journal article·2024-05Open access

Mechanisms of structural evolution of laminates with immiscible components under high-pressure torsion

A. Mazilkin, V. Tavakkoli, O. Davydenko, Y. Beygelzimer, E. Boltynjuk, T. Boll, B. Straumal, B. Baretzky, Y. Estrin, R. Kulagin

Acta Materialia· Volume 269

Abstract

The mechanism of structural evolution of a three-layer Cu-Mo-Cu laminate under high-pressure torsion (HPT) was studied using scanning and transmission electron microscopy, atom probe tomography, and nanoindentation, complemented with finite element calculations. The results demonstrate a gradual refinement of the structure of the Mo component; a greater degree of refinement is observed in the peripheral part of the disk-shaped HPT specimen, although some heterogeneity of the structure remains even at a gigantic degree of shear deformation accumulated therein. The elemental distribution calculated from STEM-EDX mapping as well as 3D reconstruction of atom probe tomography results shows a significant degree of mixing of the sample components at the atomic level, the concentration of copper in molybdenum and molybdenum in copper reaching ∼4.3 at.% and ∼6 at.%., respectively. These observations correlate with nanoindentation results showing an increase in the hardness of both phases due to strain hardening and solid solution strengthening, as well as grain refinement. Numerical simulations made it possible to provide a detailed description of the stages of the structure fragmentation, including its self-organizing nature, to show the formation of rupture forerunners in the hard Mo layer, and the deformation of harder fragments in a softer matrix. The experimental results are supported by a model assuming a fractal self-organization of a self-similar structure during HPT processing.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and mechanical properties · Advanced materials and composites · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (90)

