journal article·2025-12

Revealing the activation energies for H desorption from spherical semi-coherent and incoherent V4C3 precipitates in martensitic medium-Mn steel

Jin-Young Lee, Minjeong Kim, Hyun-Bin Jeong, Won Hui Jo, Jae Bok Seol, Changhun Kim, Donghwa Lee, Young-Kook Lee

Acta Materialia· Volume 301
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (96)

Show source-provided references
1. Medium-Mn steels for hot forming application in the automotive industry10.1007/s12613-020-2179-9 ↗
2. Investigation on microstructure and martensitic transformation mechanism for the warm-stamped third-generation automotive medium-Mn steel10.1115/1.4037017 ↗
3. An introduction to medium-Mn steel: metallurgy, mechanical properties and warm stamping process10.1016/j.matdes.2016.01.048 ↗
4. The effect of process temperatures on the microstructure and tensile properties of warm-stamped Nb-bearing medium-Mn steel10.1007/s11661-019-05570-w ↗
5. Design of high strength medium-Mn steel using machine learning10.1016/j.msea.2022.143148 ↗
6. Inverse design of high-strength medium-Mn steel using a machine learning-aided genetic algorithm approach10.1016/j.jmrt.2024.09.237 ↗
7. A comparative study of query strategies in Pareto active learning for heat treatment optimization of medium-Mn steel10.1016/j.jmrt.2025.06.157 ↗
8. Effect of reverted austenite fraction on hydrogen embrittlement of TRIP-aided medium Mn steel (0.1C-5Mn)10.1016/j.engfailanal.2019.01.018 ↗
9. Enhancing hydrogen embrittlement resistance of lath martensite by introducing nano-films of interlath austenite10.1007/s11661-015-3009-y ↗
10. Hydrogen embrittlement behavior of high strength low carbon medium manganese steel under different heat treatments10.1016/j.ijhydene.2019.10.103 ↗
11. Hydrogen absorption and embrittlement of martensitic medium-Mn steels10.1016/j.corsci.2023.111304 ↗
12. Hydrogen desorption mechanism associated with ε carbide decomposition in martensitic medium-Mn steel10.1016/j.jmrt.2025.07.082 ↗
13. Effects of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
14. Hydrogen trapping behavior in vanadium-added steel10.2355/isijinternational.43.527 ↗
15. Effect of tempering duration on hydrogen embrittlement of vanadium-added tempered martensitic steel10.1016/j.ijhydene.2021.03.109 ↗
16. Effect of Ti alloying on the resistance to hydrogen embrittlement in (Nb+Mo)-alloyed ultra-high-strength hot-stamping steels
17. Hydrogen trapping by TiC particles in iron10.1016/0001-6160(84)90210-4 ↗
18. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
19. Effects of alloying elements and microstructure on the susceptibility of welded HSLA steel to hydrogen-induced cracking and sulfide stress cracking10.1016/j.msea.2008.11.064 ↗
20. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
21. Thermal desorption spectroscopy evaluation of hydrogen trapping capacity of NbC and NbN precipitates10.1007/s11661-013-2181-1 ↗
22. M4C3 precipitation in Fe-C-Mo-V steels and relationship to hydrogen trapping10.1098/rspa.2006.1688 ↗
23. Influence of vanadium on the hydrogen embrittlement of aluminized ultra-high strength press hardening steel10.1016/j.msea.2018.08.027 ↗
24. Role of vanadium carbide in hydrogen embrittlement of press-hardened steels: strategy from 1500 to 2000MPa10.3389/fmats.2020.611390 ↗
25. Direct observation of hydrogen-trapping sites in vanadium carbide precipitation steel by atom probe tomography10.1016/j.scriptamat.2012.04.022 ↗
26. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
27. Hydrogen trapping and embrittlement of titanium- and vanadium carbide-containing steels after high-temperature hydrogen charging10.1007/s10853-024-09611-7 ↗
28. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
29. Thermal desorption analysis of hydrogen in high strength martensitic steels10.1007/s11661-011-0909-3 ↗
30. First - principles study of hydrogen - carbide interaction in bcc Fe10.1016/j.ijhydene.2023.09.222 ↗
31. Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel10.1016/j.actamat.2018.05.003 ↗
32. Somerday · 2009
33. Effects of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
34. Hydrogen absorption of incoherent TiC particles in iron from environment at high temperatures10.1007/s11661-004-0060-5 ↗
35. Qualification of the tomographic reconstruction in atom probe by advanced spatial distribution map techniques10.1016/j.ultramic.2009.03.016 ↗
36. On the microstructural evolution and partitioning behavior of L12-structured γ′-based Co-Ti-W alloys upon Cr and Al alloying10.1016/j.intermet.2018.10.027 ↗
37. On the stacking fault forming probability and stacking fault energy in carbon-doped 17 at% Mn steels via transmission electron microscopy and atom probe tomography10.1016/j.jmst.2021.11.027 ↗
38. Elements of X-ray diffraction10.1063/1.3060306 ↗
39. Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel10.1016/j.actamat.2012.04.010 ↗
40. Kiuchi · 1986 · 29
41. The effect of pre-strain on the resistance to hydrogen embrittlement in 316L austenitic stainless steel10.2320/matertrans.M2014036 ↗
42. The use of silver decoration technique in the study of hydrogen transport in metallic materials10.1007/BF02671932 ↗
43. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
44. From ultrasoft pseudopotentials to the projector augmented-wave method10.1103/PhysRevB.59.1758 ↗
45. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
