Influence of positive active material type and grid alloy on corrosion layer structure and composition in the valve regulated lead/acid battery
Source abstract
Abstract
Performance of a valve regulated lead/acid battery is affected by the properties of the positive grid corrosion layer. An investigation has been carried out using a range of experimental techniques to study the influence of corrosion layer composition and structure on cyclic performance. A number of designs of battery were manufactured with different grids and positive active materials (PAMs). Two grid types were used consisting of either pure lead or a lead/tin alloy. Variations in PAM composition and structure were obtained by forming electrodes from grey oxide pastes containing additions of, red lead, tetrabasic lead sulphate, or sulphuric acid (sulphated). Results indicated that both grid alloy composition and PAM type affect the corrosion layer properties. Ultra-microtoming was used to prepare sections of the grid/corrosion layer interface. Results showed that corrosion propagated along tin rich grain boundaries.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced battery technologies research · Advanced Battery Technologies Research · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. A theory of the grid/positive active mass (PAM) interface and possible methods to improve PAM utilization and cycle life of lead/acid batteries10.1016/0378-7753(94)02152-S ↗
2. The lead/acid battery lead dioxide active mass: a gel-crystal system with proton and electron conductivity10.1149/1.2069034 ↗
3. Operational experience with valve regulated lead/acid batteries10.1016/0378-7753(94)01980-A ↗
4. Some physical properties of sputtered PbO2 films10.1016/0022-3697(62)90237-8 ↗
5. Effects of grid alloy on the properties of positive-plate corrosion layers in lead/acid batteries. Implications for premature capacity loss under repetitive deep-discharge cycling service10.1016/0378-7753(94)80017-0 ↗
6. Influence of antimony on the structure and the degree of hydration of the anodic PbO2 layer formed an Pb–Sb electrodes10.1149/1.2055119 ↗
7. Mechanism of action of Sn on the passivation phenomena in the lead/acid battery positive plate (Sn free effect)10.1149/1.2096603 ↗
8. Garche · Electrochimica. Acta · 1981 · 26 · 136310.1016/0013-4686(81)90003-7 ↗
9. Nelson · J. Power Sources · 1991 · 33 · 16510.1016/0378-7753(91)85058-5 ↗
10. Characterisation of defects observed within the positive grid corrosion layer of the valve regulated lead/acid battery10.1016/S0378-7753(01)00856-4 ↗
11. Optimas 6.1, Optimas UK Ltd., West Maling, Kent, UK.