Local impact of cell degradation on transport and structural properties in the cathode catalyst layer of a polymer electrolyte membrane fuel cell
Source abstract
Abstract
Fuel cells can be a solution for carbon-free transport, but are affected by high price and limited lifetime. Material level degradation mechanisms are understood but structure changes require more analysis. This study investigates the degradation impact on material, transport and structural properties in the cathode catalyst layer. A 500 h AST using automotive load cycle and conditions (80 °C, 2.5/2.3 bar abs , 50%/30% relative humidity, 1.3/1.5 stoichiometry at anode and cathode) is applied and alterations of these properties are discussed. Whilst the membrane's influence appears to be minor, Pt/C degradation mainly caused the performance decay on the material level (−37% active area). The structural analysis revealed local pore size reduction and a 0.6 μm thick layer at the interface cathode catalyst layer (CCL)/membrane with collapsed porosity. Besides carbon and catalyst degradation, ionomer migration within the catalyst layer during wet/dry cycles cause the pores to fill with ionomer. The local ionomer concentration increased more at humid conditions at air outlet (+59%) and results in decreased proton transport resistance (−38%) and increased oxygen transport resistance (+10%). Consequently, this work reveals that the ionomer macroscopically migrates into the CCL pores during fuel cell operation and this represents an important additional degradation mechanism.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Membrane-based Ion Separation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. PEM fuel cell applications in road transport10.3390/en16176129 ↗
2. D. Hart, S. Jones, X. Cordobes, G. Bates, J. Lewis. The fuel cell industry review 2022. The ERM International Group Limited. https://www.erm.com/contentassets/55c43361e857413387f28fbacea6e91a/the-fuel-cell-industry-review-2022.pdf.
3. Technical and commercial challenges of proton-exchange membrane (PEM) fuel cells10.3390/en14010144 ↗
4. Thompson · Nat. Catal. · 2019 · 2 · 55810.1038/s41929-019-0291-x ↗
5. The catalyst layer and its dimensionality – a look into its ingredients and how to characterize their effects10.1016/j.jpowsour.2016.01.091 ↗
6. Degradation mechanisms of proton exchange membrane fuel cell under typical automotive operating conditions10.1016/j.pecs.2020.100859 ↗
7. Review on mechanisms and recovery procedures for reversible performance losses in polymer electrolyte membrane fuel cells10.1016/j.jpowsour.2020.229375 ↗
8. The challenges in reliable determination of degradation rates and lifetime in polymer electrolyte membrane fuel cells
9. Structure, property, and performance of catalyst layers in proton exchange membrane fuel cells10.1007/s41918-022-00175-1 ↗
10. A comprehensive review of PEMFC durability in dynamic operation: critical stressors, degradation analysis, and lifetime prognostics
11. A review of platinum-based catalyst layer degradation in proton exchange membrane fuel cells10.1016/j.jpowsour.2009.06.073 ↗
12. On/off cycling test of low-temperature PEM fuel cell at fully humidified conditions10.1080/15435075.2019.1671394 ↗
13. Experimental observations of microstructure changes in the catalyst layers of proton exchange membrane fuel cells under wet-dry cycles10.1149/2.0391806jes ↗
14. Tracking the evolution of mechanical degradation in fuel cell membranes using 4D in situ visualization10.1016/j.jpowsour.2018.11.049 ↗
15. Membrane and active layer degradation upon PEMFC steady-state operation10.1149/1.2775218 ↗
16. Microscopic investigation of platinum deposition in PEMFC cross-sections using AFM and SEM10.1149/2.130306jes ↗
17. R.L. Borup, A. Kusoglu, K.C. Neyerlin, R. Mukundan, R.K. Ahluwalia, D.A. Cullen, K.L. More, A.Z. Weber, D.J. Myers; Recent developments in catalyst-related PEM fuel cell durability; Curr. Opin. Electrochem. 21 (2020) 192-200; https://doi.org/10.1016/j.coelec.2020.02.007.10.1016/j.coelec.2020.02.007 ↗
18. Effect of carbon corrosion on wettability of PEM fuel cell electrodes10.1149/2.0231912jes ↗
19. Local impact of load cycling on degradation in polymer electrolyte fuel cells10.1016/j.apenergy.2019.114210 ↗
20. Insights into degradation of the membrane–electrode assembly performance in low-temperature PEMFC: the catalyst, the ionomer, or the interface?10.1021/acsami.2c12327 ↗
21. Quantitative in situ analysis of ionomer structure in fuel cell catalytic layers10.1021/acsami.6b07188 ↗
