The counterintuitive impact of separator–electrolyte combinations on the cycle life of graphite–silicon composite electrodes
Source abstract
Abstract
Abstract Thin polymeric membranes such as Celgard are commonly used as separators in Li-ion batteries to ensure high volumetric energy density. Independently, for silicon-based electrodes fluoroethylene carbonate (FEC) is often added to the electrolyte to improve the cycling stability of the cell. Here we demonstrate that, counterintuitively, this separator–electrolyte combination negatively affects the performance of graphite–Si electrodes in half-cells. In a statistical evaluation of the cycling behavior of C–Si electrode cells with various separators and either with or without FEC addition, we show that by improving the solid electrolyte interphase on the silicon particles, FEC addition leads to inhomogeneous current distribution in the electrodes, therefore favoring lithium dendrite growth and leading to irreversible failure with Celgard. In contrast, self-recovery is observed with simple glass-fiber separators. Without FEC, neither dendrites nor failure are observed, but cells with Celgard suffer from poorer electrochemical performance, due to clogging by the thick polymeric layer formed using standard electrolytes, than cells with thicker and hydrophilic separators.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. McDowell · Adv. Mater. · 2013 · 25 · 496610.1002/adma.201301795 ↗
2. Luo · J. Electrochem. Soc. · 2015 · 162 · A250910.1149/2.0131514jes ↗
3. Szczech · Energy Environ. Sci. · 2011 · 4 · 5610.1039/C0EE00281J ↗
4. Ma · Nano-Micro Lett. · 2014 · 6 · 34710.1007/s40820-014-0008-2 ↗
5. Casimir · Nano Energy · 2016 · 27 · 35910.1016/j.nanoen.2016.07.023 ↗
6. Choi · J. Power Sources · 2006 · 161 · 125410.1016/j.jpowsour.2006.05.049 ↗
7. Dalavi · J. Electrochem. Soc. · 2012 · 159 · A64210.1149/2.076205jes ↗
8. Kim · Curr. Appl. Phys. · 2014 · 14 · 59610.1016/j.cap.2014.02.008 ↗
9. Bordes · J. Power Sources · 2014 · 257 · 16310.1016/j.jpowsour.2013.12.144 ↗
10. Xu · Chem. Mater. · 2015 · 27 · 259110.1021/acs.chemmater.5b00339 ↗
11. Etacheri · Langmuir · 2012 · 28 · 96510.1021/la203712s ↗
12. Lin · Chem. Commun. · 2012 · 48 · 726810.1039/c2cc31712e ↗
13. Chen · ChemSusChem · 2014 · 7 · 54910.1002/cssc.201300770 ↗
14. Schroder · Chem. Mater. · 2015 · 27 · 553110.1021/acs.chemmater.5b01627 ↗
15. Zhang · J. Power Sources · 2007 · 164 · 35110.1016/j.jpowsour.2006.10.065 ↗
16. Yang · Membranes · 2012 · 2 · 36710.3390/membranes2030367 ↗
17. Arora · Chem. Rev. · 2004 · 104 · 441910.1021/cr020738u ↗
18. Gómez-Cámer · Carbon · 2016 · 105 · 4210.1016/j.carbon.2016.04.022 ↗
19. Obrovac · Electrochem. Solid-State Lett. · 2004 · 7 · A9310.1149/1.1652421 ↗
20. Obrovac · J. Electrochem. Soc. · 2007 · 154 · A10310.1149/1.2402112 ↗
21. Li · J. Electrochem. Soc. · 2007 · 154 · A15610.1149/1.2409862 ↗
22. Oumellal · J. Mater. Chem. · 2011 · 21 · 620110.1039/c1jm10213c ↗
23. Peng · J. Electrochem. Soc. · 2015 · 162 · A707210.1149/2.0061513jes ↗
24. Song · J. Electrochem. Soc. · 2000 · 147 · 321910.1149/1.1393886 ↗
25. Zhu · J. Membr. Sci. · 2016 · 504 · 8910.1016/j.memsci.2016.01.020 ↗
26. J. Conder, S. Urbonaite, L. Gubler, P. Novák, PSI Electrochemistry Laboratory, Annual Report, (2013) 37–38.
27. Jung · J. Electrochem. Soc. · 2016 · 163 · A170510.1149/2.0951608jes ↗
28. Wu · Nat. Commun. · 2014 · 5 · 519310.1038/ncomms6193 ↗
29. Wandt · Energy Environ. Sci. · 2015 · 8 · 135810.1039/C4EE02730B ↗
30. Song · J. Electrochem. Soc. · 2013 · 160 · A87310.1149/2.101306jes ↗
31. Cannarella · J. Electrochem. Soc. · 2015 · 162 · A136510.1149/2.1051507jes ↗
32. Jana · J. Power Sources · 2015 · 275 · 91210.1016/j.jpowsour.2014.11.056 ↗