Self-assembled zinc polyethylenimine shield for long-lasting zinc anodes

Ying Chen, Suxia Yan, Taofeng Li, Zhilong Zhang, Li Zhang, Xiaohui Song, Junfeng Liu, Yong Wang, Edison Huixiang Ang

Publisher page

Abstract

The zinc (Zn) anode of aqueous zinc-ion batteries (AZIBs) faces significant challenges, including dendritic growth, hydrogen evolution reactions, and corrosion, which impede their commercial application. Here, we present a strategy for creating an artificial surface coating layer, Zn-polyethylenimine (Zn-PEI) coordination polymer, formed on the Zn anode surface. The robust Zn-PEI protective layer, rich in amine groups, accelerates ion transport and provides a uniform electric field, thereby suppressing dendrite formation. Additionally, this layer prevents direct contact between the Zn surface and the electrolyte, reducing other side reactions such as hydrogen evolution, surface corrosion, and passivation. The charged amine groups in PEI preferentially expose the Zn (101) crystal plane, which has weak thermodynamic stability, to achieve ordered and densely packed Zn (101) deposition. Consequently, Zn-PEI@Zn//Zn-PEI@Zn symmetric cells exhibit a remarkable cycling life of over 2000 h under the conditions of 1 mA cm −2 and 1 mAh cm −2, and Zn-PEI@Zn//Cu asymmetric cells maintain an average coulombic efficiency of 99.7 % after 1000 stable cycles. This strategy effectively addresses the inherent issues of dendrite growth and hydrogen evolution in Zn anodes, laying a solid foundation for the development of high-performance AZIBs.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced battery technologies research · Advanced Battery Materials and Technologies · Conducting polymers and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Recent progress on Zn anodes for advanced aqueous zinc‐ion batteries10.1002/aenm.202300606 ↗
2. Optimizing interfacial electronic coupling with metal oxide to activate inert polyaniline for superior electrocatalytic hydrogen generation10.1002/cey2.3 ↗
3. Comprehensive review onzinc‐ionbattery anode: challenges and strategies10.1002/inf2.12306 ↗
4. Innovative solutions for high-performance silicon anodes in lithium-ion batteries: overcoming challenges and real-world applications10.1007/s40820-024-01388-3 ↗
5. Fast‐charging anode materials for sodium‐ion batteries10.1002/adma.202404574 ↗
6. Polyvinyl alcohol coating induced preferred crystallographic orientation in aqueous zinc battery anodes10.1016/j.nanoen.2022.107269 ↗
7. Concentrated dual-cation electrolyte strategy for aqueous zinc-ion batteries10.1039/D1EE01472B ↗
8. Tannin acid induced anticorrosive film toward stable Zn-ion batteries10.1016/j.nanoen.2022.107721 ↗
9. Modulated bonding interaction in propanediol electrolytes toward stable aqueous zinc-ion batteries10.1007/s40843-021-1841-5 ↗
10. Issues and future perspective on zinc metal anode for rechargeable aqueous zinc‐ion batteries10.1002/eem2.12067 ↗
11. Engineering interfacial layers to enable Zn metal anodes for aqueous zinc-ion batteries10.1016/j.ensm.2021.09.012 ↗
12. Eliminating the micropore confinement effect of carbonaceous electrodes for promoting Zn-ion storage capability10.1002/adma.202203744 ↗
13. Building sustainable saturated fatty acid-zinc interfacial layer toward ultra-stable zinc metal anodes10.1021/acs.nanolett.3c00741 ↗
14. An artificial polyacrylonitrile coating layer confining zinc dendrite growth for highly reversible aqueous zinc-based batteries10.1002/advs.202100309 ↗
15. Taurine-mediated dynamic bridging strategy for highly stable Zn metal anode
16. Chelating dicarboxylic acid as a multi-functional electrolyte additive for advanced Zn anode in aqueous Zn-ion batteries10.1016/j.jpowsour.2023.233593 ↗
17. Facilely constructing ultrahigh lattice-matched Cuzn5 epitaxial interface for dendrite-free Zn metal anode10.1016/j.jechem.2024.08.023 ↗
18. Advanced filter membrane separator for aqueous zinc-ion batteries10.1002/smll.202003106 ↗
19. Manipulating crystallographic orientation of zinc deposition for dendrite‐free zinc ion batteries10.1002/aenm.202101299 ↗
20. Industrial waste derived separators for Zn‐ion batteries achieve homogeneous Zn(002) deposition through low chemical affinity effects10.1002/smll.202311203 ↗
21. Direct self-assembly of mxene on Zn anodes for dendrite-free aqueous zinc-ion batteries10.1002/anie.202012322 ↗
22. Engineering hydrophobic protective layers on zinc anodes for enhanced performance in aqueous zinc-ion batteries10.1016/j.jechem.2024.05.035 ↗
23. ‐Situ ultrafast construction of zinc tungstate interface layer for highly reversible zinc anodes10.1002/anie.202319661 ↗
24. Backside coating for stable Zn anode with high utilization rate
