journal article·2025-11Open access

Coupling differential voltage analysis and distribution of relaxation times II: Evaluating the impact of Si content in the degradation of coated NMC811/SiGr cells

Matheus Leal de Souza, Mathieu Morcrette

Abstract

The degradation of coated LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cells with Silicon-Graphite (SiGr) composite anodes containing varying Si content is investigated using Differential Voltage Analysis (DVA), Incremental Capacity Analysis (ICA) and Distribution of Relaxation Times (DRT). ICA distinguishes Si from Gr specific degradation processes. It is observed an incomplete delithiation-related Si capacity loss in cells with 7 % and 11 % Si, which increases during early cycles and later stabilizes. Such behavior is not the reported permanent Si loss of active material, as the capacity of moderately and highly lithiated Si remains unchanged. Instead, a sudden rise in resistance at low states of charge is revealed. That is likely due to Si particle-particle contact loss during shrinkage, after particles are accommodated by a grown Solid Electrolyte Interphase (SEI) matrix and due to SEI cracks closure when particles contract. Data suggest a minimal threshold amount of Si may be necessary to trigger it, explained by Gr acting as electrical-contact keeper to Si particles. The proposed coupling of techniques made observable Si-driven effects in NMC811/SiGr cells, capacity fading primarily due to loss of lithium inventory and resistance increase dominated by the Si at lower voltages and by the NMC811 at medium and higher voltages.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Coupling differential voltage analysis and distribution of relaxation times I: evaluating the impact of NMC811 coating in the degradation of NMC811/Gr cells10.1016/j.jpowsour.2025.237184 ↗
2. The success story of graphite as a lithium-ion anode material – fundamentals, remaining challenges, and recent developments including silicon (Oxide) composites10.1039/D0SE00175A ↗
3. Challenges for rechargeable Li batteries10.1021/cm901452z ↗
4. The state of understanding of the lithium-ion-battery graphite solid electrolyte interphase (SEI) and its relationship to formation cycling10.1016/j.carbon.2016.04.008 ↗
5. Electric vehicle batteries: status and perspectives of data-driven diagnosis and prognosis10.3390/batteries8100142 ↗
6. A review of recent developments in Si/C composite materials for Li-Ion batteries10.1016/j.ensm.2020.10.026 ↗
7. Toward practical high-energy and high-power lithium battery anodes: present and future10.1002/advs.202105213 ↗
8. Towards a better understanding of the degradation mechanisms of Li-Ion full cells using Si/C composites as anode10.1016/j.jpowsour.2022.231408 ↗
9. The electrode-electrolyte interface in Li-Ion batteries: current understanding and new insights10.1021/acs.jpclett.5b01727 ↗
10. Electrolyte additives for lithium ion battery electrodes: progress and perspectives10.1039/C6EE00123H ↗
11. Electrochemical Characterization of Cu-Catalysed Si Nanowires as an Anode for Lithium-Ion Cells10.1155/2020/4272090 ↗
12. Solid electrolyte interphase growth and capacity loss in silicon electrodes10.1021/jacs.6b02882 ↗
13. On the capacity losses seen for optimized Nano-Si composite electrodes in Li-Metal half-cells10.1002/aenm.201901608 ↗
14. Investigation of the failure mechanisms of Li-Ion pouch cells with Si/Graphite composite negative electrodes and single wall carbon nanotube conducting additive10.1149/1945-7111/ad3398 ↗
15. Parasitic reactions in nanosized silicon anodes for lithium-ion batteries10.1021/acs.nanolett.6b04551 ↗
16. A comparative study of polyacrylic acid (PAA) and carboxymethyl cellulose (CMC) binders for Si-Based electrodes10.1016/j.electacta.2017.11.082 ↗
17. Sodium Carboxymethyl Cellulose: a Potential Binder for Si Negative Electrodes for Li-Ion Batteries10.1149/1.2398725 ↗
18. Enhanced cycle performance of SiO-C composite anode for lithium-ion batteries10.1016/j.jpowsour.2007.03.081 ↗
19. SiO anode: from fundamental mechanism toward industrial application10.1002/smll.202102641 ↗
20. Research progress on silicon/carbon composite anode materials for lithium-ion battery10.1016/j.jechem.2017.12.012 ↗
21. Alloy negative electrodes for Li-Ion batteries10.1021/cr500207g ↗
