Improving critical current density and cycling stability of NaSICON solid electrolytes by powder aerosol deposited CuO interlayers
Source abstract
Abstract
Solid-solid interfacial instabilities remain major obstacles for the industrialization of cost-effective, high energy density solid-state sodium batteries (SSSB). In this work, a conversion-type CuO interlayer was successfully deposited onto both sides of Na 3 Zr 2 Si 2 PO 12 (NZSP) solid electrolyte (SE) discs by powder aerosol deposition (PAD) to enhance the interfacial compatibility between sodium metal and SE. While unmodified symmetric cells suffer from progressive interfacial degradation, and limited critical current density, incorporating PAD-CuO interlayers on NZSP SE discs significantly reduces interfacial resistance and increases the critical current density up to 5.0 mA cm −2 . This value is further increased to 7.4 mA cm −2 by thermal post-treatment. Long-term galvanostatic cycling demonstrates stabilized overvoltages during plating/stripping experiments, indicating progressive interphase activation and improved Na + transport. Overall, these results demonstrate that PAD enables the fabrication of functional interlayers for stabilizing the Na|NZSP interface and may provide a foundation for fully PAD-processed scalable architectures in next-generation SSSBs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Sodium and sodium-ion energy storage batteries10.1016/j.cossms.2012.04.002 ↗
2. Survey of the transport properties of sodium superionic conductor materials for use in sodium batteries10.1016/j.jpowsour.2014.09.137 ↗
3. Crystal structures and crystal chemistry in the system Na1+xZr2SixP3−xO1210.1016/0025-5408(76)90073-8 ↗
4. Na3Zr2Si2PO12: a stable Na+-Ion solid electrolyte for solid-state batteries10.1021/acsaem.0c00820 ↗
5. Graphene regulated ceramic electrolyte for solid-state sodium metal battery with superior electrochemical stability10.1021/acsami.8b19519 ↗
6. Guided-formation of a favorable interface for stabilizing Na metal solid-state batteries10.1039/D0TA01498B ↗
7. Uniform Na metal plating/stripping design for highly reversible solid-state Na metal batteries at room temperature10.1002/smll.202204487 ↗
8. Atomically bonding Na anodes with metallized ceramic electrolytes by ultrasound welding for high‐energy/power solid‐state sodium metal batteries10.1002/cey2.299 ↗
9. Interfacial reactivity benchmarking of the sodium ion conductors Na3PS4 and sodium β-Alumina for protected sodium metal anodes and sodium all-solid-state batteries10.1021/acsami.6b10119 ↗
10. Interface issues and challenges for NASICON-based solid-state sodium-metal batteries
11. Interfaces in solid-state sodium-ion batteries: NaCoO2 thin films on solid electrolyte substrates10.1016/j.electacta.2018.02.109 ↗
12. Solid-state sodium batteries10.1002/aenm.201703012 ↗
13. Enhancing ion transport and suppressing electron conduction: a hybrid interlayer for stable garnet‐based solid‐state batteries10.1002/adfm.202426002 ↗
14. Improving Na/Na3Zr2Si2PO12 interface via SnOx/Sn film for high-performance solid-state sodium metal batteries10.1002/smtd.202100339 ↗
15. Evaluating electrolyte-anode interface stability in sodium all-solid-state batteries10.1021/acsami.2c12759 ↗
16. A series of hybrid multifunctional interfaces as artificial SEI layer for realizing dendrite free, and long‐life sodium metal anodes
17. Sodium–gallium alloy layer for fast and reversible sodium deposition10.1002/sus2.97 ↗
18. Protective NaSICON interlayer between a sodium-tin alloy anode and sulfide-based solid electrolytes for all-solid-state sodium batteries10.1021/acsami.3c09256 ↗
19. Stabilizing Li1.3Al0.3Ti1.7(PO4)3 |Li metal anode interface in solid‐state batteries by kevlar aramid nanofiber‐based protective coating10.1002/adfm.202306748 ↗
20. Status and prospects of hydroborate electrolytes for all-solid-state batteries10.1016/j.ensm.2019.08.032 ↗
21. Na‐K interlayer driven Na‐NASICON solid‐state batteries
22. Atomic layer deposition derived zirconia coatings on Ni‐rich cathodes in solid‐state batteries: correlation between surface constitution and cycling performance10.1002/smsc.202200073 ↗
23. Stabilizing the interface of NASICON solid electrolyte against Li metal with atomic layer deposition10.1021/acsami.8b06366 ↗
24. Physical vapor deposition in solid-state battery development: from materials to devices10.1002/advs.202002044 ↗
25. Advances in ceramic thin films fabricated by pulsed laser deposition for intermediate-temperature solid oxide fuel cells10.1021/acs.energyfuels.0c02338 ↗
