journal article·2025-11

Influence of the interface layer on the fracture toughness of Ti2AlNb/Ti6Al4V layered metal composite

Wanying Du, Xin Wang, Boxin Wei, Xuewen Li, Guojian Cao, Wenbin Fang, Hao Wu, Guohua Fan

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Titanium Alloys Microstructure and Properties · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Formation of equiaxed O bands at the interface of TiAl/Ti2AlNb heterostructures: abnormal growth of O variants and novel annealed twins10.1016/j.coco.2024.102243 ↗
2. Microstructure and mechanical properties of continuous drive friction welded Ti2AlNb alloy under different rotational rates10.1016/S1003-6326(24)66604-5 ↗
3. Fracture toughness of Ti2AlNb alloy with different Al content: intrinsic mechanism, extrinsic mechanism and prediction model10.1016/j.jallcom.2023.170068 ↗
4. Controlling the tensile properties of a high-strength-ductility Ti2AlNb alloy by hot rolling10.1016/j.jmrt.2024.09.020 ↗
5. Effect of processing parameters on the microstructure and mechanical properties of TiAl/Ti2AlNb laminated composites10.1016/j.jmst.2021.08.067 ↗
6. Phase transformation and microstructure control of Ti2AlNb-based alloys: a review10.1016/j.jmst.2020.11.022 ↗
7. Interlaminar toughening and self-healing mechanism for hard-and-soft layered composite laminates10.1016/j.compositesa.2024.108623 ↗
8. Enhanced interlaminar fracture toughness of unidirectional CFRP laminates with tailored microstructural heterogeneity of toughening layer10.1016/j.compositesa.2023.107872 ↗
9. Microstructure and properties of Ti/TiO2@SiC/Ti6Al4V composites by selective laser melting10.1016/j.coco.2025.102331 ↗
10. Interface characteristics and mechanical properties of a Ti–TiAl laminated composite10.1016/j.matchar.2023.113468 ↗
11. Enhanced strength and toughness in TC4-(GNPs/TC4) composites via heterogeneous multi-scale lamination design10.1016/j.matchar.2024.114184 ↗
12. Effect of annealing temperature on as-cast Ti6Al4V–5Cu alloy microstructure, tensile properties, and fracture toughness
13. Microstructure and mechanical properties of Ti6Al4V based laminated composites at various rolling reductions10.1016/j.coco.2022.101212 ↗
14. Additive manufacturing of (TiB+TiC)/Ti6Al4V composites with tailored network reinforcement architecture10.1016/j.coco.2023.101611 ↗
15. Design a Ti6Al4V–Ti43Al9V laminated composite with high strength and fracture toughness10.1016/j.vacuum.2023.112556 ↗
16. In-situ synthesis of high strength and toughness TiN/Ti6Al4V sandwich composites by laser powder bed fusion under a nitrogen-containing atmosphere10.1016/j.compositesb.2023.110534 ↗
17. Architecture design and significant toughness enhancement of Ti6Al4V based composites with gradient laminate distributed TiB10.1016/j.matchar.2023.113253 ↗
18. Combining fasting diffusion and microstructure regulation to achieve high-quality diffusion bonding of Ti2AlNb/TA2 at low temperature10.1016/j.matchar.2024.114593 ↗
19. The interface structure and its impact on the mechanical behavior of TiAl/Ti2AlNb laminated composites10.1016/j.msea.2021.142095 ↗
20. Achieving optimal Ti content via interfacial reaction layer characteristics of Diamond/Cu–Sn–Ti composites10.1016/j.ceramint.2024.04.131 ↗
21. Extending the modified transverse crack tensile test for mode II fracture toughness characterisation of hybrid interfaces10.1016/j.compositesb.2024.112063 ↗
22. Interface effects on the fracture mechanism of a high-toughness aluminum-composite laminate10.1007/s11661-008-9679-y ↗
23. Effect of grain morphology and interface on the toughness of nacre-like aluminas10.1016/j.actamat.2024.120338 ↗
24. Deformation behavior of brittle/ductile multilayered composites under interface constraint effect10.1016/j.ijplas.2016.11.005 ↗
25. Regulating crack propagation in laminated metal matrix composites through architectural control10.1016/j.compositesb.2019.107503 ↗
26. Microstructure evolution and bending fracture mechanism of as-rolled gradient-laminated network titanium matrix composites10.1016/j.matchar.2024.113976 ↗
27. Effect of layer sequence on the mechanical properties of Ti/TiAl laminates10.1016/j.matdes.2018.02.003 ↗
