The traditional high-temperature sintering (HTS) hinders the acquisition of solid electrolytes (SEs) pellets with ideal ionic conductivity due to the volatilization of Li, the generation of secondary phases and thermal cracks. Reducing the sintering temperature holds significant importance for densifying oxide SEs and co-sintering SEs with electrode materials. Herein, densified and fine-grained NASICON-type SEs with high ionic conductivity are prepared through cold sintering process (CSP). The Li 1.3Al 0.3Ti 1.7(PO 4) 3 (LATP) pellets prepared at 170 °C via CSP undergo subsequently annealing at 750 °C for 1 h to recrystallize the amorphous phase and promoting grain growth and fusion, thus enhancing mechanical strength and ionic conductivity. The resulting LATP electrolytes show limited grain growth and exhibit relative density of ∼100 % and ionic conductivity in excess of 10 −3 S cm −1 at 25 °C, as well as display superior electrochemical stability in Li symmetric cells. Compare to HTS, the CSP-assisted annealing method is anticipated to enable the low-temperature densification of SEs and the co-sintering of electrode materials with SEs, offering a viable technical solution for advancing the development and application of all-solid-state batteries.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Achieving high-energy and high-safety lithium metal batteries with high-voltage-stable solid electrolytes10.1016/j.matt.2023.02.012 ↗
2. Solid-state batteries: the critical role of mechanics10.1126/science.abg5998 ↗
3. Approaching practically accessible solid-state batteries: stability issues related to solid electrolytes and interfaces10.1021/acs.chemrev.9b00268 ↗
4. Understanding interface stability in solid-state batteries10.1038/s41578-019-0157-5 ↗
5. Critical current density in solid-state lithium metal batteries: mechanism, influences, and strategies10.1002/adfm.202009925 ↗
6. Solid garnet batteries10.1016/j.joule.2019.03.019 ↗
7. Recent advances in Li1+xAlxTi2−x(PO4)3 solid-state electrolyte for safe lithium batteries10.1016/j.ensm.2018.10.012 ↗
8. Perspective on design and technical challenges of Li-garnet solid-state batteries10.1080/14686996.2021.2018919 ↗
9. Inorganic solid-state electrolytes for lithium batteries: mechanisms and properties governing ion conduction10.1021/acs.chemrev.5b00563 ↗
10. Synthesis and properties of NaSICON‐type LATP and LAGP solid electrolytes10.1002/cssc.201900725 ↗
11. Review of ionic conductivity properties of NASICON type inorganic solid electrolyte LATP10.1021/acsaelm.3c01747 ↗
12. Stabilizing the NASICON solid electrolyte in an inert atmosphere as a function of physical properties and sintering conditions for solid-state battery fabrication10.1021/acsaem.2c02464 ↗
13. Development of the cold sintering process and its application in solid-state lithium batteries10.1016/j.jpowsour.2018.05.015 ↗
14. Influence of sintering temperature on conductivity and mechanical behavior of the solid electrolyte LATP10.1016/j.ceramint.2019.04.191 ↗
15. Impact of sintering temperature on phase formation, microstructure, crystallinity and ionic conductivity of Li1.5Al0.5Ti1.5(PO4)310.1016/j.ssi.2019.05.016 ↗
16. Insights into the reactive sintering and separated specific grain/grain boundary conductivities of Li1.3Al0.3Ti1.7(PO4)310.1016/j.jpowsour.2021.229631 ↗
17. Combined quantitative microscopy on the microstructure and phase evolution in Li1.3Al0.3Ti1.7(PO4)3 ceramics10.1007/s40145-019-0354-0 ↗
18. Ceramic–salt composite electrolytes from cold sintering10.1002/adfm.201807872 ↗
