Damage and self-healing mechanisms of 2D SiCf/SiC composites during high-temperature low-cycle fatigue in air: A combined in-situ acoustic emission and microscopy study
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Mechanical Behavior of Composites · Thermal properties of materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Long-term ceramic matrix composite for aeroengine10.1007/s40145-022-0611-5 ↗
2. Micromechanical properties and microstructural evolution of amosic-3 SiC/SiC composites irradiated by silicon ions10.1016/j.jeurceramsoc.2020.02.023 ↗
3. Microstructure response of amosic-3 SiC/SiC composites under self-ion irradiation10.1016/j.jeurceramsoc.2021.11.032 ↗
4. In-situ TEM investigations on the microstructural evolution of SiC fibers under ion irradiation: amorphization and grain growth10.1016/j.jeurceramsoc.2022.11.029 ↗
5. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
6. An investigation of fatigue failures of turbine blades in a gas turbine engine by mechanical analysis10.1016/S1350-6307(01)00005-X ↗
7. Design and life prediction issues for high-temperature engineering ceramics and their composites10.1016/S1359-6454(96)00143-7 ↗
8. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: I, an experimental approach10.1111/j.1151-2916.1994.tb07015.x ↗
9. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: II, modeling10.1111/j.1151-2916.1994.tb07016.x ↗
10. Oxidation of SiC/BN/SiC ceramic matrix composites in dry and wet oxygen at intermediate temperatures10.1016/j.jeurceramsoc.2022.04.003 ↗
11. Mechanical properties and microstructural evolution of Cansas-III SiC fibers after thermal exposure in different atmospheres10.1016/j.ceramint.2022.07.206 ↗
12. Wilson · 2018
13. Oxidation behavior of 3D SiCf/SiBCN composites at 800–1200 °C10.1016/j.jeurceramsoc.2020.08.057 ↗
14. Effects of fiber architecture on matrix cracking for melt-infiltrated SiC/SiC composites10.1111/j.1744-7402.2009.02422.x ↗
15. Fatigue of ceramic matrix composites10.1016/0956-7151(94)00304-Z ↗
16. Cyclic fatigue of ceramic-matrix composites at ambient and elevated temperatures10.1016/0266-3538(96)00025-5 ↗
17. Fatigue behavior of an advanced SiC/SiC ceramic composite with a self-healing matrix at 1300 °C in air and in steam10.1016/j.msea.2016.09.076 ↗
18. Cyclic-fatigue behavior of SiC/SiC composites at room and high temperatures10.1111/j.1151-2916.1996.tb08078.x ↗
19. Multiscale investigation on fatigue properties and damage of a 3D braided SiC/SiC + PyC/SiC composites in the full stress range at 1300 °C10.1016/j.jeurceramsoc.2021.11.045 ↗
20. Research progress on in-situ monitoring of damage behavior of SiCf/SiC ceramic matrix composites at high temperature environments
21. Stress-dependent matrix cracking in 2D woven SiC-fiber reinforced meltinfiltrated SiC matrix composites10.1016/j.compscitech.2003.10.022 ↗
22. In-plane cracking behavior and ultimate strength for 2D woven and braided melt-infiltrated SiC/SiC composites tensile loaded in off-axis fiber directions10.1111/j.1551-2916.2007.01887.x ↗
23. Microscale characterization of damage accumulation in CMCs10.1016/j.jeurceramsoc.2020.05.077 ↗
24. Unsupervised and supervised classification of AE data collected during fatigue test on CMC at high temperature10.1016/j.compositesa.2011.10.016 ↗
25. The anti-oxidation mechanism of SiCf/SiC-B4C modified with Al2O3 in wet atmosphere based on machine learning10.1111/jace.18525 ↗
26. Analysis of acoustic emission energy release during static fatigue tests at intermediate temperatures on ceramic matrix composites: towards rupture time prediction10.1016/j.compscitech.2012.03.011 ↗
27. Challenges and limitations in the identification of acoustic emission signature of damage mechanisms in composites materials10.3390/app8081267 ↗
28. Acoustic emission and lifetime prediction during static fatigue tests on ceramic-matrix-composite at high temperature under air10.1016/j.compositesa.2010.03.008 ↗
29. Damage mechanism identification and failure behavior of 2D needle-punched SiCf/SiC composites based on acoustic emission and digital image correlation10.1016/j.matchar.2024.114491 ↗
30. A methodology to measure the interface shear strength by means of the fiber push-in test10.1016/j.compscitech.2012.08.011 ↗
31. Analysis of damage mechanisms and associated acoustic emission in two SiC/[Si–B–C] composites exhibiting different tensile behaviours. Part I: damage patterns and acoustic emission activity10.1016/j.compscitech.2007.12.001 ↗
