Abstract

Abstract The proton conductivity at the interface of Nafion and sulfonated polypyrrolone composite membrane decreases by 56% from 0.039 S cm −1 to 0.017 S cm −1 , due to phase separation after annealing this binary composite membrane at 140 °C, which is 10 °C above the glass transition temperature of Nafion polymer. After annealing the membrane, the change in the relative intensity of the lower angles of the X-ray diffraction (XRD) peaks located at ca. 11.9°, 17.5° and 19.7° indicates an increase of the low spacing region for the polymer chains of the composite membrane and atomic force microscopy (AFM) measurement depicts a morphological evolution from an uniform dispersion to a spherules micro-structure, implying the aggregation of polymer chains of the annealed composite membrane. These results are combined to reveal there is a microphase separation of this binary composite membrane as it is annealed at 140 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Conducting polymers and applications · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Zimmerman · J. Polym. Sci. Part B Polym. Phys. · 1999 · 37 · 123510.1002/(SICI)1099-0488(19990615)37:12<1235::AID-POLB5>3.0.CO;2-J ↗
2. Zimmerman · J. Polym. Sci. Part B Polym. Phys. · 1999 · 37 · 125110.1002/(SICI)1099-0488(19990615)37:12<1251::AID-POLB6>3.0.CO;2-E ↗
3. Mahajan · J. Phys. Chem. B · 2010 · 114 · 835710.1021/jp104078h ↗
4. Asano · J. Am. Chem. Soc. · 2006 · 128 · 176210.1021/ja0571491 ↗
5. Chen · Electrochem. Commun. · 2007 · 9 · 71810.1016/j.elecom.2006.11.004 ↗
6. Swier · Polym. Eng. Sci. · 2005 · 45 · 108110.1002/pen.20361 ↗
7. Xu · Electrochim. Acta · 2005 · 50 · 328010.1016/j.electacta.2004.12.014 ↗
8. Burns · Macromolecules · 2003 · 36 · 237410.1021/ma0259261 ↗