Nickel/10 mol% scandia - 1 mol% yttria stabilised zirconia (10Sc1YSZ) fuel electrodes for solid oxide electrolysis cells
Source abstract
Abstract
Degradation of the fuel electrode remains a key challenge to solve for a wider adoption of solid oxide electrolysis cell (SOEC) technology to produce green H 2 . In this context, alternatives to the nickel (Ni)/8 mol% yttria stabilised zirconia (8YSZ) fuel electrode, less prone to Ni migration, are being sought. In this work, 10 mol% scandia-1 mol% yttria stabilised zirconia (10Sc1YSZ) is investigated as such an alternative. 10Sc1YSZ-based cells were fabricated by tape casting, screen printing and low temperature sintering. Improvements in durability are observed compared to the state-of-the-art Ni/8YSZ-based cells, which is found to correlate with absent Ni migration. A voltage degradation rate of 2 %/kh is measured at 750 °C and −0.75 A/cm 2 . Recovery of lost cell performance at −1.0 A/cm 2 is found through idling the cell under open circuit conditions, indicating reversibility of fuel electrode degradation. Multi-physics impedance modelling is used to analyse changes in microstructural parameters. The phase stability of 10Sc1YSZ and reduction conditions of the electrodes are investigated, showing an impact on the cell durability. The Ni/10Sc1YSZ fuel electrodes, requiring only minor modifications to the state-of-the-art Ni/yttria stabilised zirconia electrodes, demonstrate improved durability and suppressed Ni migration.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Nuclear Materials and Properties · Molten salt chemistry and electrochemical processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Cost competitiveness of electrolytic hydrogen10.1016/j.joule.2019.07.006 ↗
2. Perspective of the role of hydrogen in the 21st century energy transition10.1016/j.enconman.2021.114898 ↗
3. Carbon abatement costs of green hydrogen across end-use sectors10.1016/j.joule.2024.09.003 ↗
4. Recent advances in solid oxide cell technology for electrolysis10.1126/science.aba6118 ↗
5. Techno-economic analysis of current and emerging electrolysis technologies for green hydrogen production10.1016/j.enconman.2022.116162 ↗
6. Global land and water limits to electrolytic hydrogen production using wind and solar resources10.1038/s41467-023-41107-x ↗
7. Electrolysis of carbon dioxide in solid oxide electrolysis cells10.1016/j.jpowsour.2009.02.093 ↗
8. Encapsulated Co–Ni alloy boosts high-temperature CO2 electroreduction
9. Water electrolysis: from textbook knowledge to the latest scientific strategies and industrial developments10.1039/D0CS01079K ↗
10. Ni migration in solid oxide cell electrodes: review and revised hypothesis10.1002/fuce.202100072 ↗
11. 3D microstructural characterization of Ni/yttria-stabilized zirconia electrodes during long-term CO2 electrolysis10.1039/D3TA01503C ↗
12. Quantifying galvanostatic degradation of solid oxide electrolysis cells: the onset of accelerated degradation of Ni-yttria stabilized zirconia electrode10.1016/j.jpowsour.2024.234490 ↗
13. Degradation in solid oxide electrolysis cells during long term testing10.1002/fuce.201900081 ↗
14. Understanding the ni migration in solid oxide cell: a coupled experimental and modeling approach10.1149/1945-7111/acc1a3 ↗
15. Effect of the operating temperature on the degradation of solid oxide electrolysis cells10.1016/j.jpowsour.2024.234541 ↗
16. Poisoning of solid oxide electrolysis cells by impurities10.1149/1.3464804 ↗
17. TOF-SIMS characterization of impurity enrichment and redistribution in solid oxide electrolysis cells during operation10.1039/C4DT01053A ↗
18. Oxygen electrode degradation in solid oxide cells operating in electrolysis and fuel cell modes: LSCF destabilization and interdiffusion at the electrode/electrolyte interface10.1016/j.ijhydene.2021.07.054 ↗
19. Interdiffusion between gadolinia doped ceria and yttria stabilized zirconia in solid oxide fuel cells: experimental investigation and kinetic modeling10.1016/j.jpowsour.2019.227152 ↗
20. Ionic/electronic conductivity, thermal/chemical expansion and oxygen permeation in Pr and Gd co-doped ceria PrxGd0.1Ce0.9–xO1.95–δ10.1149/2.0531713jes ↗
21. Accelerated ceria–zirconia solubilization by cationic diffusion inversion at low oxygen activity10.1039/C6TA06308J ↗
22. The defect structure of the double layer in yttria-stabilised zirconia10.1016/S0167-2738(02)00484-8 ↗
23. The electrochemical double-layer capacitance of yttria-stabilised zirconia10.1016/S0167-2738(01)01017-7 ↗
24. Integrated 3D modeling unravels the measures to mitigate nickel migration in solid oxide fuel/electrolysis cells10.1039/D3TA06563D ↗
25. Tracking degradation in solid oxide cells by a coupled time and frequency domain multi-physics model: a case study on nickel migration in electrolysis mode10.1016/j.jpowsour.2025.238388 ↗