25. Ultrahigh‐rate and long‐life zinc–metal anodes enabled by self‐accelerated cation migration10.1002/aenm.202100982 ↗
26. Stimulating Zn2+ permselectivity for prominent zinc anode reversibility by designing a self-assembled artificial layer10.1016/j.cej.2022.140827 ↗
27. Ultrathin surface coating of nitrogen-doped graphene enables stable zinc anodes for aqueous zinc-ion batteries10.1002/adma.202101649 ↗
28. Carbon-based nanomaterials for stabilizing zinc metal anodes towards high-performance aqueous zinc-ion batteries
29. Realizing fast plating/stripping of high-performance Zn metal anode with a low Zn loading10.55713/jmmm.v34i2.2009 ↗
30. Layer-by-Layer zinc metal anodes to achieve long-life zinc-ion batteries10.1016/j.cej.2021.133902 ↗
31. Metal‐organic framework integrated anodes for aqueous zinc‐ion batteries10.1002/aenm.201904215 ↗
32. A semi-interpenetrating network polymer coating for dendrite-free Zn anodes10.1016/j.jpowsour.2022.232622 ↗
33. Engineering an artificial coating layer of metal porphyrin‐based porous organic polymers toward high stable aqueous zinc‐ion batteries
34. A dynamic and self-adapting interface coating for stable Zn-metal anodes10.1002/adma.202105133 ↗
35. Polymers for aqueous zinc‐ion batteries: from fundamental to applications across core components10.1002/aenm.202303967 ↗
36. Polymer coating with balanced coordination strength and ion conductivity for dendrite-free zinc anode10.1002/adma.202307727 ↗
37. Phase inversion‐induced porous polymer coating for high rate and stable zinc anode10.1002/adfm.202401760 ↗
38. Thermal‐cyclized polyacrylonitrile artificial protective layers toward stable zinc anodes for aqueous zinc‐based batteries
39. Boosting uniform nucleation and suppressing hydrogen evolution with an in-situ formed zinc hyaluronate protective film on zinc anodes10.1016/j.jcis.2023.08.047 ↗
40. Tuning vertical electrodeposition for dendrites-free zinc-ion batteries10.1021/acsnano.4c00288 ↗
41. Dendrite‐free zinc anode via oriented plating with alkaline earth metal ion additives10.1002/adfm.202401537 ↗
42. The effect of polyethyleneimine as an electrolyte additive on zinc electrodeposition mechanism in aqueous zinc-ion batteries10.1016/j.electacta.2017.11.116 ↗
43. Revealing the effect of polyethylenimine on zinc metal anodes in alkaline electrolyte solution for zinc–air batteries: mechanism studies of dendrite suppression and corrosion inhibition10.1039/D0TA06929A ↗
44. Biomass-derived polymer as a flexible “zincophilic–hydrophobic” solid electrolyte interphase layer to enable practical Zn metal anodes10.1016/j.jcis.2024.04.234 ↗
45. Mechanism for zincophilic sites on zinc‐metal anode hosts in aqueous batteries10.1002/aenm.202003419 ↗
46. Highly stable Zn metal anodes enabled by atomic layer deposited Al2o3 coating for aqueous zinc-ion batteries10.1039/D0TA00748J ↗
47. Ultrathin surface coating enables stabilized zinc metal anode10.1002/admi.201800848 ↗
48. Proton-selective coating enables fast-kinetics high-mass-loading cathodes for sustainable zinc batteries10.1038/s41467-024-46464-9 ↗
49. A low fraction electrolyte additive as interface stabilizer for Zn electrode in aqueous batteries10.1016/j.ensm.2022.10.029 ↗
50. Engineering an artificial coating layer of metal porphyrin‐based porous organic polymers toward high stable aqueous zinc‐ion batteries10.1002/adfm.202400032 ↗
51. Fast ion transport at solid–solid interfaces in hybrid battery anodes10.1038/s41560-018-0096-1 ↗
52. Sustainable biopolymeric hydrogel interphase for dendrite-free aqueous zinc-ion batteries10.1016/j.cej.2021.133532 ↗
53. Tailoring desolvation kinetics enables stable zinc metal anodes10.1039/D0TA06622B ↗
54. A patternable and in situ formed polymeric zinc blanket for a reversible zinc anode in a skin‐mountable microbattery10.1002/adma.202007497 ↗
55. Ultrafast superfilling construction of a metal artificial interface for long-term stable zinc anodes10.1002/adma.202300850 ↗
56. Converting commercial Zn foils into single (002)-textured Zn with millimeter-sized grains for highly reversible aqueous zinc batteries
57. Texture exposure of unconventional (101)Zn facet: enabling dendrite‐free Zn deposition on metallic zinc anodes10.1002/aenm.202304003 ↗
58. Janus interface enables reversible Zn-ion battery by regulating interfacial water structure and crystal-orientation10.1039/D3SC05334B ↗
59. Recent progress and perspective in electrode materials for K‐ion batteries10.1002/aenm.201702384 ↗
60. Aqueous vs. Nonaqueous Zn-ion batteries: consequences of the desolvation penalty at the interface10.1039/C8EE00378E ↗
61. Facet‐termination promoted uniform Zn (100) deposition for high‐stable zinc‐ion batteries10.1002/aenm.202301517 ↗