journal article·2024-09Open access

The tremendous challenge of suitable KPF6-based electrolytes for 4 V-class K-metal cells

Nicolas Dautain, Jean-Frédéric Martin, Dane Sotta, Philippe Azais, David Peralta

Abstract

The high reactivity of potassium metal leads to the degradation of electrolytes based on KPF$_6$ dissolved in carbonates when used in K-metal cells. This phenomenon induces poor electrochemical performances for such cells, especially when they contain a high potential positive electrode material (beyond 4 V vs. K$^+$/K). In this study, we used a Prussian White (PW) K$_2$Mn[Fe(CN)$_6$] cathode material combined with a precisely described potassium metal electrode preparation to compare the performances of KPF$_6$-based electrolytes without additive or in presence of DTD (1,3,2-DioxaThiolane 2,2-Dioxide), FEC (FluoroEthylene Carbonate) or VC (Vinylene Carbonate). Focusing on 0.7 M KPF$_6$ in EC:DEC (1:1) electrolyte, we showed that the formation and oxidation of EGEC (Ethylene Glycol bis-(Ethyl Carbonate)) can explain the high initial irreversible capacity and low coulombic efficiency observed upon cycling. No improvement is obtained in presence of DTD, while FEC addition addresses the high initial irreversible capacity by suppressing initial EGEC formation. However, electrolyte and potassium metal electrode ageing still occurs in presence of FEC, leading to bad capacity retention and still low coulombic efficiency. Finally, we found that VC addition permits both good capacity retention and high coulombic efficiency of PW|K cells: it suppresses efficiently EGEC formation upon cycling by forming a resistive but stable passivation layer at the surface of potassium metal, hence limiting electrolyte and potassium electrode ageing. We demonstrate that VC is an additive of choice for KPF$_6$-based electrolytes in K-metal cells, allowing an accurate evaluation of the electrochemical performances of high potential potassium-based insertion materials with potassium metal as a reference electrode.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Research development on K-ion batteries10.1021/acs.chemrev.9b00463 ↗
2. Research development on sodium-ion batteries10.1021/cr500192f ↗
3. Carbon electrodes for K-ion batteries10.1021/jacs.5b06809 ↗
4. Potassium intercalation into graphite to realize high-voltage/high-power potassium-ion batteries and potassium-ion capacitors10.1016/j.elecom.2015.09.002 ↗
5. Thermodynamic functions of transfer of single ions from water to nonaqueous and mixed solvents: Part 3 - standard potentials of selected electrodes10.1351/pac198557081129 ↗
6. A potassium-rich iron hexacyanoferrate/dipotassium terephthalate@carbon nanotube composite used for K-ion full-cells with an optimized electrolyte10.1039/C7TA05460B ↗
7. A novel K-ion battery: hexacyanoferrate(II)/graphite cell10.1039/C7TA00220C ↗
8. Crystallite size control of prussian white analogues for nonaqueous potassium-ion batteries10.1021/acsenergylett.7b00179 ↗
9. A Fe/Mn-based prussian blue analogue as a K-rich cathode material for potassium-ion batteries10.1002/celc.201700410 ↗
10. Prussian white analogues as promising cathode for non-aqueous potassium-ion batteries10.1016/j.elecom.2017.02.012 ↗
11. Low-cost high-energy potassium cathode10.1021/jacs.6b12598 ↗
12. KVPO4F and KVOPO4 toward 4 volt-class potassium-ion batteries10.1039/C6CC10280H ↗
13. Origin of capacity degradation of high-voltage KVPO 4 F cathode10.1149/1945-7111/aba54e ↗
14. Effect of the electrode/electrolyte interface structure on the potassium-ion diffusional and charge transfer rates: towards a high voltage potassium-ion battery10.1016/j.electacta.2017.11.131 ↗
15. Spray-dried K3V(PO4)2/C composites as novel cathode materials for K-ion batteries with superior electrochemical performance10.1016/j.jpowsour.2020.229057 ↗