22. High-resolution analysis of ionomer loss in catalytic layers after operation10.1149/2.0151806jes ↗
23. An epoxy-free sample preparation approach to enable imaging of ionomer and carbon in polymer electrolyte membrane fuel cells10.1002/adfm.202209733 ↗
24. Electrochemical characterization of evolving ionomer/electrocatalyst interactions throughout accelerated stress tests10.1016/j.jpowsour.2022.232490 ↗
25. Tracking the evolution of ionomer film and catalyst material to unravel PEMFC performance degradation10.1149/1945-7111/ada111 ↗
26. Quantification and evolution on degradation mechanisms of proton exchange membrane fuel cell catalyst layer under dynamic testing conditions10.1016/j.ijhydene.2023.01.109 ↗
27. Quantification on degradation mechanisms of polymer exchange membrane fuel cell cathode catalyst layers during bus and stationary durability test protocols10.1016/j.jpowsour.2021.230878 ↗
28. Degradation behavior of ionomer in the cathode catalyst layer of polymer electrolyte fuel cells10.1016/j.apenergy.2025.125759 ↗
29. Ionomer migration within PEMFC catalyst layers induced by humidity changes10.1016/j.elecom.2019.106590 ↗
30. EU harmonised test protocols for PEMFC MEA testing in single cell configuration for automotive applications
31. Evaluation of reversible and irreversible degradation rates of polymer electrolyte membrane fuel cells tested in automotive conditions10.1016/j.jpowsour.2016.07.049 ↗
32. Corrosion of carbon supports at cathode during hydrogen/air replacement at anode studied by visualization of oxygen partial pressures in a PEFC—Start-up/shut-down simulation10.1016/j.jpowsour.2010.11.092 ↗
33. Characterization of ionic conductivity profiles within proton exchange membrane fuel cell gas diffusion electrodes by impedance spectroscopy10.1149/1.1390804 ↗
34. Ionic conductivity of PEMFC electrodes: effect of nafion loading10.1149/1.1611493 ↗
35. Chapter “Preparation and Characterization of Highly Dispersed Electrocatalytic Materials”
36. Electrocatalytic oxidation of methanol on platinum nanoparticles electrodeposited onto porous carbon substrates10.1023/A:1018434609543 ↗
37. Insight into carbon corrosion of different carbon supports for Pt-based electrocatalysts using accelerated stress tests in polymer electrolyte fuel cells10.1016/j.jpowsour.2022.232209 ↗
38. Characterizing the structural degradation in a PEMFC cathode catalyst layer: carbon corrosion10.1149/1.3139963 ↗
39. Analysis of polarization curves to evaluate polarization sources in hydrogen/air PEM fuel cells10.1149/1.1860034 ↗
40. Local impact of load cycling on degradation in polymer electrolyte fuel cells10.1016/j.apenergy.2019.114210 ↗
41. Physical modeling of catalyst degradation in low temperature fuel cells: platinum oxidation, dissolution, particle growth and platinum band formation
42. Impact of gas partial pressure on PEMFC chemical degradation10.1149/1.2356171 ↗
43. Electro-osmotic drag coefficient and proton conductivity in nafion membrane for PEMFC10.1016/j.ijhydene.2009.09.013 ↗
44. Modification, degradation, and mitigation of perfluorosulfonic acid proton exchange membranes for fuel cells: a review10.1021/acsami.5c02335 ↗
45. Research on the mechanisms of contact resistance and structural deformation impact on PEMFC performance10.1016/j.csite.2025.106845 ↗
46. Hydrogen oxidation artifact during platinum oxide reduction in cyclic voltammetry analysis of low-loaded PEMFC electrodes10.1007/s12678-020-00627-6 ↗
47. Analysis and modeling of PEMFC degradation: effect on oxygen transport10.1016/j.jpowsour.2012.04.069 ↗
48. An in situ technique for analyzing ionomer coverage in catalyst layers10.1016/j.jelechem.2013.01.026 ↗
49. A review of PEM fuel cell durability: materials degradation, local heterogeneities of aging and possible mitigation strategies10.1002/wene.113 ↗
50. PEMFC catalyst layers: the role of micropores and mesopores on water sorption and fuel cell activity10.1021/am200590w ↗
51. Effect of operating conditions on carbon corrosion in polymer electrolyte membrane fuel cells10.1016/j.jpowsour.2009.04.006 ↗
52. PEM fuel cell start-up/shut-down losses vs relative humidity: the impact of water in the electrode layer on carbon corrosion10.1149/2.0931816jes ↗
53. Nafion structural phenomena at platinum and carbon interfaces10.1021/ja9033928 ↗
54. A systematic approach for matching simulated and experimental polarization curves for a PEM fuel cell10.1016/j.ijhydene.2019.11.057 ↗