journal article·2008-10

A new lead alloy current-collector manufactured by a powder rolling process and its corrosion behavior under lead-acid battery conditions

Masanori Sakai, Yasuo Kondo, Satoshi Minoura, Takeo Sakamoto, Tokiyoshi Hirasawa

Journal of Power Sources· Volume 185· Issue 1
Publisher page

Abstract

Abstract A new powder rolling process for manufacturing current-collector sheets for lead-acid batteries has been developed. Gas-atomized lead–tin and lead–tin–calcium alloy powders obtained by a rapid solidification process in air were employed as raw materials for the powder rolling process. The corrosion behavior of powder-rolled lead–tin alloys with various compositions of tin has been investigated. A dipping corrosion test of square plain sheets of the alloys was performed in H 2 SO 4 at 75 °C. The test was repeated up to 20 cycles with each cycle consisting of a controlled 10 mA cm −2 oxidation current for 6 h and a rest under open circuit voltage for 6 h. The extent of corrosion–elongation and the appearance of the corroded surface of the tested specimens were the main observations. The corrosion–elongation of the corroded sheet of a powder-rolled lead alloy containing 1.5 wt% tin with ca. 200 μm initial thickness was less than 5%, whereas that of the corroded sheet of the cast-rolled lead alloy containing 1.5 wt% tin with the same initial thickness was 25–30% under the same corrosion test conditions. The corroded powder-rolled sheet of the 1.5 wt% tin lead alloy has uniform corrosion, but the cast-rolled sheet of lead alloy containing 1.5 wt% tin was much distorted and was perforated by the corrosion. Intergranular corrosion of the powder-rolled lead–tin alloys was much suppressed as compared with that of the cast-rolled lead–tin alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Moseley · J. Power Sources · 2004 · 133 · 10410.1016/j.jpowsour.2003.12.034 ↗
2. Moseley · J. Power Sources · 2006 · 157 · 310.1016/j.jpowsour.2006.02.031 ↗
3. Moseley · 2007
4. Bhardwaj · J. Power Sources · 1999 · 78 · 13010.1016/S0378-7753(99)00022-1 ↗
5. Bhardwaj · J. Power Sources · 2000 · 91 · 5110.1016/S0378-7753(00)00486-9 ↗
6. Caballero · J. Power Sources · 2004 · 125 · 24610.1016/j.jpowsour.2003.07.005 ↗
7. Bourguignon · J. Power Sources · 2003 · 113 · 30110.1016/S0378-7753(02)00525-6 ↗
8. Xu · J. Power Sources · 2006 · 155 · 42010.1016/j.jpowsour.2005.04.026 ↗
9. Slavkov · J. Power Sources · 2002 · 112 · 19910.1016/S0378-7753(02)00368-3 ↗
10. Rocca · J. Power Sources · 2006 · 161 · 66610.1016/j.jpowsour.2006.04.140 ↗
11. Jullian · J. Power Sources · 2003 · 116 · 18510.1016/S0378-7753(02)00705-X ↗
12. Koura · Denki Kagaku · 2005 · 2 · 135
13. Dehmas · J. Power Sources · 2006 · 159 · 72110.1016/j.jpowsour.2005.07.094 ↗
14. Mukaitani · J. Power Sources · 2006 · 158 · 89710.1016/j.jpowsour.2006.05.013 ↗
15. Hilger · Mater. Charact. · 1990 · 24 · 15910.1016/1044-5803(90)90033-G ↗
16. Lushina · J. Power Sources · 2005 · 148 · 9510.1016/j.jpowsour.2005.01.044 ↗
17. Bode · 1977 · 345
18. Mukaitani · J. Power Sources · 2005 · 144 · 52810.1016/j.jpowsour.2004.11.047 ↗
19. Warlimont · J. Power Sources · 2005 · 144 · 48610.1016/j.jpowsour.2004.11.052 ↗
20. Yang · J. Chem. Phys. · 1998 · 109 · 1033110.1063/1.477688 ↗
21. Morimoto · J. Electrochem. Soc. · 1988 · 135 · 29310.1149/1.2095603 ↗
22. Yamada · J. Power Sources · 2005 · 113 · 35210.1016/j.jpowsour.2004.10.012 ↗
23. Jones · 1992