26. The effect of polished surface microstructure of ceramic electrolyte on solid-state sodium metal batteries10.1016/j.ceramint.2023.08.195 ↗
27. Improving the alkali metal electrode/inorganic solid electrolyte contact via room-temperature ultrasound solid welding10.1038/s41467-021-27473-4 ↗
28. Aerosol deposition of ceramic thick films at room temperature: densification mechanism of ceramic layers10.1111/j.1551-2916.2006.01030.x ↗
29. Room temperature fabrication of Binder‐free Na3V2(PO4)3/C high‐loading electrode films via the powder aerosol deposition method10.1002/batt.202500902 ↗
30. Aerosol deposition method for fabrication of nano crystal ceramic layer10.4028/www.scientific.net/MSF.449-452.43 ↗
31. An overview of the aerosol deposition method: process fundamentals and new trends in materials applications
32. Powder aerosol deposition as a method to produce garnet‐type solid ceramic electrolytes: a study on electrochemical film properties and industrial applications10.1002/ente.202100211 ↗
33. Room temperature manufacture of dense NaSICON solid electrolyte films for all-solid-state-sodium batteries10.1007/s10853-023-08642-w ↗
34. Stabilizing Na3Zr2Si2PO12/Na interfacial performance by introducing a clean and Na-Deficient surface10.1021/acs.chemmater.0c00474 ↗
35. Stability of NASICON materials against water and CO2 uptake10.1016/j.ssi.2016.11.006 ↗
36. What happens during thermal post-treatment of powder aerosol deposited functional ceramic films? Explanations based on an experiment-enhanced literature survey10.1002/adma.201908104 ↗
37. Toward robust ionic conductivity determination of sulfide‐based solid electrolytes for solid‐state batteries
38. Exploring the origin of ZrO2 phase in Na3Zr2Si2PO12 ceramic electrolyte10.1016/j.ceramint.2022.11.084 ↗
39. Solid-state synthesis of NASICON (Na3Zr2Si2PO12) using nanoparticle precursors for optimisation of ionic conductivity10.1007/s10853-019-04162-8 ↗
40. Reaction of NASICON with water10.1016/S0167-2738(01)00683-X ↗
41. Improving ionic conductivity of von-alpen-type NASICON ceramic electrolytes via magnesium doping10.26599/JAC.2023.9220738 ↗
42. Electrochemical impedance spectroscopy for all‐solid‐state batteries: theory, methods and future outlook10.1002/celc.202100108 ↗
43. Analyzing void formation and rewetting of thin in situ-formed Li anodes on LLZO10.1016/j.joule.2022.09.009 ↗
44. Toward a fundamental understanding of the lithium metal anode in solid-state Batteries-An Electrochemo-Mechanical study on the garnet-type solid electrolyte Li6.25Al0.25La3Zr2O1210.1021/acsami.9b02537 ↗
45. Evaluating the use of critical current density tests of symmetric lithium transference cells with solid electrolytes10.1002/aenm.202302383 ↗
46. Critical current density in solid‐state lithium metal batteries: mechanism, influences, and strategies
47. Recent advances in electrochemical impedance spectroscopy for solid-state batteries
48. Semi-solid alkali metal electrodes enabling high critical current densities in solid electrolyte batteries10.1038/s41560-021-00786-w ↗
49. Interfacial chemistry in solid-state batteries: formation of interphase and its consequences10.1021/jacs.7b09531 ↗
50. Growth process of α-Al2O3 ceramic films on metal substrates fabricated at room temperature by aerosol deposition10.1111/j.1551-2916.2011.04493.x ↗
51. How to treat powders for the room temperature aerosol deposition method to avoid porous, low strength ceramic films10.1016/j.jeurceramsoc.2018.08.008 ↗
52. Intermediate Cu-O-Si phase in the Cu-SiO2/Si(111) system: growth, elemental, and electrical studies10.1021/acsomega.1c02646 ↗
53. Peak-fitting of Cu 2p photoemission spectra in Cu0, Cu1+, and Cu2+ oxides: a method for discriminating Cu0 from Cu1+10.1016/j.apsusc.2023.156960 ↗
54. Electrochemical impedance Spectroscopy-A tutorial10.1021/acsmeasuresciau.2c00070 ↗
55. Electrochemical impedance spectroscopy of metal oxide electrodes for energy applications10.1021/acsaem.9b01965 ↗
56. Critical stripping current leads to dendrite formation on plating in lithium anode solid electrolyte cells10.1038/s41563-019-0438-9 ↗
57. A review of the features and analyses of the solid electrolyte interphase in Li-ion batteries10.1016/j.electacta.2010.05.072 ↗
58. The fast charge transfer kinetics of the lithium metal anode on the garnet‐type solid electrolyte Li6.25Al0.25La3Zr2O1210.1002/aenm.202000945 ↗
59. SnF2 ‐induced highly current‐tolerant solid electrolytes for solid‐state sodium batteries
60. Symmetric cells as an analytical tool for battery research: Assembly, operation, and data analysis strategies10.1149/1945-7111/acaf42 ↗