Abstract

Cracks are a common defect in the catalyst layers (CLs) of proton exchange membrane fuel cells (PEMFCs), deteriorating their performance. This study proposes benzoic acid as a cracking inhibitor in the catalyst ink. The additive strengthens the network of catalyst particles by promoting attractive interaction within them. Molecular dynamics simulations demonstrate that the inhibitor facilitates the desorption of ionomer from the Pt/carbon surface, weakening the repulsion force within catalyst particles. Rheology experiments indicate that the addition of benzoic acid transforms the catalyst ink from a sol-like to a gel-like, improving its viscosity and storage modulus. The stronger attractive interactions within the inhibitor-added ink impart anti-cracking ability, preventing stress release during the drying process. Furthermore, optical microscopy reveals a significant decrease in both the crack area and the maximum length of cracks in the CL after incorporating the inhibitor. Specifically, the crack area decreases from 13% to 2%, while the maximum crack length decreases from nearly 400 μm to 150 μm. Single cell tests show that the inhibitor-added sample exhibits a higher peak power density of 0.893 W/cm 2 compared to the standard sample`s 0.873 W/cm 2. Overall, this study presents an effective method for manufacturing high-quality CLs in PEMFCs, ensuring improved performance.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Electrochemical Analysis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Designing the next generation of proton-exchange membrane fuel cells10.1038/s41586-021-03482-7 ↗
2. Electrocatalysts for PEM fuel cells
3. Advanced platinum-based oxygen reduction electrocatalysts for fuel cells10.1021/acs.accounts.0c00488 ↗
4. Current progress and performance improvement of Pt/C catalysts for fuel cells10.1039/D0TA08312G ↗
5. Stabilizing Pt-based electrocatalysts for oxygen reduction reaction: fundamental understanding and design strategies
6. Understanding the functions and modifications of interfaces in membrane electrode assemblies of proton exchange membrane fuel cells10.1039/D1TA01591E ↗
7. Study on the thermal transient of cathode catalyst layer in proton exchange membrane fuel cell under dynamic loading with a two-dimensional model
8. Recent developments of microenvironment engineering of single‐atom catalysts for oxygen reduction toward desired activity and selectivity
9. Carbon-based single atom catalysts for tailoring the ORR pathway: a concise review10.1039/D1TA06144E ↗
10. Recent developments in Pt–Co catalysts for proton-exchange membrane fuel cells
11. PEM fuel cell system control: a review10.1016/j.renene.2017.06.027 ↗
12. Analysis of proton exchange membrane fuel cells voltage drops for different operating parameters10.1016/j.ijhydene.2017.06.082 ↗
13. Controlling cracking formation in fuel cell catalyst layers10.1016/j.jpowsour.2019.02.058 ↗
14. Effect of dispersion method and catalyst on the crack morphology and performance of catalyst layer of PEMFC10.1149/1945-7111/ac3598 ↗
15. Analysis of crack formation during fuel cell catalyst ink drying process. Reduction of catalyst layer cracking by addition of high boiling point solvent10.1016/j.colsurfa.2021.127153 ↗
16. Development of high-performance roll-to-roll-coated gas-diffusion-electrode-based fuel cells10.1016/j.jpowsour.2021.230039 ↗
17. Reusability of decal substrates for the fabrication of catalyst coated membranes10.1016/j.ijadhadh.2019.102473 ↗
18. Optimization of catalyst ink composition for the preparation of a membrane electrode assembly in a proton exchange membrane fuel cell using the decal transfer10.1016/j.ijhydene.2012.09.013 ↗
19. Dependence of polymer electrolyte fuel cell performance on preparation conditions of slurry for catalyst layers10.1016/j.jpowsour.2009.04.015 ↗
20. Formulation of carbon black-ionomer dispersions for thin film formation in fuel cells10.1016/j.partic.2018.08.001 ↗
21. Recent progress of catalyst ink for roll-to-roll manufacturing paired with slot die coating for proton exchange membrane fuel cells
22. Morphological features (defects) in fuel cell membrane electrode assemblies10.1016/j.jpowsour.2005.12.027 ↗
23. 3D visualization of membrane failures in fuel cells10.1016/j.jpowsour.2017.01.129 ↗
24. 4D in situ visualization of electrode morphology changes during accelerated degradation in fuel cells by X-ray computed tomography10.1016/j.jpowsour.2017.03.058 ↗
