journal article·2011-05Open access

Interfacial failure via encapsulation of external particulates in an outward-growing thermal oxide

Keeyoung Jung, Chang-Soo Kim, Frederick S. Pettit, Gerald H. Meier

Journal of Power Sources· Volume 196· Issue 10

Abstract

Abstract A Cr2O3-forming Ni-base superalloy and this alloy coated with a Pt-modified aluminide coating were exposed to SiO2 powder and cyclically oxidized at 950 °C. The uncoated alloy showed a considerable amount of spallation and buckling whereas the Pt–NiAl coated alloy remained protective throughout hundred 1 h-cycles. The interfacial failure is mainly ascribed to the increased thermal strain by the encapsulation of external SiO2 particulates in an outward-growing Cr2O3 layer. However, the particles were not embedded in the thermally grown oxide of the Pt–NiAl coated alloy due to the slow inward-growing characteristics of Al2O3 scales. The buckling of the Cr2O3 scale with embedded SiO2 was analyzed with (1) a classical buckling criterion using the instantaneous coefficients of thermal expansion of the constituents, and (2) finite element analyses (FEA) to estimate the local interfacial shear stresses. It turns out that the thermal strain with embedded SiO2 is larger than the experimentally determined critical thermal strain (ɛb) explaining the buckling of the oxide scale observed in the experiment. The FEA results demonstrate that local shear stresses at the metal/oxide interface are significantly amplified near the SiO2 particles showing that the buckling of oxide can be readily initiated especially in the vicinity of the embedded particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Wenglarz · 2002
2. Reed · 1971
3. Wright · Int. J. Hydrogen Energy · 2007 · 32 · 361010.1016/j.ijhydene.2006.08.049 ↗
4. Wenglarz · 2003 · 4-45
5. Birks · 2006
6. Borom · Surf. Coat. Technol. · 1996 · 86–87 · 11610.1016/S0257-8972(96)02994-5 ↗
7. Mercer · Acta Mater. · 2005 · 53 · 102910.1016/j.actamat.2004.11.028 ↗
8. Krämer · Mater. Sci. Eng. A · 2008 · 490 · 2610.1016/j.msea.2008.01.006 ↗
9. Evans · J. Eur. Ceram. Soc. · 2008 · 28 · 140510.1016/j.jeurceramsoc.2007.12.023 ↗
10. Wellman · Tribol. Int. · 2008 · 41 · 65710.1016/j.triboint.2007.10.004 ↗
11. Chiang · J. Mater. Eng. · 1984 · 6 · 71
12. Jung · Mater. Sci. Forum · 2008 · 595–598 · 80510.4028/www.scientific.net/MSF.595-598.805 ↗
13. Kutchko · Fuel · 2006 · 85 · 253710.1016/j.fuel.2006.05.016 ↗
14. Bordenet · Mater. Sci. Forum · 2008 · 595–598 · 26110.4028/www.scientific.net/MSF.595-598.261 ↗
15. Holcomb · 2009
16. Schilke · 2004
17. Gordon · Acta Mater. · 2007 · 55 · 337510.1016/j.actamat.2007.01.034 ↗
18. Quadakkers · Oxid. Met. · 1989 · 32 · 6710.1007/BF00665269 ↗
19. Evans · Prog. Mater. Sci. · 2001 · 46 · 50510.1016/S0079-6425(00)00020-7 ↗
20. Ruud · J. Am. Ceram. Soc. · 2001 · 84 · 154510.1111/j.1151-2916.2001.tb00875.x ↗
21. Yanar · Metall. Mater. Trans. A · 2006 · 37 · 156310.1007/s11661-006-0100-4 ↗
22. Touloukian · 2002
23. Zhang · Metall. Mater. Trans. A · 1999 · 30 · 267910.1007/s11661-999-0308-1 ↗
24. Evans · Corros. Sci. · 1984 · 24 · 20910.1016/0010-938X(84)90051-9 ↗
25. Timoshenko · 1961
26. Evans · Proc. R. Soc. A · 1993 · 440 · 110.1098/rspa.1993.0001 ↗
27. Christl · Oxid. Met. · 1989 · 31 · 110.1007/BF00665485 ↗
28. Schütze · Oxid. Met. · 1995 · 44 · 2910.1007/BF01046722 ↗
29. Schütze · 1997
30. Schütze · Oxid. Met. · 2010 · 73 · 38910.1007/s11085-009-9185-7 ↗
31. Tien · 1975 · 200
32. Trexler · Scr. Mater. · 2006 · 55 · 56110.1016/j.scriptamat.2006.04.033 ↗
33. Delesse · Ann. Mine. · 1862 · 13 · 379
34. Shenoy · Int. J. Plasticity · 2006 · 22 · 230110.1016/j.ijplas.2006.03.003 ↗
35. Sun · J. Power Sources · 2008 · 176 · 16710.1016/j.jpowsour.2007.10.027 ↗