Abstract In this study, dense electrolyte ceramic Sm0.2Ce0.8O2−δ (SDC) thin films are successfully deposited on NiO-SDC anode substrate by aerosol deposition (AD) with oxygen as the carrier gas at the substrate temperature ranging from room temperature to 300 °C. To remove the effect of humidity on the starting powders, this study found that, in depositing SDC films, having the starting powders preheat-treated at 200 °C helped generate a smooth and dense layer, though a lower deposition rate was achieved. At a deposition time of 22 min, SDC films with a uniform thickness of 1.5 μm and grain sizes of ≈67 nm are obtained. SOFC single cells are then built by screen printing a LSCF cathode on the anode-supported substrates with SDC electrolyte. The cross-sectional SEM micrographs exhibit highly dense, granular, and crack-free microstructures. The open circuit voltages (OCV) of the single cells decrease with the rise in temperature, dropping from 0.81 V at 500 °C to 0.59 V at 700 °C. Maximum power densities (MPD) decline with decreasing operating temperature from 0.34 to 0.01 W cm−2 due to the increase of the R0 and RP of the single cells. The electrochemical results testify to the fine quality of SDC films as well as illustrate the electrolyte thickness effect and the effect of mixed ionic and electronic conduction of the SDC electrolyte in the reducing atmosphere.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalysis and Oxidation Reactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Mata · Int. J. Hydrogen Energy · 2007 · 32 · 79610.1016/j.ijhydene.2006.12.012 ↗
2. Wen · Solid State Ionics · 2002 · 148 · 51310.1016/S0167-2738(02)00098-X ↗
3. Joo · J. Power Sources · 2008 · 180 · 19510.1016/j.jpowsour.2008.02.013 ↗
4. Ivers-Tiffée · J. Eur. Ceram. Soc. · 2001 · 21 · 180510.1016/S0955-2219(01)00120-0 ↗
5. Zhang · Electrochim. Acta · 2008 · 53 · 499810.1016/j.electacta.2008.01.095 ↗
6. Fergus · J. Power Sources · 2006 · 162 · 3010.1016/j.jpowsour.2006.06.062 ↗
7. Jordan · Solid State Ionic · 2008 · 17910.1016/j.ssi.2007.12.008 ↗
8. Yang · J. Power Sources · 2007 · 164 · 18210.1016/j.jpowsour.2006.09.102 ↗
9. Zao · Int. J. Hydrogen Energy · 2010 · 35 · 73110.1016/j.ijhydene.2009.10.090 ↗
10. Liu · J. Power Sources · 2010 · 195 · 704610.1016/j.jpowsour.2010.04.083 ↗
11. Chou · Nano Lett. · 2009 · 9 · 362610.1021/nl901724j ↗
12. Mineshige · Solid State Ionics · 2004 · 175 · 48310.1016/j.ssi.2004.03.050 ↗
13. Tarancon · J. Nanosci. Nanotechnol. · 2010 · 10 · 132710.1166/jnn.2010.1837 ↗
14. Charoirochkul · J. Eur. Ceram. Soc. · 2004 · 24 · 252710.1016/j.jeurceramsoc.2003.08.008 ↗
15. Yan · J. Power Sources · 2008 · 180 · 37310.1016/j.jpowsour.2008.02.035 ↗
16. Zhang · J. Power Sources · 2008 · 175 · 80010.1016/j.jpowsour.2007.10.021 ↗
17. Moon · Int. J. Hydrogen Energy · 2008 · 33 · 175810.1016/j.ijhydene.2007.12.062 ↗
18. Leng · Int. J. Hydrogen Energy · 2004 · 29 · 102510.1016/j.ijhydene.2004.01.009 ↗
19. Chen · J. Power Sources · 2009 · 186 · 12810.1016/j.jpowsour.2008.09.061 ↗
20. Tomova · J. Power Sources · 2010 · 195 · 716010.1016/j.jpowsour.2010.05.044 ↗
21. Matsuda · J. Power Sources · 2007 · 165 · 10210.1016/j.jpowsour.2006.11.087 ↗
22. Ma · J. Power Sources · 2007 · 164 · 8610.1016/j.jpowsour.2006.09.093 ↗
23. Akedo · J. Therm. Spray Technol. · 2008 · 17 · 18110.1007/s11666-008-9163-7 ↗
24. Akedo · Recent Res. Dev. Mater. Sci. · 2001 · 2 · 51
25. Akedo · J. Soc. Powder Technol. Jpn. · 2003 · 40 · 19210.4164/sptj.40.192 ↗
26. Akedo · Mater. Sci. Forum · 2004 · 449
27. Akedo · Jpn. J. Appl. Phys. · 1999 · 38 · 539710.1143/JJAP.38.5397 ↗
28. Akedo · J. Am. Ceram. Soc. · 2006 · 89 · 183410.1111/j.1551-2916.2006.01030.x ↗
29. Lebedev · J. Crystal Growth · 2005 · 275 · e130110.1016/j.jcrysgro.2004.11.109 ↗
30. Imanaka · J. Crystal Growth · 2005 · 275 · e131310.1016/j.jcrysgro.2004.11.107 ↗
31. Yu · J. Power Sources · 2005 · 152 · 2210.1016/j.jpowsour.2005.03.173 ↗
32. Ding · J. Power Sources · 2010 · 195 · 548710.1016/j.jpowsour.2010.03.075 ↗