Effect of binder on the overcharge response in LiFePO4-containing cells
Source abstract
Abstract
Abstract Two types of small pouch cells based on LiFePO4/graphite, one containing a N-methyl pyrrolidinone (NMP)-soluble binder, poly(vinylidene difluoride), and the other an aqueous-soluble binder, styrene-butadiene rubber/carboxymethylcellulose were systematically charged to 100, 120, 140, 160, 180, and 250% state of charge (SOC). The cells were then discharged to 3.0 V at room temperature before being disassembled for postmortem analysis. Microstructural changes in the anode associated with increasing SOC were more pronounced in the aqueous processed cells in comparison to the NMP-processed cells. Dendrite formation was observed on the aqueous-processed anode at 120% SOC, while the NMP-processed anode surface does not show dendrites until 250% SOC. Overall, the aqueous-processed anode surfaces displayed more evidence of microstructural degradation as a function of increasing SOC. In the NMP-processed cells, four organic compounds on the anode surface were found to show a dependence on SOC, while only two displayed a similar dependency in the aqueous-processed cells. The nature of the binder changed the number and composition of the species found at the anode.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Narayana · ChemPhysChem · 2015 · 16 · 117910.1002/cphc.201402674 ↗
2. Wang · Phys. Chem. Chem. Phys. · 2013 · 15 · 684910.1039/c3cp50992c ↗
3. Wen · J. Power Sources · 2014 · 264 · 15510.1016/j.jpowsour.2014.04.077 ↗
4. Dietz Rago · J. Power Sources · 2018 · 385 · 14510.1016/j.jpowsour.2018.01.009 ↗
5. Bloom · J. Power Sources · 2018 · 385 · 15610.1016/j.jpowsour.2017.12.015 ↗
6. Bareño · J. Power Sources · 2018 · 385 · 16510.1016/j.jpowsour.2017.12.061 ↗
7. Golukov · RSC Adv. · 2015 · 5 · 5717110.1039/C5RA05897J ↗
8. Lamb · J. Power Sources · 2014 · 247 · 101110.1016/j.jpowsour.2013.08.044 ↗
9. Xu · J. Electrochem. Soc. · 2012 · 159 · A67810.1149/2.024206jes ↗
10. Larsson · J. Electrochem. Soc. · 2014 · 161 · A161110.1149/2.0311410jes ↗
11. Liu · J. Electrochem. Soc. · 2015 · 162 · A220810.1149/2.0911510jes ↗
12. Li · MRS Adv. · 2016 · 1 · 102910.1557/adv.2016.6 ↗
13. Li · J. Electrochem. Soc. · 2012 · 159 · A115210.1149/2.018208jes ↗
14. Howe · J. Mater. Sci. · 2012 · 47 · 157210.1007/s10853-011-6029-z ↗
15. Malinowski · 2002
16. Sahore · Chem. Mater. · 2019 · 31 · 288410.1021/acs.chemmater.9b00063 ↗
17. Wood · Energy Storage Mater. · 2020 · 24 · 18810.1016/j.ensm.2019.08.020 ↗