S. Möller, Axel Durdel, Luiza Streck, K.F. Muzakka, M. Finsterbusch

Abstract

Si-based anodes for Li-ion batteries improve battery performance, but introduce new fatigue mechanisms, reducing their cycle-life, compared to graphite anodes. Four 110 × 80 mm 2 electrodes of a 5.4 Ah NCA + Si/G cell after 340 cycles are analysed by ion-beam analysis in 345,000 points, providing a unique insight into the degradation of the Si-anode. Our results show an inhomogeneous state-of-charge (SoC) across the electrodes and Li immobilization at the Si-anode. After the initial formation cycling, the anode contains 10.2 atom% Li (SoC = 0), after 340 cycles this amount increases to 17.5 at.%. The F and P concentrations show most Li is immobilized as LiF. Li-silicates are only a minor fraction of the solid-electrolyte interphase, ruling them out as main driver of the accelerated degradation. The immobilized anode Li results in a cathode Li concentration drop from initially 21 at.% (SoC = 0) to 16 at.% Li after 340 cycles. This Li-loss correlates well with the aging related electrode-potential shift of 130 mV known from literature. A ±6% cathode layer thicknesses inhomogeneity is revealed through the areal density of Ni. The Li loss requires 480 mAh/g Si pre-lithiation for compensating the observed Li-immobilization, which would increase cycle-life and the initial discharge capacity.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Electron Microscopy Techniques and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Degradation diagnostics for lithium ion cells10.1016/j.jpowsour.2016.12.011 ↗
2. Recent progress and future perspective on practical silicon anode-based lithium ion batteries10.1016/j.ensm.2022.01.042 ↗
3. Calendar aging of silicon-containing batteries10.1038/s41560-021-00883-w ↗
4. Evolution and expansion of Li concentration gradient during charge–discharge cycling10.1038/s41467-021-24120-w ↗
5. A review of the state of health for lithium-ion batteries: research status and suggestions10.1016/j.jclepro.2020.120813 ↗
6. State-of-the-art characterization techniques for advanced lithium-ion batteries10.1038/nenergy.2017.11 ↗
7. Fast charging of lithium-ion batteries: a review of materials aspects10.1002/aenm.202101126 ↗
8. High capacity garnet-based all-solid-state lithium batteries: fabrication and 3D-Microstructure resolved modeling10.1021/acsami.8b06705 ↗
9. Significance of direct observation of lithium-ion distribution and potential distribution inside batteries through operando analyses10.1016/j.nxener.2024.100106 ↗
10. Direct visualization of the solid electrolyte interphase and its effects on silicon electrochemical performance10.1002/admi.201600438 ↗
11. Ionic conductivity and mechanical properties of the solid electrolyte interphase in lithium metal batteries
12. Characterization of stable solid electrolyte lithium silicate for thin film lithium battery10.1143/JPSJS.79SA.98 ↗
13. Effect of mechanical pressure on lifetime, expansion, and porosity of silicon-dominant anodes in laboratory lithium-ion cells10.1149/1945-7111/ad36e6 ↗
14. Morphological changes of silicon nanoparticles and the influence of cutoff potentials in silicon-graphite electrodes10.1149/2.1261807jes ↗
15. A new high-throughput focused MeV ion-beam analysis setup10.3390/instruments5010010 ↗
16. Differential cross-section measurements for the 7Li(p,p0)7Li, 7Li(p,p1)7Li, 7Li(p,α0)4He, 19F(p,p0)19F, 19F(p,α0)16O and 19F(p,α1,2)16O reactions10.1016/j.nimb.2012.07.020 ↗
17. SRIM – the stopping and range of ions in matter (2010)10.1016/j.nimb.2010.02.091 ↗
18. Analysis of Rutherford backscattering spectra with CNN-GRU mixture density network10.1038/s41598-024-67629-y ↗
19. The Guelph PIXE software package V10.1016/j.nimb.2021.05.004 ↗
20. Absolute local quantification of Li as function of state-of-charge in all-solid-state Li batteries via 2D MeV ion-beam analysis10.3390/batteries7020041 ↗
21. Silicon-Dominant anodes based on microscale silicon particles under partial lithiation with high capacity and cycle stability10.1149/2.1311915jes ↗
22. Modeling silicon-dominant anodes: parametrization, discussion, and validation of a newman-type model10.3390/batteries9110558 ↗
23. Perspective—Structure and stability of the solid electrolyte interphase on silicon anodes of lithium-ion batteries10.1149/1945-7111/abe984 ↗
24. MeV Ion beam analysis of granite in 10000 points
25. 3 MeV Proton Ion beam analysis of NCA/Si anode-cathode mapping
26. Silicon Solid Electrolyte Interphase (SEI) of lithium ion battery characterized by microscopy and spectroscopy10.1021/jp404155y ↗
27. Liquid electrolyte chemistries for solid electrolyte interphase construction on silicon and lithium-metal anodes10.1039/D3SC03514J ↗
28. Investigation of the Solid Electrolyte Interphase Formed by Fluoroethylene Carbonate on Si Electrodes10.1149/1.3589300 ↗
29. ‘Analysis of transient current and heat flow during voltage holds: for 70 wt% silicon anode lithium-ion cells - IOPscience’. Accessed: October. 20, 2025. [Online]. Available: https://iopscience.iop.org/article/10.1149/1945-7111/ad940e.
30. Improved performance of the silicon anode for Li-Ion batteries: understanding the surface modification mechanism of fluoroethylene carbonate as an effective electrolyte additive10.1021/acs.chemmater.5b00339 ↗
31. Depletion of electrolyte salt upon calendaric aging of lithium-ion batteries and its effect on cell performance10.1149/1945-7111/ad4821 ↗
32. Improving cycle life of silicon-dominant anodes based on microscale silicon particles under partial lithiation10.3390/batteries9010058 ↗