32. Analysis of damage mechanisms and associated acoustic emission in two SiCf/[Si–B–C] composites exhibiting different tensile behaviours. Part II: unsupervised acoustic emission data clustering10.1016/j.compscitech.2007.12.002 ↗
33. The tensile damage behavior of SiCf/SiC-B4C after oxidation in wet atmosphere based on acoustic emission pattern recognition10.1111/jace.17816 ↗
34. Effects of CVI SiC amount and deposition rates on properties of SiCf/SiC composites fabricated by hybrid chemical vapor infiltration (CVI) and precursor infiltration and pyrolysis (PIP) routes10.1016/j.ceramint.2021.06.110 ↗
35. Effects of interfacial residual stress on mechanical behavior of SiCf/SiC composites10.1007/s40145-021-0519-5 ↗
36. Thermal properties of SiOC glasses and glass ceramics at elevated temperatures10.3390/ma11020279 ↗
37. Damage monitoring and identification in SiC/SiC minicomposites using combined acousto-ultrasonics and acoustic emission10.1016/j.compositesa.2013.10.010 ↗
38. A machine learning framework for damage mechanism identification from acoustic emissions in unidirectional SiC/SiC composites
39. Use of acoustic emission for ceramic matrix composites
40. Matrix cracking onset stress and strain as a function of temperature, and characterisation of damage modes in SiCf/SiC ceramic matrix composites via acoustic emission10.1016/j.jeurceramsoc.2022.10.042 ↗
41. Grosse · 2022
42. Life assessment of thermomechanical fatigue in a woven SiC/SiC ceramic matrix composite with an environmental barrier coating at elevated temperature10.1016/j.ijfatigue.2023.107584 ↗
43. Fatigue of three advanced SiC/SiC ceramic matrix composites at 1200 °C in air and in steam10.1111/ijac.12773 ↗
44. Tensile creep and fatigue of Sylramic-iBN melt-infiltrated SiC matrix composites: retained properties, damage development, and failure mechanisms10.1016/j.compscitech.2008.08.028 ↗
45. Cyclic fatigue behaviour at high temperature of a selfhealing ceramic matrix composite10.3166/acsm.30.649-658 ↗
46. Fatigue behavior of a Hi-Nicalon™/SiC-B4C composite at 1200 °C in air and in steam10.1016/j.msea.2011.11.049 ↗
47. Fatigue behavior at high temperature in air of a 2D woven SiC/SiBC with a self healing matrix
48. Creep and fatigue behavior in Hi-Nicalon-fiber-reinforced silicon carbide composites at high temperatures10.1111/j.1151-2916.1999.tb01731.x ↗
49. Creep of SiC–SiC microcomposites10.1016/S0955-2219(99)00118-1 ↗
50. Creep behavior and failure mechanisms of CVI and PIP SiC/SiC composites at temperatures to 1650 °C in air10.1016/j.jeurceramsoc.2021.05.059 ↗
51. A novel creep-fatigue life evaluation method for ceramic-composites components10.1016/j.ijmecsci.2023.108259 ↗
52. Stress-dependence and time-dependence of the post-fatigue tensile behavior of carbon fiber reinforced SiC matrix composites10.1016/j.compscitech.2011.05.013 ↗
53. Creep and stress–strain behavior after creep for SiC fiber reinforced, melt-infiltrated SiC matrix composites10.1111/j.1551-2916.2006.00939.x ↗
54. Oxidation under stress of SiC-based fibers at intermediate temperature and ambient air10.1111/jace.19979 ↗
55. A review of SiC fiber oxidation with a new study of Hi-nicalon SiC fiber oxidation10.1002/adem.201600166 ↗
56. Observations of fatigue damage process in SiC/SiC composites at room and elevated temperatures10.1016/S0142-1123(01)00078-0 ↗
57. Kinetics of carbothermal reduction synthesis of beta silicon carbide10.1002/aic.690390311 ↗
58. Crystallization maps for SiCO amorphous ceramics10.1111/j.1551-2916.2006.01423.x ↗
59. Crystallization behavior of polymerderived Si-O-C for ceramic matrix composite processing10.1016/j.actamat.2018.01.052 ↗
60. Anderson · 2017
61. Further understanding of the improved mechanical properties for SiCf/BN/SiC composites prepared by CVI+PIP hybrid technique: application of micro-mechanical methods10.1016/j.compositesb.2024.111633 ↗
62. Effect of frequency and environment on fatigue behavior of a CVI SiC/SiC ceramic matrix composite at 1200 °C10.1016/j.compscitech.2010.11.008 ↗
63. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
64. The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
65. Reducing the self-healing temperature of Ti2AlC MAX phase coating by substituting Al with Sn10.1016/j.jeurceramsoc.2019.09.009 ↗
66. Preparation of self-healing Cf/SiBCN(O) composite using a novel polyborosilazane10.1016/j.ceramint.2022.07.100 ↗
67. Monotonic tension, fatigue and creep behavior of SiC-fiber-reinforced SiC-matrix composites: a review10.1016/S0266-3538(99)00014-7 ↗