Performance and operando failure analysis of laser-perforated Li–Cu reference electrodes in lithium-ion pouch cells
Source abstract
Abstract
The potential of reference electrodes in future-oriented battery technologies relies critically on their design optimization. Previous studies show that locating reference electrodes within the effective stack region, while maintaining a minimally invasive geometry, is essential for precise and artifact-free electrochemical sensing. Here, we fabricated a highly porous (93%) microscale Li–Cu reference electrode by in-situ Li deposition on a laser-perforated Cu substrate. Since Li reference electrodes remain intrinsically unstable, we implemented a three-stage workflow to evaluate their performance and failure behavior. First, galvanostatic deposition of 0.5 mAh cm −2 Li delivered a stable reference potential for over 3000 h. A subsequent parametric study showed that Li stability depends on both deposition parameters and operating conditions. Accelerated failure during operation was linked to active Li consumption into inactive species, as revealed by coupled thickness–potential monitoring and supported by complementary analyses. Finally, benchmark testing confirmed that the perforated design enables reliable potential tracking with negligible blocking effects under the investigated conditions, supporting diagnostic measurements such as differential analysis and EIS. This work advances the understanding of Li-based reference electrodes and highlights perforated designs as a promising strategy for reliable sensing in battery systems.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Handling complexity in virtual battery development with a simplified systems modeling approach10.3390/wevj15110525 ↗
2. Kampker · 2024
3. Enabling battery digital twins at the industrial scale10.1016/j.joule.2023.05.005 ↗
4. Wassiliadis · 2024
5. Degradation mechanisms and mitigation strategies of nickel-rich NMC-based lithium-ion batteries10.1007/s41918-019-00053-3 ↗
6. A review of degradation mechanisms and recent achievements for Ni-rich cathode-based Li-ion batteries10.1002/aenm.202103005 ↗
7. Li plating as unwanted side reaction in commercial Li-ion cells–A review10.1016/j.jpowsour.2018.02.063 ↗
8. On the correlation between surface chemistry and performance of graphite negative electrodes for li ion batteries10.1016/S0013-4686(99)00194-2 ↗
9. How fast can a Li-ion battery be charged? Determination of limiting fast charging conditions10.1021/acsaem.0c03114 ↗
10. Lithium plating at the cell edge induced by anode overhang during cycling in lithium-ion batteries: Part II. Simulation and experimental validation10.1149/1945-7111/ad9a02 ↗
11. Modeling electrochemical transport within a three-electrode system10.1149/1945-7111/abdafb ↗
12. A versatile reference electrode for lithium ion battery use10.1149/1945-7111/ada7a4 ↗
13. Online adaptive anode potential-controlled fast charging of lithium-ion cells using a validated electrochemical model-based virtual reference electrode10.1016/j.jpowsour.2024.234620 ↗
14. Modeling losses in a three electrode system towards fast charge control10.1149/1945-7111/adca5b ↗
15. Method—deconvoluting losses in lithium-ion batteries via a versatile reference electrode10.1149/1945-7111/ad9a03 ↗
16. 4-electrode full cells for operando Li+ activity measurements and prevention of Li deposition in Li-ion cells10.1149/1945-7111/ab8976 ↗
17. A control-oriented electrochemical model for lithium-ion battery. Part II: Parameter identification based on reference electrode10.1016/j.est.2019.101101 ↗
18. Determination of electrolyte transport properties with a multi-reference-electrode cell10.1149/1945-7111/ac03f1 ↗
19. Design and demonstration of three-electrode pouch cells for lithium-ion batteries10.1149/2.0031709jes ↗
20. Investigation of different locations for reference electrodes inside lithium-ion pouch cells10.1016/j.jpowsour.2023.233986 ↗
21. Critical review of the use of reference electrodes in li-ion batteries: a diagnostic perspective10.3390/batteries5010012 ↗
22. Multi-reference electrode lithium-ion pouch cell design for spatially resolved half-cell potential and impedance measurements10.1149/1945-7111/ad048d ↗
23. Enhancing precision and durability of built-in Cu-Li reference electrodes in lithium-ion batteries: A critical review10.1021/acsenergylett.4c02431 ↗
24. A toolbox of reference electrodes for lithium batteries10.1002/adfm.202108449 ↗
25. Zhou · 2007
26. Structural vulnerability control by encapsulation strategy toward durable lithium metal reference electrodes10.1002/aenm.202304502 ↗
27. Testing lithium-ion battery with the internal reference electrode: an insight into the blocking effect10.1149/2.0141814jes ↗
28. Errors in the reference electrode measurements in real lithium-ion batteries10.1016/j.jpowsour.2020.228933 ↗
29. Electrode behavior RE-visited: monitoring potential windows, capacity loss, and impedance changes in Li1.03(Ni0.5Co0.2Mn0.3)0.97O2/silicon-graphite full cells10.1149/2.0271606jes ↗