46. Special points for Brillouin-zone integrations10.1103/PhysRevB.13.5188 ↗
47. High-precision sampling for Brillouin-zone integration in metals10.1103/PhysRevB.40.3616 ↗
48. Atomistic insight into hydrogen trapping at MC/BCC-Fe phase boundaries: the role of local atomic environment10.1016/j.actamat.2021.116744 ↗
49. Synergistic effects of Ta and Mo on the hydrogen embrittlement resistance in ultra-high strength hot stamping steel10.1016/j.msea.2023.144956 ↗
50. First-principles investigation of hydrogen interaction with TiC precipitates in α-Fe10.1103/PhysRevB.93.184108 ↗
51. Hydrogen trapping and storage in the group IVB-VIB transition metal carbides10.1016/j.matdes.2022.110399 ↗
52. Hydrogen trapping, desorption and clustering in heterophase interfaces of W-ZrC alloy10.1016/j.actamat.2022.118469 ↗
53. Nitrogen determination by SEM-EDS and elemental analysis10.1002/xrs.2490 ↗
54. Quantitative analysis of carbon in carbon steel using SEM/EDS followed by error correction approach10.1017/S143192761300723X ↗
55. H. Bhadeshia, R. Honeycombe, Steels: microstructure and properties, Butterworth-Heinemann, 2017.10.1016/B978-0-08-100270-4.00013-5 ↗
56. Ultralow-temperature superplasticity of high strength Fe–10Mn-3.5 Si steel10.1016/j.msea.2022.143408 ↗
57. A nano-twinned structure and tensile properties of a thermally cycled Fe-17Mn alloy10.1016/j.jallcom.2023.171466 ↗
58. The effect of silicon, vanadium and nitrogen on the microstructure and hardness of air cooled medium carbon low alloy steels10.1016/S0924-0136(02)01131-7 ↗
59. Precipitation processes in steels
60. On coherent carbonitride precipitation in commercial microalloyed steels10.1080/0950083021000056632 ↗
61. Processes, microstructure and properties of vanadium microalloyed steels10.1179/174328409X453253 ↗
62. Precipitation hardening of a FeMnC TWIP steel by vanadium carbides
63. Quantitative analysis of carbon in cementite using pulsed laser atom probe10.1016/j.ultramic.2014.06.004 ↗
64. Quantitative atom probe analysis of carbides10.1016/j.ultramic.2010.12.024 ↗
65. Quantitative measurement of carbon content in Fe–C binary alloys by atom probe tomography10.1016/j.scriptamat.2012.09.007 ↗
66. Quantitative analysis of carbon content in cementite in steel by atom probe tomography10.1016/j.ultramic.2011.03.024 ↗
67. Hydrogen trapping in quenched and tempered 0.42C-0.30Ti steel containing bimodally dispersed TiC particles10.2355/isijinternational.43.539 ↗
68. Baking effect on desorption of diffusible hydrogen and hydrogen embrittlement on hot-stamped boron martensitic steel10.3390/met9060636 ↗
69. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
70. Commentary: the Materials Project: a materials genome approach to accelerating materials innovation10.1063/1.4812323 ↗
71. Vanadium carbide coating as hydrogen permeation barrier: a DFT study10.1016/j.ijhydene.2019.01.049 ↗
72. First-principles study of hydrogen trapping and diffusion mechanisms in vanadium carbide with connecting carbon vacancies10.1016/j.ijhydene.2024.10.150 ↗
73. Di Stefano · 2016
74. Numerical analysis of hydrogen trap State by TiC and V4C3 in bcc-Fe10.2355/isijinternational.52.1693 ↗
75. Effect of titanium and vanadium nano-carbide size on hydrogen embrittlement of ferritic steels10.1038/s41529-024-00546-7 ↗
76. The determination of the elastic field of an ellipsoidal inclusion, and related problems
77. Mechanics of the hydrogen-dislocation-impurity interactions—I. Increasing shear modulus10.1016/0022-5096(94)00056-B ↗
78. Hydrogen-enhanced localized plasticity—A mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
79. ASM Handbook, vol. 1, properties and selection: irons, steels, and high performance alloys section: carbon and low-alloy steels
80. Elastic properties of metals and alloys, I. Iron, nickel, and iron-nickel alloys10.1063/1.3253127 ↗
81. The atomistic structure of metal/ceramic interfaces is the key issue for developing better properties10.3390/met4030410 ↗
82. On the evolution of stresses due to lattice misfit at a Ni-superalloy and YSZ interface10.1016/j.surfin.2018.05.007 ↗
83. Low-temperature superionic conductivity in strained yttria-stabilized zirconia10.1002/adfm.201000071 ↗
84. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
85. Turnbull · 2012 · 89
86. Generalised boundary conditions for hydrogen transport at crack tips10.1016/j.corsci.2020.108698 ↗
87. Analysis of hydrogen diffusion in the three stage electro-permeation test10.1007/s00161-023-01237-5 ↗
88. Numerical simulation of hydrogen permeation in steels10.1016/j.electacta.2018.03.061 ↗
89. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
90. Structurally complex phase engineering enables hydrogen-tolerant Al alloys10.1038/s41586-025-08879-2 ↗
91. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
92. Hydrogen-induced superabundant vacancy formation in bcc Fe: monte Carlo simulation10.1016/j.actamat.2013.12.041 ↗
93. Effect of temperature on fast hydrogen diffusion in iron: a path-integral quantum dynamics approach10.1103/PhysRevB.83.094110 ↗
94. Effect of hydrogen on the electronic structure of a grain boundary in iron10.1016/0038-1098(91)90072-4 ↗
95. The deformation of plastically non-homogeneous materials10.1080/14786437008238426 ↗
96. The key role played by dislocation core radius and energy in hydrogen interaction with dislocations10.1016/j.actamat.2019.12.033 ↗