Abstract

Abstract Spirally wound 12-V valve-regulated lead-acid batteries were subjected to conventional-charge and rapid-charge cycling tests. The cycle life was 250 cycles for the conventional-charge regime and 1000 cycles for the rapid-charge regime. In conventional-charge cycling, the positive active material quickly expanded and developed a coralloid structure in association with lowered utilisation and integrity. In rapid-charge cycling, no coralloid structure developed and the expansion was smaller and much slower. Correspondingly, the particle size of the negative active material grew in both cycling tests, but at a much slower rate in rapid-charge cycling. With the expansion of the positive active material, the negative active material was compressed. In the failed batteries, about one-third of the negative active material in the centre of the electrode was compressed almost into a solid non-porous mass. This densification process also occurred at a much slower rate in rapid-charge cycling. At the point of failure, the discharge capacity of all test batteries was limited by the negative electrode, although it was limited by the positive electrode at the beginning of the cycling tests. The cause of failure for most of the batteries, regardless of the charging regime, was the occurrence of “soak-through” shorts caused by numerous minute lead dendrites formed in the separator. This might have been encouraged by the formation of shorter distances between the two electrodes, created by the compression of the separator as a result of the expansion of the positive active material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Woodbridge · Trans. Am. Inst. Electr. Eng. · 1935 · 54 · 51610.1109/T-AIEE.1935.5057021 ↗
2. Vinal · 1935 · 244
3. Bode · 1977 · 308
4. Gosden · J. Power Sources · 1995 · 45 · 6110.1016/0378-7753(93)80009-E ↗
5. Very fast charging of lead-acid batteries
6. Nor · 1991
7. Valeriote · J. Power Sources · 1992 · 40 · 9310.1016/0378-7753(92)80041-9 ↗
8. Chang · 1993 · 405
9. Chang · J. Power Sources · 1994 · 48 · 16310.1016/0378-7753(94)80015-4 ↗
10. Chang · J. Power Sources · 1997 · 64 · 10310.1016/S0378-7753(96)02509-8 ↗
11. J.K. Nor, European Patent 0 311 460 A2, October 10, 1988; U.S. Patent 5,202,617, April 13, 1993.10.1002/sca.4950100109 ↗
12. Nor · 1991
13. J.K. Nor, Proc. 11th Int. Electric Vehicle Symposium, Florence, Italy, September 27–30, 1992, Paper No. 9.03.
14. J.K. Nor, Proc. 26th Int. Symposium on Automotive Technology, Aachen, Germany, September 13–17, 1993, Paper 93EL020, p. 375.
15. Nor · 1994
16. Barrett · J. Am. Chem. Soc. · 1951 · 73 · 37310.1021/ja01145a126 ↗
17. Gregg · 1982
18. Klug · 1974
19. Balzar · J. Appl. Crystallogr. · 1992 · 25 · 55910.1107/S0021889892004084 ↗
20. Balzar · J. Appl. Crystallogr. · 1993 · 26 · 9710.1107/S0021889892008987 ↗
21. Balzar · J. Res. Natl. Inst. Stand. Technol. · 1993 · 98 · 32110.6028/jres.098.026 ↗
22. Balzar · J. Mater. Sci. Lett. · 1992 · 11 · 141910.1007/BF00729647 ↗
23. Balzar · Powder Diffr. · 1993 · 8 · 210.1017/S0885715600017656 ↗
24. J.I. Langford, Accuracy in Powder Diffraction II, NIST Special Publication 846, US Government Printing Office, Washington, D.C., 1992, p.110.
25. De Keijser · J. Appl. Crystallogr. · 1982 · 15 · 30810.1107/S0021889882012035 ↗
26. De Keijser · J. Appl. Crystallogr. · 1983 · 16 · 30910.1107/S0021889883010493 ↗
27. Warren · 1969
28. N.H. Furman, Standard Methods of Chemical Analysis, The Elements, Vol. I, 6th edn., p. 578.
29. 1963 · 439
30. Gregg · 1982
31. Lowell · 1991
32. Chang · J. Electrochem. Soc. · 1984 · 131 · 175510.1149/1.2115955 ↗
33. Okada · Yuasa Jiho · 1996 · 81 · 3
34. Valeriote · Can. J. Chem. · 1979 · 57 · 97410.1139/v79-161 ↗
35. Danel · Electrochim. Acta · 1981 · 27 · 77110.1016/0013-4686(82)85073-1 ↗