Comparative analysis of current- and potential-controlled accelerated stress tests for Pt/C catalyst layers in a gas diffusion electrode (GDE) setup
Source abstract
Abstract
Accelerated stress tests (ASTs) are widely used to assess the durability of Pt/C oxygen reduction reaction (ORR) catalysts for polymer electrolyte membrane fuel cells (PEMFCs). While conventionally potential-controlled protocols are applied to ensure comparability, degradation is a potential-driven process, such protocols are less realistic to “real world scenarios” than current-controlled protocols. In this work, we compare potential- and current-controlled ASTs in a pressurized gas diffusion electrode (GDE) half-cell. Using Pt nanoparticles supported on highly porous ENSACO 350P carbon, we compare the influence of the two different AST approaches under otherwise identical conditions. While both protocols induce comparable losses in electrochemically active surface area (ECSA), only the current-controlled AST reveals an abrupt performance collapse associated with impaired water removal following carbon degradation. Under fixed-current conditions, transient flooding triggers sharp voltage drops and severe power losses, effects largely masked under potential control due to self-limiting reduction in water production. These findings demonstrate that current-controlled ASTs can provide mechanistic insight into the interplay between carbon degradation and water management and offer a practical, application-relevant complement to conventional potential-controlled testing for PEMFC catalyst layers. • Direct comparison of ASTs reveals distinct catalyst degradation behaviors. • Current-controlled AST exposes electrode flooding driven by carbon degradation. • Carbon corrosion under current control links directly to water management. • Current-controlled ASTs may guide strategies for water-management optimization.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Nanopore and Nanochannel Transport Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Recent developments in catalyst-related PEM fuel cell durability10.1016/j.coelec.2020.02.007 ↗
2. A review of PEM fuel cell durability: degradation mechanisms and mitigation strategies10.1016/j.jpowsour.2008.06.006 ↗
3. Scientific aspects of polymer electrolyte fuel cell durability and degradation10.1021/cr050182l ↗
4. Review: durability and degradation issues of PEM fuel cell components10.1002/fuce.200700053 ↗
5. PEM fuel cell electrocatalyst durability measurements10.1016/j.jpowsour.2006.03.009 ↗
6. A review of accelerated stress tests of MEA durability in PEM fuel cells10.1016/j.ijhydene.2008.10.012 ↗
7. Recent advances in catalyst accelerated stress tests for polymer electrolyte membrane fuel cells10.1149/2.0881807jes ↗
8. Empirical modeling of cathode electrode durability in polymer electrolyte fuel cells
9. Study of the degradation mechanisms of carbon-supported platinum fuel cells catalyst via different accelerated stress test10.1016/j.jpowsour.2014.09.012 ↗
10. Improved accelerated stress tests for ORR catalysts using a rotating disk electrode10.1149/2.0161907jes ↗
11. Accelerated life tests for fuel cells
12. Fuel cell catalyst degradation on the nanoscale10.1016/j.elecom.2008.05.032 ↗
13. Membrane and catalyst performance targets for automotive fuel cells by FCCJ membrane, catalyst, MEA WG
14. Challenges and limitations of accelerated stress testing in GDE half-cell set-ups
15. On the need of improved accelerated degradation protocols (ADPs): examination of platinum dissolution and carbon corrosion in half-cell tests10.1149/2.0731614jes ↗
16. Investigation of the corrosion of carbon supports in polymer electrolyte fuel cells using simulated start-up/shutdown cycling10.1016/j.electacta.2012.12.082 ↗
17. Testing fuel cell catalysts under more realistic reaction conditions: accelerated stress tests in a gas diffusion electrode setup
18. Benchmarking high surface area electrocatalysts in a gas diffusion electrode: measurement of oxygen reduction activities under realistic conditions10.1039/C8EE00019K ↗
19. Key considerations for high current fuel cell catalyst testing in an electrochemical half-cell10.1149/2.0891704jes ↗
20. Gas diffusion electrode setup for catalyst testing in concentrated phosphoric acid at elevated temperatures10.1063/1.4908169 ↗
21. Degradation mechanisms of Pt/C fuel cell catalysts under simulated start-stop conditions10.1021/cs300024h ↗
22. PtCo cathode catalyst morphological and compositional changes after PEM fuel cell accelerated stress testing10.1149/2.0091806jes ↗
23. Machine learning modeling for fuel cell-battery hybrid power system dynamics in a Toyota Mirai 2 vehicle under various drive cycles
24. Comparing load-cycling degradation tests in a PEM fuel cell short-stack to single-cell voltage-cycling accelerated stress tests10.1149/MA2025-02412022mtgabs ↗
25. Development of accelerated durability Test protocols for polymer electrolyte membrane fuel cell stacks under realistic operating conditions10.1002/fuce.202300263 ↗
26. A review of water flooding issues in the proton exchange membrane fuel cell10.1016/j.jpowsour.2007.12.068 ↗
27. A review on experimental evaluation of water management in a polymer electrolyte fuel cell using X-ray imaging technique10.1016/j.jpowsour.2012.12.030 ↗
28. Carbon corrosion mechanism and mitigation strategies in a proton exchange membrane fuel cell (PEMFC): a review
29. Effects of carbon corrosion on mass transfer losses in proton exchange membrane fuel cells10.1016/j.ijhydene.2016.08.223 ↗
30. Evolution of a GDE setup: beyond ambient conditions
31. Using a pressurized GDE setup to analyze effects of temperature and relative humidity on CO-stripping measurements on a commercial Pt/C ORR catalyst
32. Recent developments in the synthesis of supported catalysts10.1021/cr500486u ↗
33. de Jong · 2009
34. Preparation of supported catalysts by deposition-precipitation10.1002/9783527619528.ch4f ↗
35. Preparation of PEMFC electrodes from milligram-amounts of catalyst powder10.1149/2.1461707jes ↗
36. Wiberg · 2010
37. TOPAS and TOPAS-Academic: an optimization program integrating computer algebra and crystallographic objects written in C++10.1107/S1600576718000183 ↗
38. Water management in a PEMFC: water transport mechanism and material degradation in gas diffusion layers10.1002/fuce.201000172 ↗
39. Degradation aspects of water formation and transport in Proton Exchange Membrane Fuel Cell: a review10.1016/j.jpowsour.2013.04.044 ↗
40. A review of accelerated stress tests dedicated to proton exchange membrane fuel cells – part I: fuel cell component level
41. Improved water management of Pt/C cathode modified by graphitized carbon nanofiber in proton exchange membrane fuel cell10.1016/j.jpowsour.2018.07.126 ↗