Show source-provided references
1. Phase transitions during high pressure torsion of CuCo alloys10.1016/j.matlet.2013.12.042 ↗
2. The significance of self-annealing at room temperature in high purity copper processed by high-pressure torsion10.1016/j.msea.2016.01.027 ↗
3. Microstructures and mechanical properties of pure copper deformed severely by equal-channel angular pressing and high pressure torsion10.1016/j.msea.2007.05.083 ↗
4. Evolution of defects in copper deformed by high-pressure torsion10.1016/j.actamat.2010.12.028 ↗
5. Grain-size effect on the deformation mechanisms of nanostructured copper processed by high-pressure torsion10.1063/1.1757035 ↗
6. Effect of severe plastic deformation on the coercivity of Co–Cu alloys10.1080/09500830903246268 ↗
7. Effect of processing route on grain refinement in pure copper processed by equal channel angular extrusion10.1016/S1003-6326(16)64286-3 ↗
8. Twist extrusion as a potent tool for obtaining advanced engineering materials: a review10.1002/adem.201600873 ↗
9. Planar Twist Extrusion versus Twist Extrusion10.1016/j.jmatprotec.2010.11.006 ↗
10. Production of nanostructure copper by planar twist channel angular extrusion process10.1016/j.jallcom.2016.05.012 ↗
11. Effect of equal channel angular pressing on the thermal-annealing-induced microstructure and texture evolution of cold-rolled copper10.1016/j.msea.2016.07.050 ↗
12. Microstructural inhomogeneity in constrained groove pressed Cu-Zn alloy sheet10.1007/s11665-016-2142-0 ↗
13. Effect of high-pressure torsion on grain refinement, strength enhancement and uniform ductility of EZ magnesium alloy10.1016/j.matlet.2017.10.113 ↗
14. Influence of equal channel angular pressing in an acute angle die with a back pressure notch on grain refinement, torsion and mechanical properties of aluminium10.1002/mawe.201700102 ↗
15. Instabilities of interfaces between dissimilar metals induced by high pressure torsion10.1016/j.matlet.2018.03.200 ↗
16. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
17. Improvement of strength and ductility of an EZ magnesium alloy by applying two different ECAP concepts to processable initial states10.1016/j.msea.2018.09.070 ↗
18. Structure and mechanical and corrosion properties of a magnesium Mg–Y–Nd–Zr alloy after high pressure torsion10.1134/S0036029517110088 ↗
19. An investigation of the limits of grain refinement after processing by a combination of severe plastic deformation techniques: a comparison of Al and Mg alloys10.1016/j.msea.2017.11.090 ↗
20. An EBSD analysis of Fe-36 %Ni alloy processed by HPT at ambient and a warm temperature10.1016/j.jallcom.2018.04.194 ↗
21. Direct influence of recovery behaviour on mechanical properties in oxygen-free copper processed using different SPD techniques: HPT and ECAP10.1016/j.jmrt.2017.05.005 ↗
22. Structure Refinement and Fragmentation of Precipitates under Severe Plastic Deformation: a Review10.3390/ma15020601 ↗
23. Microstructural and texture evolution of copper-(chromium, molybdenum, tungsten) composites deformed by high-pressure-torsion10.1016/j.ijrmhm.2018.04.008 ↗
24. High-pressure torsion for pure chromium and niobium10.2320/matertrans.MD201131 ↗
25. Influence of dislocation-solute atom interactions and stacking fault energy on grain size of single-phase alloys after severe plastic deformation using high-pressure torsion10.1016/j.actamat.2014.01.036 ↗
26. High-pressure torsion of iron with various purity levels and validation of Hall-Petch strengthening mechanism10.1016/j.msea.2018.11.127 ↗
27. Strengthening of A2024 alloy by high-pressure torsion and subsequent aging10.1016/j.msea.2017.07.083 ↗
28. Activation of titanium-vanadium alloy for hydrogen storage by introduction of nanograins and edge dislocations using high-pressure torsion10.1016/j.ijhydene.2016.03.146 ↗
29. Microstructural evolution and mechanical properties of biomedical Co–Cr–Mo alloy subjected to high-pressure torsion10.1016/j.jmbbm.2015.11.015 ↗
30. Grain refinement mechanism and evolution of dislocation structure of Co–Cr–Mo alloy subjected to high-pressure torsion10.2320/matertrans.M2016052 ↗
31. High-pressure torsion of palladium: hydrogen-induced softening and plasticity in ultrafine grains and hydrogen-induced hardening and embrittlement in coarse grains10.1016/j.msea.2014.08.074 ↗
32. Equal-channel angular pressing and high-pressure torsion of pure copper: evolution of electrical conductivity and hardness with strain10.2320/matertrans.MD201109 ↗
33. Evaluating the textural and mechanical properties of an Mg-Dy alloy processed by high-pressure torsion10.1016/j.jallcom.2018.11.109 ↗
34. Texture and microhardness of Mg-Rare Earth (Nd and Ce) alloys processed by high-pressure torsion10.1016/j.msea.2018.03.114 ↗
35. Enhanced grain refinement and microhardness by hybrid processing using hydrostatic extrusion and high-pressure torsion10.1016/j.msea.2017.12.007 ↗
36. Orientation imaging microscopy and microhardness in a ZK60 magnesium alloy processed by high-pressure torsion10.1016/j.jallcom.2017.04.054 ↗
37. Effects on hardness and microstructure of AISI 1020 low-carbon steel processed by high-pressure torsion10.1016/j.jmrt.2017.05.002 ↗
38. Effect of high pressure torsion on microstructure of Cu-Sn alloys with different content of Hume Rothery phase10.1016/j.matchar.2016.06.019 ↗
39. Competition between precipitation and dissolution in Cu–Ag alloys under high pressure torsion10.1016/j.actamat.2016.09.024 ↗
40. Phase transitions in copper–silver alloys under high pressure torsion10.3139/146.111784 ↗
41. High pressure torsion of Cu–Ag and Cu–Sn alloys: limits for solubility and dissolution10.1016/j.actamat.2020.05.055 ↗