30. Fast charging of li-ion cells: Part I. Using Li/Cu reference electrodes to probe individual electrode potentials10.1149/2.0401906jes ↗
31. Three-electrode setups for lithium-ion batteries10.1149/2.0241702jes ↗
32. Three-electrode setups for lithium-ion batteries10.1149/2.0231702jes ↗
33. Development of reliable lithium microreference electrodes for long-term in situ studies of lithium-based battery systems10.1149/1.1813652 ↗
34. Application of a lithium–tin reference electrode to determine electrode contributions to impedance rise in high-power lithium-ion cells10.1016/j.electacta.2004.05.040 ↗
35. A reference electrode for in situ impedance measurements in sodium-ion batteries10.1149/2.0741915jes ↗
36. A gold micro-reference electrode for impedance and potential measurements in lithium ion batteries10.1149/2.0581610jes ↗
37. Development of a wire reference electrode for lithium all-solid-state batteries with polymer electrolyte: FEM simulation and experiment10.1149/2.0671807jes ↗
38. Reliable reference electrodes for lithium-ion batteries10.1016/j.elecom.2013.03.015 ↗
39. Designing a reference electrode – An approach to fabricate laser perforated reference electrodes for lithium-ion batteries10.1016/j.electacta.2022.141768 ↗
40. Performance of Li4Ti5O12-based reference electrode for the electrochemical analysis of all-solid-state lithium-ion batteries10.1016/j.elecom.2020.106743 ↗
41. A simple formula describing impedance artifacts due to the size and surface resistance of a reference-electrode wire in a thin-film cell10.1149/2.1121702jes ↗
42. Smart cells - battery monitoring via internal sensors
43. Distributed reference electrode for lithium plating detection and fast charging optimization in lithium-ion batteries
44. An experimental method to determine the measurement error of reference electrodes within lithium-ion batteries10.1002/celc.202300216 ↗
45. Application of perforated reference electrodes in small cell formats for rate tests and electrochemical impedance spectroscopy10.1002/ente.202300278 ↗
46. Investigation of expansion and potential of si-dominant anodes with binder modification in full cells10.1016/j.jpowsour.2025.237620 ↗
47. Li-growth and SEI engineering for anode-free Li-metal rechargeable batteries: A review of current advances10.1016/j.ensm.2023.02.036 ↗
48. “Dead lithium” formation and mitigation strategies in anode-free Li-metal batteries10.1002/batt.202400505 ↗
49. Lithium metal anodes: Advancing our mechanistic understanding of cycling phenomena in liquid and solid electrolytes10.1021/jacs.3c05715 ↗
50. Interaction of invasive reference electrodes with lithium-ion pouch cells
51. New eddy-current sensor setup for high-resolution lithium-ion cell dilation measurements10.1109/JSEN.2023.3290349 ↗
52. Spatially resolved degradation and inhomogeneity analysis of lithium-ion pouch cells using an array of eddy-current sensors10.1016/j.est.2024.110740 ↗
53. Comparative in-operando analysis of lithium-ion cell swelling in pouch cells: Constant force versus foam-buffered quasi-constant force10.1016/j.est.2026.121124 ↗
54. Lithium metal anodes: Advancing our mechanistic understanding of cycling phenomena in liquid and solid electrolytes10.1021/jacs.3c05715 ↗
55. Galvanic corrosion of lithium-powder-based electrodes
56. Noninvasive in situ NMR study of “dead lithium” formation and lithium corrosion in full-cell lithium metal batteries10.1021/jacs.0c10258 ↗
57. Toward safe lithium metal anode in rechargeable batteries: a review10.1021/acs.chemrev.7b00115 ↗
58. Recent advances in understanding dendrite growth on alkali metal anodes10.1016/j.enchem.2019.100003 ↗
59. Nucleation and early stage growth of Li electrodeposits10.1021/acs.nanolett.9b03548 ↗
60. Revisiting the electroplating process for lithium-metal anodes for lithium-metal batteries10.1002/anie.201912217 ↗
61. Nanoscale nucleation and growth of electrodeposited lithium metal10.1021/acs.nanolett.6b04755 ↗
62. Principles of crystal nucleation and growth10.2113/0540057 ↗
63. Corner-, edge-, and facet-controlled growth of nanocrystals10.1126/sciadv.abf1410 ↗
64. In situ analysis of Li plating and stripping behaviors under dynamic current conditions for realistic application scenarios10.1002/advs.202414396 ↗
65. Decoupling accurate electrochemical behaviors for high-capacity electrodes via reviving three-electrode vehicles10.1002/aenm.202204077 ↗
66. Modeling the SEI-formation on graphite electrodes in LiFePO4 batteries10.1149/2.0161506jes ↗
67. Connecting the irreversible capacity loss in Li-ion batteries with the electronic insulating properties of solid electrolyte interphase (SEI) components10.1016/j.jpowsour.2016.01.078 ↗
68. Dynamic spatial progression of isolated lithium during battery operations10.1038/s41586-021-04168-w ↗
69. Impact of size and position of lithium metal reference electrodes on the measurement of lithium-plating overpotential10.1149/1945-7111/ac2469 ↗
70. The success story of graphite as a lithium-ion anode material–fundamentals, remaining challenges, and recent developments including silicon (oxide) composites10.1039/D0SE00175A ↗