By conducting experiments under pressures on the matrix of a single molten carbonate fuel cell (mcfc), as well as by performing comparative sintering experiments with and without the molten carbonate, changes in the maximum pore diameter, pore-size distribution, crystalline phase, brunauer-emmett-teller (bet) surface area and surface configuration were measured. the parameters of the effectiveness of the gas barrier (delta p > 0.1 mpa) and the porosity (40% < 8 < 70%) were taken as lifetime criteria for the matrix. by using regression equations based on the experimental results, the matrix was estimated by two aspects: maximum pore diameter and porosity for commercial requirements. meanwhile, changes in the maximum pore diameter, pore-size distribution and porosity for estimating the sintering behavior were presented and explained theoretically. rearrangements, slips and dissolutions of the alpha-lithium aluminate (alpha-lialo2) particles were observed in the matrices, which promote the alteration of the pore diameter and porosity during the sintering processes. (c) 2006 published by elsevier b.v.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Advanced ceramic materials synthesis · Thermal and Kinetic Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. 1993 · 399
2. Yasue · J. Power Sources · 1998 · 71 · 8910.1016/S0378-7753(97)02715-8 ↗
3. Eichenberger · J. Power Sources · 1998 · 71 · 9510.1016/S0378-7753(97)02716-X ↗
4. Hong · Korean J. Chem. Eng. · 2000 · 17 · 19310.1007/BF02707142 ↗
5. Tomimatsu · J. Electrochem. Soc. · 1997 · 144 · 418210.1149/1.1838163 ↗
6. Hatoh · Electrochemistry (Japan) · 1989 · 57 · 728
7. Veringa · J. Mater. Sci. · 1991 · 26 · 598510.1007/BF01113874 ↗
8. Terada · J. Power Sources · 1998 · 75 · 22310.1016/S0378-7753(98)00115-3 ↗
9. Nakagawa · Electrochemistry (Japan) · 1997 · 65 · 231
10. Murai · J. Eletrochem. Soc. · 1996 · 143 · 277610.1149/1.1837106 ↗
11. Sotouchi · J. Electrochem. Soc. · 1992 · 139 · 112710.1149/1.2069351 ↗
12. Takizawa · J. Power Sources · 2002 · 109 · 12710.1016/S0378-7753(02)00045-9 ↗
13. Arendt · J. Electrochem. Soc. · 1980 · 127 · 1160
14. Lin · Electrochim. Acta · 2002 · 47 · 145110.1016/S0013-4686(01)00833-7 ↗
15. Böhme · Int. J. Hydrogen Energy · 1994 · 19 · 34910.1016/0360-3199(94)90067-1 ↗
16. Lin · Electrochemistry (China) · 1998 · 4 · 406
17. Lacovangelo · J. Electrochem. Soc. · 1988 · 135 · 22110.1149/1.2095559 ↗
18. Lin · Electrochemistry (China) · 2000 · 6 · 109
19. Kinoshita · J. Electrochem. Soc. · 1982 · 129 · 21610.1149/1.2123760 ↗
20. Swain · 1994
21. Kim · J. Power Sources · 2001 · 99 · 2610.1016/S0378-7753(00)00689-3 ↗
22. Kirk-Othmer · 1982
23. Yin · 2002