16. Nonaqueous liquid electrolytes for lithium-based rechargeable batteries10.1021/cr030203g ↗
17. Electrolytes and interphases in Li-ion batteries and beyond10.1021/cr500003w ↗
18. Potassium metal as reliable reference electrodes of nonaqueous potassium cells10.1021/acs.jpclett.9b00711 ↗
19. Paving the way for K-ion batteries: role of electrolyte reactivity through the example of Sb-based electrodes10.1021/acsami.8b08902 ↗
20. Impact of the salt anion on K metal reactivity in EC/DEC studied using GC and XPS analysis10.1021/acsami.1c19537 ↗
21. 1,3,2-Dioxathiolane 2,2-dioxide as an electrolyte additive for K-metal cells10.1021/acsenergylett.1c01238 ↗
22. Impact of electrolyte decomposition products on the electrochemical performance of 4 V class K-ion batteries10.1039/D3SC02111D ↗
23. Effect of the electrolyte on K-metal batteries10.1039/D0CC05024E ↗
24. Highly concentrated electrolyte solutions for 4 V class potassium-ion batteries10.1039/C8CC04433C ↗
25. KFSA/glyme electrolytes for 4 V-class K-ion batteries10.1039/D0TA08851J ↗
26. A nonflammable electrolyte enabled high performance K0.5MnO2 cathode for low-cost potassium-ion batteries10.1021/acsenergylett.0c00912 ↗
27. The quest for stable potassium-ion battery chemistry
28. Reversible dendrite-free potassium plating and stripping electrochemistry for potassium secondary batteries10.1021/jacs.7b04945 ↗
29. Towards K-ion and Na-ion batteries as “beyond Li-ion,”10.1002/tcr.201700057 ↗
30. Roadmap for potassium-ion batteries
31. Development of nonaqueous electrolytes for high-voltage K-ion batteries10.1246/bcsj.20210412 ↗
32. Safe electrolyte for long-cycling alkali-ion batteries10.1038/s41893-024-01275-0 ↗
33. Molecular-level design for a phosphate-based electrolyte for stable potassium-ion batteries10.1063/5.0178871 ↗
34. H. Zhang, H. Wang, W. Li, Y. Wei, B. Wen, D. Zhai, F. Kang, Enabling High-Performance Potassium-Ion Batteries by Manipulating Interfacial Chemistry, Adv. Funct. Mater. n/a (n.d.) 2312368. https://doi.org/10.1002/adfm.202312368.10.1002/adfm.202312368 ↗
35. A low-strain potassium-rich prussian blue analogue cathode for high power potassium-ion batteries10.1002/anie.202103475 ↗
36. Exploring the role of crystal water in potassium manganese hexacyanoferrate as a cathode material for potassium-ion batteries10.3390/cryst11080895 ↗
37. Additives engineered nonflammable electrolyte for safer potassium ion batteries10.1002/adfm.202001934 ↗
38. Less is more: trace amount of a cyclic sulfate electrolyte additive enable ultra-stable graphite anode for high-performance potassium-ion batteries10.1021/acsami.2c12704 ↗
39. All-solid-state potassium polymer batteries enabled by the effective pretreatment of potassium metal10.1021/acsenergylett.2c01096 ↗
40. Glyoxal-based electrolytes for potassium-ion batteries10.1016/j.ensm.2022.02.041 ↗
41. Identification and quantification of the main electrolyte decomposition by-product in Na-ion batteries through FEC: towards an improvement of safety and lifetime10.1149/2.0671702jes ↗
42. Deciphering the multi-step degradation mechanisms of carbonate-based electrolyte in Li batteries10.1016/j.jpowsour.2007.11.110 ↗
43. Anode passivation and electrolyte solvent disproportionation: mechanism of ester exchange reaction in lithium‐ion batteries10.1149/1.1837726 ↗
44. Mechanistic insights into the intercalation and interfacial chemistry of mesocarbon microbeads anode for potassium ion batteries10.1002/smll.202103557 ↗
45. Effects of fluoroethylene carbonate-induced solid-electrolyte-interface layers on carbon-based anode materials for potassium ion batteries10.1016/j.apsusc.2021.149193 ↗
46. Origins of irreversible capacity loss in hard carbon negative electrodes for potassium-ion batteries10.1063/5.0003257 ↗