Examining the effects of silicon based additives on the long-term cycling capabilities of cylindrical cells
Source abstract
Abstract
There is an ever increasing demand for higher power and energy in EVs and the use of anodes with a percentage of silicon (Si) is becoming more prevalent to meet those demands. This article describes the results of a systematic study on electrochemical performance and the impact of mechanical changes within two types of batteries of commercial relevance that are nominally identical except their anode chemistry. We analyse 32 cells with a composite anode comprising graphite and a silicon-based component, and 30 cells with conventional graphite anodes and reveal through X-ray computed tomography that jelly roll deformations nucleate as a result of the swelling of the anode layers towards the centre of the cell. Furthermore, although Si causes large mechanical changes in the architecture of the jelly roll, with respect to the SOH window relevant for EVs, the presence of a small percentage of Si does not have a highly detrimental impact on the cycling performance of the cells. In fact, with respect to cell degradation, it appears that commercial cells have not yet reached the limit of Si loading in composite anodes, and there is room for improvement in cell capacities to meet the increasing demands on EVs.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Brief history of early lithium-battery development10.3390/ma13081884 ↗
2. Electrical energy storage for transportation - approaching the limits of, and going beyond, lithium-ion batteries10.1039/c2ee21892e ↗
3. An attempt to formulate nonflammable lithium ion electrolytes with alkyl phosphates and phosphazenes10.1149/1.1467946 ↗
4. Yoshio · 2009
5. Safety mechanisms in lithium-ion batteries10.1016/j.jpowsour.2005.12.002 ↗
6. Synthesis and characterization of Zn-doped LiCo0.3Ni0.4(xMn0.3ZnxO2 cathode materials for lithium-ion batteries10.1016/j.jallcom.2008.09.055 ↗
7. Cyclability study of silicon-carbon composite anodes for lithium-ion batteries using electrochemical impedance spectroscopy10.1016/j.electacta.2011.02.014 ↗
8. Reaction of Li with alloy thin films studied by in situ AFM10.1149/1.1613668 ↗
9. Evolution of the Si electrode/electrolyte interface in lithium batteries characterized by XPS and AFM techniques: the influence of vinylene carbonate additive10.1016/j.ssi.2012.03.042 ↗
10. Silicon solid electrolyte interphase (SEI) of lithium ion battery characterized by microscopy and spectroscopy10.1021/jp404155y ↗
11. Volume, pressure and thickness evolution of Li-ion pouch cells with silicon-composite negative electrodes10.1149/2.1691712jes ↗
12. Investigation of cycling-induced microstructural degradation in silicon-based electrodes in lithium-ion batteries using X-ray nanotomography10.1016/j.electacta.2017.08.161 ↗
13. Microstructural degradation of silicon electrodes during lithiation observed via operando X-ray tomographic imaging10.1016/j.jpowsour.2016.12.070 ↗
14. In-operando X-ray tomography study of lithiation induced delamination of Si based anodes for lithium-ion batteries10.1149/2.0081407eel ↗
15. 4D analysis of the microstructural evolution of Si-based electrodes during lithiation: time-lapse X-ray imaging and digital volume correlation10.1016/j.jpowsour.2016.04.076 ↗
16. An advanced microstructural and electrochemical datasheet on 18650 Li-ion batteries with nickel-rich NMC811 cathodes and graphite-silicon anodes10.1149/1945-7111/abc4c1 ↗
17. Virtual unrolling of spirally-wound lithium-ion cells for correlative degradation studies and predictive fault detection10.1039/C9SE00500E ↗
18. Cycle life estimation of lithium secondary battery by extrapolation method and accelerated aging test10.1016/S0378-7753(01)00646-2 ↗
19. Lithium plating in a commercial lithium-ion battery – a low-temperature aging study10.1016/j.jpowsour.2014.11.065 ↗
20. A mechanical aging mechanism in lithium-ion batteries10.1149/2.1001410jes ↗
21. Determining the limits and effects of high-rate cycling on lithium iron phosphate cylindrical cells10.3390/batteries6040057 ↗