42. Formation of a W-25% Cu nanocomposite during high pressure torsion10.1016/j.scriptamat.2005.02.017 ↗
43. Microstructure and thermostability of a W–Cu nanocomposite produced via high-pressure torsion10.1080/14786435.2012.704426 ↗
44. Characterization of tungsten fragmentation in a W–25%Cu composite after high-pressure torsion10.1016/j.matchar.2006.08.001 ↗
45. On the process of co-deformation and phase dissolution in a hard-soft immiscible Cu Co alloy system during high-pressure torsion deformation10.1016/j.actamat.2016.06.010 ↗
46. Structural evolution and strain induced mixing in Cu–Co composites studied by transmission electron microscopy and atom probe tomography10.1016/j.matchar.2014.12.022 ↗
47. New insights on the formation of supersaturated solid solutions in the Cu–Cr system deformed by high-pressure torsion10.1016/j.actamat.2014.02.003 ↗
48. Microstructure and failure characteristics of nanostructured molybdenum–copper composites10.1002/adem.201900474 ↗
49. On nanostructured molybdenum–copper composites produced by high-pressure torsion10.1007/s10853-017-1142-2 ↗
50. Structural characteristics of Cu/Ti bimetal composite produced by accumulative roll-bonding (ARB)10.1016/j.matdes.2016.09.094 ↗
51. The mechanism of formation of nanostructure and dissolution of cementite in a pearlitic steel during high pressure torsion10.1016/S1359-6454(03)00419-1 ↗
52. Annealing behaviour of nanostructured carbon steel produced by severe plastic deformation10.1016/S1359-6462(03)00478-0 ↗
53. Microstructure and mechanical properties of UFG medium carbon steel processed by HPT at increased temperature10.1007/s10853-010-4482-8 ↗
54. Characterization of ultra-fine grained steel samples produced by high pressure torsion via magnetic Barkhausen noise analysis10.1016/j.msea.2009.09.006 ↗
55. Tensile properties and work hardening behaviors of ultrafine grained carbon steel and pure iron processed by warm high pressure torsion10.1016/j.msea.2013.05.008 ↗
56. Tensile property of submicrocrystalline pure Fe produced by HPT-straining10.4028/www.scientific.net/MSF.584-586.597 ↗
57. Formation of fine cementite precipitates in an ultra-fine grained low carbon steel10.1016/S1359-6462(02)00512-2 ↗
58. Structural refinement of low alloyed steels during severe plastic deformation10.1016/j.msea.2004.01.096 ↗
59. Bulk nanocrystalline ferrite stabilized through grain boundary carbon segregation10.1002/adem.201800443 ↗
60. Strengthening via microstructure refinement in bulk Al-4 mass% Fe alloy using high-pressure torsion10.2320/matertrans.MD201127 ↗
61. Mechanical alloying of the immiscible system W-Cu10.1016/0965-9773(95)00082-8 ↗
62. Structural study of nanocrystalline solid solution of Cu–Mo obtained by mechanical alloying10.1016/j.msea.2012.03.105 ↗
63. Nanocrystalline formation in immiscible Cu-Mo system subjected to mechanical alloying10.1166/jnn.2007.069 ↗
64. Effects of ternary alloy additions on the microstructure of highly immiscible Cu alloys subjected to severe plastic deformation: an evaluation of the effective temperature model10.1016/j.actamat.2019.03.023 ↗
65. Mixing instabilities during shearing of metals10.1038/s41467-017-01879-5 ↗
66. Pattern formation during deformation of metallic nanolaminates
67. Instability of a molybdenum layer under deformation of a CuMoCu laminate by high-pressure torsion10.1016/j.matlet.2021.130378 ↗
68. Folding in metal polycrystals: microstructural origins and mechanics10.1016/j.actamat.2017.08.018 ↗
69. Non-Newtonian Fluids: an Introduction
70. QForm, (n.d.) https://www.qform3d.com/.
71. Plastic deformation of polycrystalline molybdenum: experimental data and macroscopic model accounting for its anisotropy and tension–compression asymmetry10.1016/j.ijsolstr.2015.08.021 ↗
72. The Cu-Mo (Copper-Molybdenum) system10.1007/BF02841703 ↗
73. Composite materials: science and engineering, third edition
74. Gripping prospective of non-shear flows under high-pressure torsion10.3390/ma16020823 ↗
75. Kachanov · 2004
76. 1978
77. The thick yield surface: idea and approach for investigating its structure10.1080/01418619908214293 ↗
78. Models for ductile damage and fracture prediction in cold bulk metal forming processes: a review10.1007/s12289-015-1262-7 ↗
79. Bridgman · 1964
80. Grain refinement versus voids accumulation during severe plastic deformations of polycrystals: mathematical simulation10.1016/j.mechmat.2004.07.006 ↗
81. Second paper on statistics associated with the random disorientation of cubes10.1093/biomet/45.1-2.229 ↗
82. On the lognormal distribution law for particle sizes on crushing
83. M.A. Meyers, K.K. Chawla, M.A. Meyers, K. Kumar, C. Frontmatter, Mechanical behavior of materials-mechanical behavior of materials more information, (n.d.). www.cambridge.org (accessed November 15, 2023).
84. Nano-indentation nanohardness and elastic modulus evolution of molybdenum processed by high-pressure torsion10.1080/02670836.2020.1740863 ↗
85. Microstructures and mechanical properties of pure V and Mo processed by high-pressure torsion10.2320/matertrans.M2009375 ↗
86. Microstructure and microhardness evolution in pure molybdenum processed by high-pressure torsion10.1002/adem.201901022 ↗
87. Evolution of microstructural homogeneity in copper processed by high-pressure torsion10.1016/j.scriptamat.2010.05.030 ↗
88. Effect of high-pressure torsion on hardness and electrical resistivity of commercially pure Cu
89. Evidence for an early softening behavior in pure copper processed by high-pressure torsion10.1007/s10853-015-9499-6 ↗
90. Microstructures and microhardness of an aluminum alloy and pure copper after processing by high-pressure torsion10.1016/j.msea.2005.08.133 ↗