Effects of the first heat up procedure on mechanical properties of solid oxide fuel cell sealing materials

Markus Rautanen, Valtteri Pulkkinen, Johan Tallgren, Olli Himanen, Jari Kiviaho

Publisher page

Abstract

SOFC stack seals need to be correctly dimensioned to achieve a gas tight stack with low electrical contact resistances. Mechanical properties of SOFC stack sealing materials are presented for three assembly and first heat up procedures: applying full compressive stress at room temperature before first heat up (1), applying no compressive stress before first heat up and applying the full compressive stress at operating temperature (2), applying partial compressive stress at room temperature and full compressive stress at operating temperature after first heat up (3). The behaviour of the glass seal (Schott GM31107) is not affected significantly by compressive force during heat up. Compressibility of both compressible sealing material (Thermiculite CL87) and hybrid sealing material (Thermiculite CL87LS) was found to be about 40% (between 0.1 and 0.9 MPa) at room temperature but only about 4% (between 0.1 and 0.9 MPa) at 700 °C. Therefore it is beneficial to carry out as much of the compression as possible at room temperature before first heat up. This allows for maximum amount of deformability in the sealing materials resulting in the highest ability to compensate for stack manufacturing and assembly tolerances, which is needed to realize a gas tight stack with low electrical contact resistances.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalysis and Oxidation Reactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Reinforced composite sealants for solid oxide fuel cell applications10.1016/j.jpowsour.2011.02.002 ↗
2. Investigation of solid oxide fuel cell sealing behaviour under stack relevant conditions at Forschungzentrum Jülich10.1016/j.jpowsour.2010.09.041 ↗
3. Mechanical reliability and durability of SOFC stacks. Part II: modelling of mechanical failures during ageing and cycling10.1016/j.ijhydene.2012.03.023 ↗
4. Effects of clamping load on the thermal stress distribution in a planar SOFC with compressive sealing10.1149/1.3205543 ↗
5. Sealants for solid oxide fuel cells10.1016/j.jpowsour.2005.05.002 ↗
6. Mechanical properties of oriented mica glass ceramic10.1016/S0022-3093(97)00299-8 ↗
7. New Glass Ceramic Sealants for SOFCs10.1149/1.3205682 ↗
8. Compressive mica seals for SOFC applications10.1016/S0378-7753(01)00811-4 ↗
9. SOFC sealing with Thermiculite 866 and Thermiculite 866 LS10.1149/05701.2365ecst ↗
10. Compression properties and leakage tests of mica-based seals for SOFC applications10.1002/fuce.200900029 ↗
11. Glass coated compressible solid oxide fuel cell seals10.1016/j.jpowsour.2013.08.085 ↗
12. Gaskets for sealing solid oxide fuel cells10.1016/S1350-4789(07)70376-8 ↗
13. Flexitallic, “Thermiculite 866/866LS,” Flexitallic Ltd, [Online]. Available: http://www.flexitallicsofc.com/downloads/Flexitallic_SOFC_thermiculite_866.pdf. [Accessed 28 01 2015].
14. ThyssenKrupp. [Online]. Available: http://www.fcdic.com/ja/member/data/Crofer22H.pdf.