Structural changes of bare and AlPO4-coated LixCoO2 (x=0.24 and 0.1) upon thermal annealing ≥200°C
Source abstract
Abstract
Abstract Structural changes of bare and AlPO 4 -coated Li x CoO 2 with a coating thickness of 20 and 200 nm are investigated at x = 0.24 and 0.1 after thermal annealing at 200, 300, and 400 °C using XRD and Co K-edge XANES (X-ray absorption near-edge structure) and EXAFS (extended X-ray absorption fine structure). Both the bare and coated cathodes exhibit faster phase transformation into spinel phases at lower annealing temperatures as x in Li x CoO 2 is decreased. Bare Li x CoO 2 cathodes exhibit phase transitions from Li x Co 2 O 4 to Co 3 O 4 spinel as the annealing temperature is increased and the x is value decreased, which suggests a possible reaction according to (1/2)Li x Co 2 O 4 → x Li 2 CO 3 + (1/3)Co 3 O 4 + (2/3)O 2 . However, the coated cathodes sustain a Li x Co 2 O 4 phase even at 400 °C and x = 0.1. This indicates that the AlPO 4 coating layer suppresses the Li x Co 2 O 4 phase decomposition into Co 3 O 4 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Magnetic Properties and Synthesis of Ferrites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Choi · J. Electrochem. Soc. · 2002 · 149 · A16210.1149/1.1431574 ↗
2. MacNeil · J. Electrochem. Soc. · 2002 · 149 · A91210.1149/1.1483865 ↗
3. Baba · Solid State Ionics · 2002 · 148 · 31110.1016/S0167-2738(02)00067-X ↗
4. Lee · J. Electrochem. Soc. · 2005 · 152 · A182410.1149/1.1979193 ↗
5. Cho · Angew. Chem. Int. Ed. · 2003 · 42 · 161810.1002/anie.200250452 ↗
6. Cho · Electochim. Acta · 2003 · 48 · 280710.1016/S0013-4686(03)00415-8 ↗
7. S.W. Martin, Ph.D. Thesis, Purdue University, 1986.
8. 1994 · vol. 1