26. Point defects in oxides: tailoring materials through defect engineering10.1146/annurev-matsci-062910-100442 ↗
27. Characteristic and challenges of scandia stabilized zirconia as solid oxide fuel cell material–in depth review10.1016/j.ssi.2023.116302 ↗
28. Doping of scandia-stabilized zirconia electrolytes for intermediate-temperature solid oxide fuel cell: a review10.1016/j.ceramint.2021.08.285 ↗
29. Correlation between ionic radius and cation diffusion in stabilised zirconia10.1016/j.ssi.2004.07.051 ↗
30. Structural disorder in doped zirconias, part i: the Zr0.85Sc0.2–xYxO1.9 (0.0 ≤ x ≤ 0.2) system10.1021/cm102808k ↗
31. Structural disorder in doped zirconias, part ii: vacancy ordering effects and the conductivity maximum10.1021/cm102809t ↗
32. The system Y2O3 – Sc2O3 – ZrO2: phase stability and ionic conductivity studies10.1016/0955-2219(91)90037-Z ↗
33. Degradation of the electrical conductivity in stabilised zirconia system: part ii: Scandia-stabilised zirconia10.1016/j.ssi.2004.07.039 ↗
34. Evaluation of isotope diffusion coefficient and surface exchange coefficient of ScSZ series oxide by oxygen isotope exchange method10.1016/j.ssi.2017.02.002 ↗
35. Determination of surface exchange coefficients of LSM, LSCF, YSZ, GDC constituent materials in composite SOFC cathodes10.1149/1.3555122 ↗
36. Surface and grain boundary analysis of doped zirconia ceramics studied by AES and XPS10.1007/BF01105274 ↗
37. Effect of segregation on surface and near-surface chemistry of yttria-stabilized zirconia10.1021/jp212133z ↗
38. Absence of dopant segregation to the surface of scandia and yttria co-stabilized zirconia10.1149/2.003206esl ↗
39. Investigation of scandia–yttria–zirconia system as an electrolyte material for intermediate temperature fuel cells—influence of yttria content in system (Y2O3)x (Sc2O3)11–x (ZrO2)8910.1016/j.ssi.2004.02.007 ↗
40. Electrochemical characterization of Ni/ScYSZ electrodes as SOFC anodes10.1149/2.045404jes ↗
41. Durability of solid oxide fuel cells using sulfur containing fuels10.1016/j.jpowsour.2011.02.053 ↗
42. Effects of Ni diffusion on the accelerated conductivity degradation of scandia-stabilized zirconia films under a reducing atmosphere10.1016/j.jeurceramsoc.2016.02.007 ↗
43. Origin of microstructural degradation in nickel oxide–scandia–ceria-stabilized zirconia during reduction10.1021/acsaem.4c02754 ↗
44. Densification behavior of yttria-stabilized zirconia powders for solid oxide fuel cell electrolytes10.1007/s40145-018-0282-4 ↗
45. Sintering, phase composition and ionic conductivity of zirconia–scandia–ceria10.1016/j.jpowsour.2013.01.140 ↗
46. Strength and hydrothermal stability of NiO–stabilized zirconia solid oxide cells fuel electrode supports10.1016/j.jeurceramsoc.2021.01.052 ↗
47. High-temperature degradation of tetragonal zirconia in solid oxide fuel and electrolysis cells: a critical challenge for long-term durability and a solution10.1016/j.jeurceramsoc.2024.04.042 ↗
48. Ni/YSZ electrodes structures optimized for increased electrolysis performance and durability10.1016/j.ssi.2016.06.003 ↗
49. Advanced test method of solid oxide cells in a plug-flow setup10.1149/1.3116247 ↗
50. Advanced insights into gas conversion and diffusion impedance of solid oxide cells by 2D multi-physics modelling10.1016/j.jpowsour.2023.233739 ↗
51. Segmented durability testing of solid oxide electrolysis cells: from model-aided design to proof of concept10.1016/j.electacta.2025.147348 ↗
52. Validation of a physically-based solid oxide fuel cell anode model combining 3D tomography and impedance spectroscopy10.1016/j.ijhydene.2016.09.100 ↗
53. Impact of reduction parameters on the initial performance and stability of Ni/(Sc)YSZ cermet anodes for SOFCs10.1149/1.3701328 ↗
54. Characteristic impedance spectrum associated with partial reduction of electrolyte and/or electrode of zirconia cells10.5796/electrochemistry.61.756 ↗
55. Defect structure of yttria-stabilized zirconia and its influence on the ionic conductivity at elevated temperatures10.1103/PhysRevB.59.14202 ↗
56. Effect of NiO-to-Ni transformation on conductivity and structure of yttria-stabilized ZrO210.1111/j.1151-2916.2001.tb01067.x ↗
57. New opportunities for tailored nanoparticle catalysts through exsolution from inherently disordered defect fluorite-type oxides10.1039/D4TA06854H ↗
58. Enhancement of catalytic performance in Zr0.1Ce0.9O2-δ through transition metal doping and exsolution10.1016/j.ssi.2025.116868 ↗
59. Ni exsolution from (NiO)x (ZrO2)1-x for catalytic CO2 valorization
60. The Ni-O (nickel-oxygen) system10.1007/BF02868949 ↗
61. Lu · 2013
62. Effect of annealing on the electrical conductivity of the Y2O3–ZrO2 system10.1016/j.jpowsour.2003.11.084 ↗
63. A parameter study of solid oxide electrolysis cell degradation: microstructural changes of the fuel electrode10.1016/j.electacta.2018.04.170 ↗