28. Improved impact toughness of laminate heterogeneous AZ31/GW103K alloys by interface delamination10.1016/j.msea.2023.144882 ↗
29. The interfacial microstructure and fracture toughness of W/Ta multilayer composites10.1016/j.msea.2021.142272 ↗
30. Unravelling the competitive effect of microstructural features on the fracture toughness and tensile properties of near beta titanium alloys10.1016/j.jmst.2021.04.032 ↗
31. Formation of heterogeneous interfaces in the TiAl/Ti2AlNb layered composite and its effect on the fracture toughness10.1016/j.jmst.2024.02.064 ↗
32. Biomimetic micro-laminated structure endows cermet with excellent strength and toughness using CoCrCuFeNi as infiltration layers10.1016/j.ceramint.2023.09.201 ↗
33. Hierarchically enhanced impact resistance of bioinspired composites10.1002/adma.201700060 ↗
34. Bažant · 1997
35. Bio-inspired design of SiCf-reinforced multi-layered Ti-intermetallic composite10.1016/j.matdes.2016.03.138 ↗
36. Electron beam powder bed fusion of Y2O3/γ-TiAl nanocomposite with balanced strength and toughness
37. Simultaneously achieving high tensile strength and fracture toughness of Ti/Ti-Al multilayered composites10.1016/j.intermet.2017.06.007 ↗
38. Simultaneous enhancements of strength, ductility, and toughness in a TiB reinforced titanium matrix composite10.1016/j.actamat.2023.118995 ↗
39. Interfacial characteristics and mechanical properties of TiAl/Ti6Al4V laminate composite (LMC) fabricated by vacuum hot pressing10.1016/j.msea.2018.07.086 ↗
40. Enhanced tensile strength and fracture toughness of a Ti-TiAl metal-intermetallic laminate (MIL) composite10.1016/j.intermet.2019.106684 ↗
41. Fracture mechanism of a high tensile strength and fracture toughness Ti6Al4V–TiAl laminated composite10.1016/j.jallcom.2019.153088 ↗
42. Synthesis and mechanical properties of innovative (TiB/Ti)-Ti3Al micro-laminated composites10.1016/j.jallcom.2017.01.047 ↗
43. Microstructure and mechanical properties of bimodal heterogeneous TiBw/TC4 composites with high strength and toughness10.1016/j.msea.2025.147908 ↗
44. Making ultrastrong steel tough by grain-boundary delamination10.1126/science.aba9413 ↗
45. Tensile and bending behaviors and characteristics of laminated Ti-(TiBw/Ti) composites with different interface status10.1016/j.compositesb.2016.10.001 ↗
46. On macroscopic and microscopic analyses for crack initiation and crack growth toughness in ductile alloys10.1007/BF02815305 ↗
47. Impact toughness improvement of high-strength aluminium alloy by intrinsic and extrinsic fracture mechanisms via hot roll bonding10.1016/j.scriptamat.2009.04.030 ↗
48. Crack deflection at an interface between dissimilar elastic materials: role of residual stresses10.1016/0020-7683(94)90025-6 ↗
49. Crack point stress singularities at a Bi-Material interface10.1115/1.3630064 ↗
50. Edge-bonded dissimilar orthogonal elastic wedges under normal and shear loading10.1115/1.3601236 ↗
51. Orthotropy rescaling and implications for fracture in composites10.1016/0020-7683(91)90208-W ↗
52. Energy criterion for crack deflection at an interface between two orthotropic media10.1016/0022-5096(94)90034-5 ↗
53. Mathematical analysis in the mechanics of fracture
54. 3D printing of biomimetic composites with improved fracture toughness10.1016/j.actamat.2019.04.052 ↗
55. Developing a low-alloyed fine-grained Mg alloy with high strength-ductility based on dislocation evolution and grain boundary segregation10.1016/j.scriptamat.2021.114414 ↗
56. Plastic slip mechanisms in high-temperature titanium alloys: insights into silicide and Ti3Al precipitates on ductility10.1016/j.scriptamat.2024.116412 ↗
57. Deformation mechanism of bimodal microstructure in Ti-6Al-4V alloy: the effects of intercritical annealing temperature and constituent hardness10.1016/j.jmst.2020.08.057 ↗
58. Theory of dislocations10.1016/0502-8205(49)90004-0 ↗
59. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
60. Indentation size effects in crystalline materials: a law for strain gradient plasticity10.1016/S0022-5096(97)00086-0 ↗
61. Geometrically necessary dislocations and strain-gradient plasticity: a few critical issues10.1016/S1359-6462(02)00335-4 ↗
62. Inhomogeneity effects on the crack driving force in elastic and elastic–plastic materials10.1016/S0022-5096(02)00025-X ↗