19. Cold sintering process of composites: bridging the processing temperature gap of ceramic and polymer materials10.1002/adfm.201602489 ↗
20. Cold sintering-enabled interface engineering of composites for solid-state batteries10.3389/fenrg.2023.1149103 ↗
21. Cold sintering: current status and prospects10.1557/jmr.2017.262 ↗
22. Cold sintering process: a novel technique for low‐temperature ceramic processing of ferroelectrics10.1111/jace.14554 ↗
23. Densification of a NASICON-type LATP electrolyte sheet by a cold-sintering process10.3390/ma14164737 ↗
24. Insight into the microstructure and ionic conductivity of cold sintered NASICON solid electrolyte for solid-state batteries10.1021/acsami.9b08132 ↗
25. Li-ion conductive Li1.3Al0.3Ti1.7(PO4)3 (LATP) solid electrolyte prepared by cold sintering process with various sintering additives10.3390/nano12183178 ↗
26. Cold sintering process of Li1.5Al0.5Ge1.5(PO4)3 solid electrolyte10.1111/jace.14727 ↗
27. Thermally stable ceramic-salt electrolytes for Li metal batteries produced from cold sintering using DMF/water mixture solvents10.3390/nano13172436 ↗
28. Advances in Cold Sintering : improving energy consumption and unlocking new potential in component manufacturing10.1595/205651320X15814150061554 ↗
29. Roadmap for densification in cold sintering: chemical pathways10.1016/j.oceram.2020.100019 ↗
30. Solid-state Li metal battery enabled by cold sintering at 120 °C10.1016/j.mtphys.2021.100476 ↗
31. Microstructure and ionic conductivities of NASICON-type Li1.3Al0.3Ti1.7(PO4)3 solid electrolytes produced by cold sintering assisted process10.1016/j.jallcom.2023.168702 ↗
32. Influence of LiBF4 sintering aid on the microstructure and conductivity of LATP solid electrolyte10.1016/j.ceramint.2021.01.004 ↗
33. Origin of outstanding stability in the lithium solid electrolyte materials: insights from thermodynamic analyses based on first-principles calculations10.1021/acsami.5b07517 ↗
34. Effect of microcracking on ionic conductivity in LATP10.1016/j.jpowsour.2012.06.081 ↗
35. Strengthening Hf0.95Ta0.05B2 ceramic with ultrafine grains and high-density dislocations10.1016/j.jeurceramsoc.2023.05.026 ↗
36. Modeling of an all-solid-state battery with a composite positive electrode10.1016/j.etran.2024.100315 ↗
37. High electronic conductivity as the origin of lithium dendrite formation within solid electrolytes10.1038/s41560-018-0312-z ↗
38. Rational design of hierarchical “ceramic‐in‐polymer” and “polymer‐in‐ceramic” electrolytes for dendrite‐free solid‐state batteries10.1002/aenm.201804004 ↗
39. Interface engineering of Li1.3Al0.3Ti1.7(PO4)3 ceramic electrolyte via multifunctional interfacial layer for all-solid-state lithium batteries10.1016/j.jpowsour.2020.228125 ↗
40. Local electronic structure variation resulting in Li ‘filament’ formation within solid electrolytes10.1038/s41563-021-01019-x ↗
41. Interfaces and interphases in all-solid-state batteries with inorganic solid electrolytes10.1021/acs.chemrev.0c00101 ↗
42. Chemomechanical origins of the dynamic evolution of isolated Li filaments in inorganic solid-state electrolytes10.1021/acs.nanolett.3c03321 ↗
43. Chemomechanical failure mechanism study in NASICON-type Li1.3Al0.3Ti1.7(PO4)3 solid-state lithium batteries10.1021/acs.chemmater.9b05295 ↗
44. Effect of surface microstructure on electrochemical performance of garnet solid electrolytes10.1021/am508111r ↗
45. Field assisted sintering of fine-grained Li7−3xLa3Zr2AlxO12 solid electrolyte and the influence of the microstructure on the electrochemical performance10.1016/j.jpowsour.2016.01.086 ↗