Abstract

Cathode particle fracture is widely recognised as a major degradation mechanism in lithium-ion batteries, yet cracking also permits electrolyte wetting of newly exposed internal surfaces, modifying interfacial reaction pathways. The mechanistic role of electrolyte wetting in redistributing reactions within cracked particles remains unclear. Here, we isolate this effect through a controlled comparison between (i) a fully coupled electro-chemo-mechanical model resolving lithium concentration, electrostatic potential, and stress fields in both the active material and the electrolyte inside and outside cracks, and (ii) a single-particle chemo-mechanical model employing the conventional uniform flux assumption. The coupled model predicts strong spatial heterogeneity in interfacial reaction rates, with flux amplification approximately 8×relative to the imposed uniform flux at the crack tip. Reaction redistribution, and thus lithium flux, is governed predominantly by local solid-state lithium concentration and stress variations, while electrolyte potential gradients inside cracks remain secondary under the conditions considered. Uniform flux models can underpredict delivered capacity by 25% at 1C-rate; this discrepancy increases at higher rates. They also underestimate tensile stresses throughout the delithiation process by 10%, directly affecting crack driving conditions. These results demonstrate that neglecting crack–electrolyte coupling leads to systematic underestimation of both utilisation limits and fatigue-relevant stress histories.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advanced battery technologies research · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Low-carbon technologies in automotive industry and decarbonizing transport10.1016/j.jpowsour.2023.233888 ↗
2. Comparison of the structural and electrochemical properties of layered Li[NixCoyMnz]O2 (x=1/3, 0.5, 0.6, 0.7, 0.8 and 0.85) Cathode material for Lithium-Ion batteries10.1016/j.jpowsour.2013.01.063 ↗
3. A review on the key issues of the lithium ion battery degradation among the whole life cycle10.1016/j.etran.2019.100005 ↗
4. Degradation mechanism of Ni-Enriched NCA cathode for lithium batteries: Are microcracks really critical?10.1021/acsenergylett.9b00733 ↗
5. Anisotropic lattice strain and mechanical degradation of high- and low-nickel NCM cathode materials for Li-Ion batteries10.1021/acs.jpcc.6b12885 ↗
6. Intergranular cracking as a major cause of Long-Term capacity fading of layered cathodes10.1021/acs.nanolett.7b00379 ↗
7. Chemistry–mechanics–geometry coupling in positive electrode materials: a scale-bridging perspective for mitigating degradation in lithium-ion batteries through materials design10.1039/D2SC04157J ↗
8. Capacity fading of Ni-Rich Li[Nix Coy Mn1−−x−−y ]O2 (0.6 ≤x ≤ 0.95) cathodes for high-energy-density Lithium-Ion batteries: Bulk or surface degradation?10.1021/acs.chemmater.7b05269 ↗
9. Capacity fading of Ni-Rich NCA cathodes: Effect of microcracking extent10.1021/acsenergylett.9b02302 ↗
10. The genesis and control of microcracks in nickel-rich cathode materials for lithium-ion batteries10.1039/D3SE00844D ↗
11. Microstructural observation of LiNi0.8 Co0.15 Al0.05 O2 after charge and discharge by scanning transmission electron microscopy10.1149/2.073207jes ↗
12. Computational modeling of Li-ion batteries10.1007/s00466-016-1325-8 ↗
13. A review on modeling of electro-chemo-mechanics in lithium-ion batteries10.1016/j.jpowsour.2018.12.011 ↗
14. Review on the numerical modeling of fracture in active materials for lithium ion batteries10.1016/j.jpowsour.2023.232875 ↗
15. Modeling crack growth during Li extraction in storage particles using a fracture phase field approach10.1149/2.0281602jes ↗
16. Modeling crack growth during Li insertion in storage particles using a fracture phase field approach10.1016/j.jmps.2016.04.004 ↗
17. Quantifying the influence of charge rate and cathode-particle architectures on degradation of Li-ion cells through 3D continuum-level damage models10.1016/j.jpowsour.2021.230415 ↗
18. A chemo-mechanical damage model at large deformation: numerical and experimental studies on polycrystalline energy materials10.1016/j.ijsolstr.2021.111099 ↗
19. Modeling coupled Chemo-Mechanical behavior of randomly oriented NMC811 polycrystalline Li-Ion battery cathodes10.1149/1945-7111/ac1811 ↗
