On the cycle behavior of various graphitic negative electrodes in a propylene carbonate-based electrolyte for lithium ion batteries
Source abstract
Abstract
Abstract We investigated the negative electrode behaviors of several mesocarbon microbeads (MCMB) heat-treated over 2000 °C in 1 M LiPF6/propylene carbonate (PC) electrolyte under various charge–discharge current densities. A higher current density provided improved (a highly graphitized MCMB)/Li cell cycle stability as lower graphitized MCMB electrode was used. In addition, two pre-cycles at a higher current density also provided better cycle stability in subsequent cycles at a lower current density. For example, MCMB 6 μm in diameter and heat-treated at 2800 °C cycled stably at a current density of 0.2 mA cm−2 after 2 pre-cycles at 0.5 mA cm−2. A higher current density may provide an adequate surface film at the first charging.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Dey · J. Electrochem. Soc. · 1970 · 117 · 22210.1149/1.2407470 ↗
2. Eichinger · J. Electroanal. Chem. · 1976 · 74 · 18310.1016/S0022-0728(76)80234-3 ↗
3. Arakawa · J. Electroanal. Chem. · 1987 · 217 · 27310.1016/0022-0728(87)85045-3 ↗
4. Fong · J. Electrochem. Soc. · 1990 · 137 · 200910.1149/1.2086855 ↗
5. Ohusid · J. Power Sources · 1993 · 43–44 · 47
6. Fujimoto · J. Power Sources · 1996 · 63 · 12710.1016/S0378-7753(96)02446-9 ↗
7. Inaba · J. Power Sources · 1997 · 68 · 22110.1016/S0378-7753(96)02555-4 ↗
8. R. Imhof, P. Novák, in: C.F. Holmes, A.R. Landgrebe (Eds.), Proceedings of the Symposium on Batteries for Portable Applications and Electric Vehicles, PV 97-18, The Electrochemical Society Proceedings Series, Pennington, NJ, 1997, p. 313.
9. Fujimoto · J. Power Sources · 1998 · 72 · 22610.1016/S0378-7753(97)02691-8 ↗
10. Wrodnigg · J. Electrochem. Soc. · 1999 · 146 · 47010.1149/1.1391630 ↗
11. Wang · J. Power Sources · 1998 · 74 · 14210.1016/S0378-7753(98)00017-2 ↗
12. Inaba · Electrochemistry · 1999 · 67 · 115310.5796/electrochemistry.67.1153 ↗
13. Naji · Electrochim. Acta · 2000 · 45 · 189310.1016/S0013-4686(99)00410-7 ↗
14. Wang · J. Power Sources · 2001 · 93 · 12310.1016/S0378-7753(00)00552-8 ↗
15. Houska · J. Appl. Phys. · 1954 · 25 · 150310.1063/1.1702373 ↗
16. Tatsumi · J. Electrochem. Soc. · 1995 · 142 · 71610.1149/1.2048523 ↗
17. Morita · Electrochim. Acta · 1993 · 38 · 172110.1016/0013-4686(93)85068-A ↗
18. Kanno · J. Electrochem. Soc. · 1992 · 139 · 339710.1149/1.2069090 ↗
19. Aurbach · J. Power Sources · 1997 · 68 · 9110.1016/S0378-7753(97)02575-5 ↗
20. E. Peled, in: S. Megahed, B. Barnett, L. Xie (Eds.), Rechargeable Lithium and Lithium-Ion Batteries, PV 94-28, The Electrochemical Society, Pennington, NJ 1995.
21. Fong · J. Electrochem. Soc. · 1990 · 137 · 200910.1149/1.2086855 ↗