Study of passivation at the positive active material/grid interface in lead–acid batteries
Source abstract
Abstract
Abstract A valuable additive — boric acid — to eliminate passivation of the active material/grid interface in positive plates of lead–acid batteries has been selected through comparison of single-cell discharge tests. This overcomes the problem of rapid decline in initial performance when using low-antimony (1.7 wt.%) grid alloys. The performance of the oxide film on positive grids, as well as its composition and amount, is determined through cathodic reduction of the film with a linear sweep voltammetric (LSV) method. The results confirm that passivation of the positive grid and rapid decline in the initial discharge voltage are due to a resistive layer of PbSO4, and not PbOn (1≤n≤2). The PbOn layer has little effect on passivation. The findings of this study are useful for the production of lead–acid batteries.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Supercapacitor Materials and Fabrication
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. Culpin · J. Power Sources · 1992 · 38 · 6310.1016/0378-7753(92)80096-T ↗
2. Wei · Acta Chimica Sinica · 1992 · 50 · 467
3. Pavlov · J. Power Sources · 1993 · 42 · 34510.1016/0378-7753(93)90002-I ↗
4. Simon · J. Power Sources · 1994 · 50 · 14110.1016/0378-7753(93)01893-M ↗
5. Brinic · J. Power Sources · 1995 · 55 · 1910.1016/0378-7753(94)02151-R ↗
6. Pavlov · J. Power Sources · 1993 · 46 · 17110.1016/0378-7753(93)90016-T ↗