Optimum operating conditions of DIR-MCFC without vapor-phase carbonate pollution
Source abstract
Abstract
Abstract In direct internal reforming-molten carbonate fuel cells (DIR-MCFC), deterioration of catalytic activity takes place in the anode channel due to both liquid-phase pollution and vapor-phase pollution. Although the liquid-phase pollution can be solved by installing protective barrier, an effective defense method and a reactivation method of vapor-phase polluted catalyst have not established yet. In order to study the reactivation method, the adhesion form of potassium compounds in the polluted catalyst under the various gas conditions was evaluated by using a thermogravimetric analyzer in which water vapor can feed. Additionally, the activity of the treated catalyst was also tested by a differential reactor. As a result, KOH changes to K 2 CO 3 under a CO 2 concentration of 25% or more. KOH becomes a solid-phase from the liquid-phase when it is changed into K 2 CO 3 . Therefore, the catalyst can not be reactive because K 2 CO 3 chokes pores of the catalyst. However, the activity of the polluted catalyst is revived to 80% of the initial activity by controlling the gas species concentration, especially CO 2 . Moreover, the catalytic activity can be revived under a steam–carbon ratio of 2.0 or more. Based on the results obtained by these fundamental experiments, the reactivation methods of catalyst polluted are proposed as follows: (i) catalyst should be loaded more upstream in the anode; (ii) in order to reactivate the polluted catalyst, the DIR-MCFC should maintain a steam–carbon ratio of 2.0 or more; (iii) gas conditions to activate the catalyst should be applied regularly.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Catalysis and Hydrodesulfurization Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. C. Hirai, M. Matsumura, S. Tanaka, Studies on reforming catalyst for internal reforming molten carbonate fuel cell, Abstract Book of the 29th Battery Symposium in Japan, vols. 79–80, 1988.
2. Y. Gonjyo, M. Matsumura, S. Tanaka, Performance of internal reforming molten carbonate fuel cell—activity of internal reforming catalyst vs. cell voltage, Abstract book of the 29th Battery Symposium in Japan, vols. 81–82, 1988.
3. Development of internal reforming molten carbonate fuel cell stacks
4. Steam reforming of hydrocarbons on nobel metal catalysts. Part 8. Steam reforming of methane on supported ruthenium catalysts10.1627/jpi1958.33.152 ↗
5. Deterioration mechanism of direct internal reforming catalyst10.1252/jcej.31.734 ↗
6. Deterioration of a catalyst’s activity by liquid-phase MC poisoning in DIR-MCFC
7. A Study on degradation phenomena of reforming catalyst in DIR-MCFC
8. Deterioration of a catalyst’s activity in direct internal reforming-molten carbonate fuel cells (effect of adsorption of vapor-phase molten carbonate)
9. Relationship between catalytic activity and gas-phase pollution fractions in the catalyst in DIR-MCFC (reactivation method of polluted catalyst by vapor-phase carbonate)
10. JANAF Thermochemical Tables, third ed., vol. 14, 1985, pp. 606–608, 628, 1219–1222, 1273–1275.