journal article·2006-07

The effects of different additives in electrolyte of AGM batteries on self-discharge

M. Safari Yazd, A. Molazemi, M.H. Moayed

Journal of Power Sources· Volume 158· Issue 1
Publisher page

Abstract

Abstract Hydrogen and oxygen evolution at the negative and positive electrodes in AGM batteries are the main reasons of self-discharging. The self-discharge of five AGM batteries was investigated by measuring different potential between two electrodes during 48 days. Five different battery electrolytes were used including 35% (w/w) H2SO4 without additives and the remaining contain 7.1, 9.94, and 21.3 g l−1 sodium sulfate, 4 g l−1 boric acid, 3 g l−1 citric acid, and finally 0.7 and 1 g l−1 stearic acid except one containing boric acid that the concentration of H2SO4 was 36% (w/w). The results revealed that the rate of self-discharge for battery without additive was 0.01 V day−1. The battery with boric acid showed the lowest rate of self-discharge with 0.0025 V day−1. It was also found that stearic and citric acids are comparatively appropriate additives for decreasing the self-discharge. They caused a decrease of the self-discharge rate to 0.005 and 0.0075 V day−1 on appropriate concentration, respectively. In compared to other additives, sodium sulfate showed to be not an appropriate additive for decreasing battery self-discharging. The rate of 0.03 V day−1 of self-discharging was obtained for the battery containing all selected concentration of sodium sulfate during first 4 days of measuring.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Technologies Research · Supercapacitor Materials and Fabrication · Fuel Cells and Related Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Crompton · 2000 · vol. 31
2. Gladstone · Nature · 1882 · 25 · 22110.1038/025221a0 ↗
3. Ruetschi · J. Power Sources · 2004 · 127 · 3310.1016/j.jpowsour.2003.09.052 ↗
4. Ruetschi · J. Electrochem. Soc. · 1958 · 105 · 10510.1149/1.2428756 ↗
5. Bullock · J. Electrochem. Soc. · 1976 · 123 · 32710.1149/1.2132819 ↗
6. Berndt · J. Power Sources · 2001 · 100 · 2910.1016/S0378-7753(01)00881-3 ↗
7. Manders · J. Power Sources · 1998 · 73 · 15210.1016/S0378-7753(98)00032-9 ↗
8. Bullock · J. Electrochem. Soc. · 1982 · 129 · 139310.1149/1.2124172 ↗
9. Ullmann's Encyclopedia of Industrial Chemistry, sixth ed., vol. A3, Wiley, 1990, p. 378.
10. Lam · J. Power Sources · 1998 · 73 · 3610.1016/S0378-7753(98)00020-2 ↗
11. Cooper · J. Power Sources · 2003 · 113 · 20010.1016/S0378-7753(02)00515-3 ↗
12. Symanski · J. Electrochem. Soc. · 1988 · 138 · 54810.1149/1.2095655 ↗
13. Kirchev · J. Power Sources · 2003 · 113 · 24510.1016/S0378-7753(02)00520-7 ↗
14. Grayson · 1991 · vol. 3
15. Wu · J. Power Sources · 2002 · 107 · 16210.1016/S0378-7753(01)01001-1 ↗
16. Badawy · J. Power Sources · 1995 · 55 · 1110.1016/0378-7753(94)02022-U ↗
17. Wei · J. Power Sources · 1994 · 52 · 2510.1016/0378-7753(94)01929-0 ↗
18. Mahato · J. Electrochem. Soc. · 1983 · 130 · 213910.1149/1.2119541 ↗