25. Characterization of membrane degradation growth in fuel cells using X-ray computed tomography10.1149/2.0251806jes ↗
26. The effect of mechanical fatigue on the lifetimes of membrane electrode assemblies10.1115/1.4000629 ↗
27. Effect of dispersion solvent in catalyst ink on proton exchange membrane fuel cell performance10.1016/S1452-3981(23)18202-2 ↗
28. Steering and in situ monitoring of drying phenomena during film fabrication10.1007/s11998-019-00206-5 ↗
29. Molecular dynamics study of ionomer adsorption at a carbon surface in catalyst ink10.1016/j.electacta.2016.04.004 ↗
30. Influence of ionomer loading and substrate wettability on the morphology of ionomer thin films using coarse-grained solvent evaporation simulations10.1021/acs.macromol.0c01303 ↗
31. Coarse-grained molecular dynamics simulation of perfluorosulfonic acid polymer in water–ethanol mixtures10.1021/acs.macromol.0c02364 ↗
32. Adsorption, desorption and coadsorption behaviors of sulfamerazine, Pb(II) and benzoic acid on carbon nanotubes and nano-silica10.1016/j.scitotenv.2020.139685 ↗
33. The role of carbon nanotube pretreatments in the adsorption of benzoic acid10.3390/ma14092118 ↗
34. Highly selective electrocatalytic hydrogenation of benzoic acid over Pt/C catalyst supported on carbon fiber10.1016/j.cej.2022.136719 ↗
35. Performance enhancement of inkjet printed multi‐walled carbon nanotubes inks using synthetic and green surfactants10.1002/admt.202001026 ↗
36. New insights on the agglomeration and sedimentation behaviours of catalyst ink of proton exchange membrane fuel cells affected by ionomers concentration10.1016/j.jpowsour.2022.232427 ↗
37. Copper nanowire dispersion through an electrostatic dispersion mechanism for high-performance flexible transparent conducting films and optoelectronic devices10.1021/acsami.8b19277 ↗
38. Particle size and zeta potential of carbon black in liquid media10.1016/j.carbon.2007.09.010 ↗
39. Imaging reactivity of the Pt–ionomer interface in fuel-cell catalyst layers10.1021/acscatal.0c01594 ↗
40. Morphology evolution and adsorption behavior of ionomers from solution to Pt/C substrates10.1021/acs.macromol.2c00533 ↗
41. Elimelech · 1998
42. Effects of Pt and ionomer ratios on the structure of catalyst layer: a theoretical model for polymer electrolyte fuel cells10.1016/j.jpowsour.2017.11.026 ↗
43. Effect of a polybenzimidazole coating on carbon supports for ionomer content optimization in polymer electrolyte membrane fuel cells10.1016/j.jpowsour.2021.229855 ↗
44. Effect of dispersant on catalyst ink properties and catalyst layer structure for high performance polymer electrolyte membrane fuel cells10.1016/j.jpowsour.2023.232664 ↗
45. Solvent effects on the rheology of fuel cell catalyst ink and the adsorption of ionomers on the particles10.1063/5.0102157 ↗
46. Macosko · 1994
47. Rheological investigation on the microstructure of fuel cell catalyst inks10.1021/acsami.8b15039 ↗
48. Influence of ionomer adsorption on agglomerate structures in high-solid catalyst inks10.1016/j.carbon.2020.07.047 ↗
49. Effect of dispersion solvents and ionomers on the rheology of catalyst inks and catalyst layer structure for proton exchange membrane fuel cells10.1021/acsami.1c07070 ↗
50. Wagner · 2012
51. Effects of ionomer and dispersion methods on rheological behavior of proton exchange membrane fuel cell catalyst layer ink10.1016/j.ijhydene.2020.07.241 ↗
52. The effect of solvent and ionomer on agglomeration in fuel cell catalyst inks: simulation by the Discrete Element Method10.1016/j.ijhydene.2019.09.012 ↗
53. Ploehn · 1990 · vol. 15 · 137
54. Versuch einer mathematischen Theorie der Koagulationskinetik kolloider Lösungen10.1515/zpch-1918-9209 ↗
55. Viscosity of (water + alcohol) mixtures under high-pressure10.1007/BF00515199 ↗
56. Drying mechanisms and stress development in aqueous alumina tape casting10.1016/j.jeurceramsoc.2004.05.028 ↗
57. Flow and fracture in drying nanoparticle suspensions10.1103/PhysRevLett.91.224501 ↗
58. Solubility of benzoic acid in mixed solvents10.1021/je060408x ↗
59. An overview of calibration materials used in thermal analysis—benzoic acid10.1016/S0040-6031(02)00108-9 ↗
60. High-performance and durable cathode catalyst layer with hydrophobic C@PTFE particles for low-Pt loading membrane assembly electrode of PEMFC10.1016/j.enconman.2019.04.014 ↗