20. Chemo-mechanical modeling of inter- and intra-granular fracture in heterogeneous cathode with polycrystalline particles for lithium-ion battery10.1016/j.jmps.2022.104839 ↗
21. A coupled phase field formulation for modelling fatigue cracking in lithium-ion battery electrode particles10.1016/j.jpowsour.2022.231805 ↗
22. Cracking and associated volumetric expansion of NMC811 secondary particles10.1016/j.jpowsour.2023.233745 ↗
23. A cohesive phase-field fracture model for chemo-mechanical environments: Studies on degradation in battery materials10.1016/j.tafmec.2023.103758 ↗
24. Direct observations of electrochemically induced intergranular cracking in polycrystalline NMC811 particles10.1039/D3TA03057A ↗
25. Electro-chemo-mechanical finite-element model of single-crystal and polycrystalline NMC cathode particles embedded in an argyrodite solid electrolyte10.1016/j.electacta.2023.142585 ↗
26. Microstructure impact on chemo-mechanical fracture of polycrystalline lithium-ion battery cathode materials10.1016/j.engfracmech.2024.110370 ↗
27. Multiscale electro-chemo-mechanical model of high-capacity amorphous silicon anode material in sodium-ion batteries
28. Chemomechanical interplay of layered cathode materials undergoing fast charging in lithium batteries10.1016/j.nanoen.2018.09.051 ↗
29. Influence of NCM particle cracking on kinetics of Lithium-Ion batteries with liquid or solid electrolyte10.1149/1945-7111/ab9a2c ↗
30. Polycrystalline and single crystalline NCM cathode materials—Quantifying particle cracking, active surface area, and lithium diffusion10.1002/aenm.202003400 ↗
31. Deciphering the interplay between wetting and Chemo-Mechanical fracture in Lithium-Ion battery cathode materials
32. Computational modeling of coupled mechanical damage and electrochemistry in ternary oxide composite electrodes10.1016/j.jpowsour.2023.234034 ↗
33. A phase field-based framework for electro-chemo-mechanical fracture: Crack-contained electrolytes, chemical reactions and stabilisation10.1016/j.cma.2023.116235 ↗
34. Electro-chemo-mechanical phase field modeling of localized corrosion: theory and COMSOL implementation10.1007/s00366-023-01833-8 ↗
35. A microstructure-sensitive electro-chemo-mechanical phase-field model of pitting and stress corrosion cracking10.1016/j.corsci.2024.112031 ↗
36. Improved cycling stability of Li[Ni0.90 Co0.05 Mn0.05 ]O2 through microstructure modification by boron doping for Li-Ion batteries10.1002/aenm.201801202 ↗
37. Simulation and optimization of the dual lithium ion insertion cell10.1149/1.2054684 ↗
38. Mechanical and structural degradation of LiNi x Mn y Co z O 2 cathode in Li-Ion batteries: An experimental study10.1149/2.1751713jes ↗
39. Heterogeneous damage in Li-ion batteries: Experimental analysis and theoretical modeling10.1016/j.jmps.2019.05.003 ↗
40. Cracking predictions of lithium-ion battery electrodes by X-ray computed tomography and modelling10.1016/j.jpowsour.2022.231119 ↗
41. Stoichiometrically driven disorder and local diffusion in NMC cathodes10.1039/D1TA01639C ↗
42. A shrinking-core model for the degradation of high-nickel cathodes (NMC811) in Li-Ion batteries: Passivation layer growth and oxygen evolution10.1149/1945-7111/abdc71 ↗
43. Influence of concentration-dependent material properties on the fracture and debonding of electrode particles with core–shell structure10.1016/j.jpowsour.2024.234395 ↗
44. Transport properties of LiPF6-Based Li-Ion battery electrolytes
45. Computational modeling of heterogeneity of stress, charge, and cyclic damage in composite electrodes of Li-Ion batteries10.1149/1945-7111/ab78fa ↗
46. A highly stabilized Ni-rich NCA cathode for high-energy lithium-ion batteries10.1016/j.mattod.2020.01.019 ↗
47. Ni–Li anti-site defect induced intragranular cracking in Ni-rich layer-structured cathode10.1016/j.nanoen.2020.105021 ↗
48. Capacity fading mechanisms in Ni-Rich single-crystal NCM cathodes10.1021/acsenergylett.1c01089 ↗
49. Surface spinel reconstruction to suppress detrimental phase transition for stable LiNi0, 8Co0. 1Mn0. 1O2 cathodes10.1007/s12274-022-4754-z ↗
50. Chemo-mechanical analysis of lithiation/delithiation of Ni-rich single crystals10.1149/1945-7111/acd47e ↗
51. Electrolytes and interphases in li-ion batteries and beyond10.1021/cr500003w ↗