305045927 ↗
2. 10.1016/j.cossms.2003.10.00610.1016/j.cossms.2003.10.006 ↗
3. 10.1016/S1359-835X(03)00140-410.1016/S1359-835X(03)00140-4 ↗
4. 10.1016/S0008-6223(03)00034-410.1016/S0008-6223(03)00034-4 ↗
5. 10.1016/j.carbon.2004.07.03010.1016/j.carbon.2004.07.030 ↗
6. 10.1016/j.compscitech.2004.02.00410.1016/j.compscitech.2004.02.004 ↗
7. 10.1016/j.compscitech.2004.01.02310.1016/j.compscitech.2004.01.023 ↗
8. 10.1016/S0969-806X(01)00422-410.1016/S0969-806X(01)00422-4 ↗
9. 10.1016/S0379-6779(98)01067-410.1016/S0379-6779(98)01067-4 ↗
10. 10.1016/j.polymer.2004.10.06810.1016/j.polymer.2004.10.068 ↗
11. 10.1016/S0009-2614(02)00948-X10.1016/S0009-2614(02)00948-X ↗
12. 10.1016/j.compscitech.2004.01.02410.1016/j.compscitech.2004.01.024 ↗
13. 10.1016/j.compscitech.2004.04.00210.1016/j.compscitech.2004.04.002 ↗
14. 10.1016/S0039-6028(02)02532-310.1016/S0039-6028(02)02532-3 ↗
15. 10.1016/j.carbon.2003.12.01210.1016/j.carbon.2003.12.012 ↗
16. 10.1016/j.carbon.2003.12.04310.1016/j.carbon.2003.12.043 ↗
17. 10.1016/j.carbon.2004.02.03210.1016/j.carbon.2004.02.032 ↗
18. 10.1016/S0925-9635(03)00185-710.1016/S0925-9635(03)00185-7 ↗
19. 10.1016/S1369-7021(04)00507-310.1016/S1369-7021(04)00507-3 ↗
20. 10.1016/S0266-3538(03)00059-910.1016/S0266-3538(03)00059-9 ↗
21. 10.1016/S0921-5093(04)00857-310.1016/S0921-5093(04)00857-3 ↗
22. 10.1063/1.161337410.1063/1.1613374 ↗
23. Murakami, Y. · 1987