22. Chatzogiannakis, D.; Ghilescu, I.; Giannadaki, G.; Cabello, M.; Casas-Cabanas, M.; Palacin, M. R. Decoupling silicon and graphite contribution in high-silicon content composite electrodes. Batteries Supercaps n/a (n/a), 2500104. https://doi.org/10.1002/batt.202500104..
23. Morphological changes of silicon nanoparticles and the influence of cutoff potentials in silicon-graphite electrodes10.1149/2.1261807jes ↗
24. Differentiating the degradation phenomena in silicon-graphite electrodes for lithium-ion batteries10.1149/2.1921712jes ↗
25. Capacity fading mechanisms of silicon nanoparticle negative electrodes for lithium ion batteries10.1149/2.0731512jes ↗
26. Comprehensive electrochemical impedance spectroscopy study of Si-Based anodes using distribution of relaxation times analysis10.1016/j.jpowsour.2020.229083 ↗
27. The value of battery diagnostics and prognostics
28. Synthesize battery degradation modes via a diagnostic and prognostic model10.1016/j.jpowsour.2012.07.016 ↗
29. Rate dependency of incremental capacity analysis (dQ/dV) as a diagnostic tool for lithium-ion batteries10.1016/j.est.2020.101329 ↗
30. Lithium-Ion battery degradation indicators via incremental capacity analysis10.1109/TIA.2019.2891213 ↗
31. Aging of a commercial Graphite/LiFePO4 cell10.1149/1.3614529 ↗
32. Mathematical model of lithium-ion batteries with blended-electrode system10.1016/j.jpowsour.2014.04.072 ↗
33. Differential voltage analyses of high-power, lithium-ion cells: 1. Technique and application10.1016/j.jpowsour.2004.07.021 ↗
34. Long-term low-rate cycling of LiCoO2/Graphite Li-Ion cells at 55°C10.1149/2.056206jes ↗
35. Electrochemical protocols to assess the effects of dissolved transition metal in Graphite/LiNiO2 cells performance10.1149/1945-7111/ac7e7a ↗
36. Understanding the impedance spectrum of 18650 LiFePO4-Cells10.1016/j.jpowsour.2012.12.020 ↗
37. Teardown analysis and characterization of a commercial lithium-ion battery for advanced algorithms in battery electric vehicles10.1016/j.est.2021.103909 ↗
38. Differential voltage curve analysis of a lithium-ion battery during discharge10.1016/j.jpowsour.2018.07.043 ↗
39. Electrochemistry visualization tool to support the electrochemical analysis of batteries10.1002/batt.202200378 ↗
40. Derivation of a distribution function of relaxation times for the (Fractal) finite length warburg10.1016/j.electacta.2017.08.154 ↗
41. In situ conductivity, impedance spectroscopy, and Ex situ Raman Spectra of amorphous silicon during the insertion/extraction of lithium10.1021/jp0729563 ↗
42. Optimized process parameters for a reproducible distribution of relaxation times analysis of electrochemical systems10.3390/batteries5020043 ↗
43. Non-invasive investigation of predominant processes in the impedance spectra of high energy lithium-ion batteries with nickel–cobalt–aluminum cathodes10.1016/j.jpowsour.2020.228189 ↗
44. Detection of lithium‐ion cells degradation through deconvolution of EIS with distribution of relaxation time10.1002/ente.202200547 ↗
45. In situ and operando investigations of failure mechanisms of the solid electrolyte interphase on silicon electrodes10.1021/acsenergylett.6b00284 ↗
46. Failure progression in the solid electrolyte interphase (SEI) on silicon electrodes10.1016/j.nanoen.2019.104257 ↗
47. Chemo-mechanical model of SEI growth on silicon electrode particles
48. Investigation of the solid electrolyte interphase formation at graphite anodes in lithium-ion batteries with electrochemical impedance spectroscopy10.1016/j.electacta.2017.01.128 ↗
49. Modeling graphite anodes with serial and transmission line models10.1016/j.jpowsour.2015.02.038 ↗
50. Material parameters affecting Li plating in Si/Graphite composite electrodes10.1016/j.electacta.2024.145010 ↗
51. Voltage dependent solid electrolyte interphase formation in silicon electrodes: monitoring the formation of organic decomposition products10.1021/acs.chemmater.5b04408 ↗
52. The critical role of carbon in marrying silicon and graphite anodes for high-energy lithium-ion batteries10.1002/cey2.2 ↗
53. Electrical conductivity of geopolymer-graphite composites: percolation, mesostructure and analytical modeling
54. Interfacially induced cascading failure in graphite‐silicon composite anodes
55. Lithium-ion battery degradation: measuring rapid loss of active silicon in silicon–graphite composite electrodes10.1021/acsaem.2c02047 ↗