journal article·2023-06

Quantitative investigation of the cycling behavior and SEI formation of tin through time-resolved microgravimetry

Ke Wang, Yug Joshi, Hong Chen, Guido Schmitz

Publisher page

Abstract

Insufficient understanding on the mechanism of electrode failure restricts the development of sensitive electrode materials such as tin-based alloys. Here-in, a non-destructive and time-resolved in-situ characterization method is proposed for the investigation of the electrode failure. The cycling behavior of tin electrode and the evolution of the Solid-Electrolyte Interface (SEI) were investigated via combining quartz crystal micro-gravimetry (QCM) with cyclic voltammetry (CV). Key findings were further confirmed by ex-situ SEM, TEM and XPS. Remarkably, opposite to the general behavior, SEI thickness grows linearly with the electrode`s thickness. This is ascribed to the continuous cracking and oxidization of Sn. However, below a critical thickness (X o), the SEI growth by cracking (X sn > X o) transitions to diffusion-controlled growth (X sn ≤ X o ). Surprisingly, after serious fracture of Sn, the QCM mass spectrometry reveals, the mass of Li 2O also cycled reversibly along with Li insertion. Despite the general belief that the SEI is formed before the lithiation, the inorganic SEI mainly composed of Li 2O and Li 2CO 3 unexpectedly forms in the later cycles during the lithiation. This inorganic part of the SEI plays the most important role of stabilizing the SEI. Preventing its formation, by using an unsuitable voltage window, results in a completely porous non-self-limiting SEI along with a porous electrode.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Conducting polymers and applications · Transition Metal Oxide Nanomaterials · Electrochemical Analysis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Challenges for rechargeable Li batteries10.1021/cm901452z ↗
2. Guidelines and trends for next-generation rechargeable lithium and lithium-ion batteries10.1039/C7CS00863E ↗
3. High-voltage liquid electrolytes for Li batteries: progress and perspectives
4. Tin-based materials as advanced anode materials for lithium ion batteries: a review
5. Tin-based anode materials with well-designed architectures for next-generation lithium-ion batteries10.1016/j.jpowsour.2016.04.105 ↗
6. Solid electrolyte interphase instability in operating lithium-ion batteries unraveled by enhanced-Raman spectroscopy10.1021/acsenergylett.1c00436 ↗
7. Improved stability of nano-Sn electrode with high-quality nano-SEI formation for lithium ion battery10.1016/j.nanoen.2014.12.041 ↗
8. Review—SEI: past, present and future10.1149/2.1441707jes ↗
9. Review of emerging concepts in SEI analysis and artificial SEI membranes for lithium, sodium, and potassium metal battery anodes
10. Generation and evolution of the solid electrolyte interphase of lithium-ion batteries10.1016/j.joule.2019.08.018 ↗
11. How can the electrode influence the formation of the solid electrolyte interface?10.1021/acsenergylett.1c01359 ↗
12. Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries10.1038/s41524-018-0064-0 ↗
13. Reaction of Li with alloy thin films studied by in situ AFM10.1149/1.1613668 ↗
14. Direct visualization of the solid electrolyte interphase and its effects on silicon electrochemical performance
15. J. Pre-solid electrolyte interphase-covered Li metal anode with improved electro-chemo-mechanical reliability in high-energy-density batteries10.1021/acsami.1c05966 ↗
16. General method of manipulating formation, composition, and morphology of solid-electrolyte interphases for stable Li-alloy anodes10.1021/jacs.7b07584 ↗
17. Morphology dependent electrochemical performance of sputter deposited Sn thin films10.1016/j.materresbull.2012.04.035 ↗
18. Dramatically enhanced reversibility of Li2O in SnO2-based electrodes: the effect of nanostructure on high initial reversible capacity10.1039/C5EE03367E ↗
19. Morphological changes in and around Sn electrodes during Li ion cycling characterized by in situ environmental TEM10.1016/j.scriptamat.2013.07.028 ↗
20. In situ monitoring of gravimetric and viscoelastic changes in 2D intercalation electrodes10.1021/acsenergylett.7b00133 ↗
21. In situ real-time gravimetric and viscoelastic probing of surface films formation on lithium batteries electrodes10.1038/s41467-017-01722-x ↗
22. In situ real-time mechanical and morphological characterization of electrodes for electrochemical energy storage and conversion by electrochemical quartz crystal microbalance with dissipation monitoring10.1021/acs.accounts.7b00477 ↗
23. Verwendung von Schwingquarzen zur Wägung dünner Schichten und zur Mikrowägung10.1007/BF01337937 ↗
24. In situ quantification of interphasial chemistry in Li-ion battery10.1038/s41565-018-0284-y ↗
25. Quantification of the mass and viscoelasticity of interfacial films on tin anodes using EQCM-D10.1021/acsami.5b07966 ↗
26. LixV2O5 – analysis of surface reactions by spectroscopic quartz crystal mircogravimetry10.1016/j.jpowsour.2016.10.073 ↗
27. Reversible oxide formation during cycling of Si anodes10.1016/j.nanoen.2021.105886 ↗
28. In-situ analysis of solid-electrolyte interphase formation and cycle behavior of Sn battery anodes10.1016/j.jpowsour.2022.231439 ↗
29. Study of copper foam-supported Sn thin film as a high-capacity anode for lithium-ion batteries10.1016/j.electacta.2009.05.051 ↗
30. Lithiation and delithiation mechanisms of gold thin film model anodes for lithium ion batteries: electrochemical characterization10.1016/j.electacta.2015.02.184 ↗