Abstract
Silicon–Graphite blended electrodes in Li-ion batteries have been proposed as a way to harness the high capacity of Si as an anode material, while minimising the negative effects of their large volume expansion. NMC 811 is the current state-of-the-art layered oxide cathode material, where the cobalt content of the cathode has been minimised. These are the two of the most promising materials for achieving electric vehicle targets in terms of performance, cyclability and price, however their degradation mechanism is not fully understood. Here these two materials have been used to manufacture 5 Ah prototype multi-layer pouch cells, which are aged and then studied using two complimentary diffraction techniques. Neutron diffraction has enabled a quantitative analysis of phase transitions in Si–Gr anodes in a pristine and degraded cell, and the alloying behaviour of Si and Li has been inferred by comparison of identical cells with either graphite or Si–Gr anodes. Synchrotron X-ray Diffraction has been used to make an operando 2D map of the cathode and anode lithiation in the pouch cell, as well as to map the volume expansion across the cell. This approach has revealed that degradation entails significant inhomogeneities across both electrodes, linked to the inhomogeneous volume expansion of the Si–Gr anodes.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Muon and positron interactions and applications · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Cars, planes, trains: where do CO2 emissions from transport come from?
2. A review of degradation mechanisms and recent achievements for Ni-rich cathode-based Li-ion batteries10.1002/aenm.202103005 ↗
3. Diverting exploration of silicon anode into practical way: A review focused on silicon-graphite composite for lithium ion batteries10.1016/j.ensm.2020.11.028 ↗
4. Differentiating the degradation phenomena in silicon-graphite electrodes for lithium-ion batteries10.1149/2.1921712jes ↗
5. Integration of graphite and silicon anodes for the commercialization of high-energy lithium-ion batteries10.1002/anie.201902085 ↗
6. A review of recent developments in Si/C composite materials for Li-ion batteries10.1016/j.ensm.2020.10.026 ↗
7. Silicon-based nanomaterials for lithium-ion batteries: A review10.1002/aenm.201300882 ↗
8. Understanding component-specific contributions and internal dynamicsin silicon/graphite blended electrodes for high-energy lithium-ion batteries
9. Anisotropic swelling and fracture of silicon nanowires during lithiation10.1021/nl201684d ↗
10. Size-dependent fracture of silicon nanoparticles during lithiation10.1021/nn204476h ↗
11. Towards a 3D-resolved model of Si/Graphite composite electrodes from manufacturing simulations10.1016/j.jpowsour.2021.230486 ↗
12. Capacity fade and its mitigation in Li-ion cells with silicon-graphite electrodes10.1021/acs.jpcc.7b06118 ↗
13. Understanding the roles of tris(trimethylsilyl) phosphite (TMSPi) in LiNi0.8Mn0.1Co0.1O2 (NMC811)/silicon–graphite (Si–Gr) lithium-ion batteries10.1002/admi.202000277 ↗
14. Quantifying microstructural dynamics and electrochemical activity of graphite and silicon-graphite lithium ion battery anodes10.1038/ncomms12909 ↗
15. The development and future of lithium ion batteries10.1149/2.0251701jes ↗
16. Performance and cost of materials for lithium-based rechargeable automotive batteries10.1038/s41560-018-0107-2 ↗
17. Graphite particle-size induced morphological and performance changes of graphite–silicon electrodes10.1149/1945-7111/ab9b9a ↗
18. Interplay between electrochemical reactions and mechanical responses in silicon–graphite anodes and its impact on degradation10.1038/s41467-021-22662-7 ↗
19. The role of silicon in silicon-graphite composite electrodes regarding specific capacity, cycle stability, and expansion10.1149/1945-7111/ac4545 ↗
20. Intrinsic origins of crack generation in Ni-rich LiNi0.8Co0.1Mn0.1O2 layered oxide cathode material10.1038/srep39669 ↗
21. Si–C/G based anode swelling and porosity evolution in 18650 casing and in pouch cell10.1016/j.jpowsour.2021.230552 ↗
22. Low-temperature charging and aging mechanisms of Si/C composite anodes in Li-ion batteries: An operando neutron scattering study10.1002/cssc.201903139 ↗
23. In-situ observation of inhomogeneous degradation in large format Li-ion cells by neutron diffraction10.1016/j.jpowsour.2013.02.066 ↗
24. In operando studies of rotating prismatic Li-ion batteries using monochromatic wide-angle neutron diffraction10.1016/j.est.2019.100772 ↗
25. High-energy lateral mapping (HELM) studies of inhomogeneity and failure mechanisms in NMC622/Li pouch cells10.1021/acs.chemmater.0c04537 ↗
26. Probing chemical heterogeneity of Li-ion batteries by in operando high energy X-ray diffraction radiography10.1016/j.jpowsour.2018.09.035 ↗
27. Lithium heterogeneities in cylinder-type Li-ion batteries – fatigue induced by cycling10.1016/j.jpowsour.2019.227466 ↗
28. Inhomogeneous distribution of lithium and electrolyte in aged Li-ion cylindrical cells10.1016/j.jpowsour.2020.228690 ↗
29. Revealing causes of macroscale heterogeneity in lithium ion pouch cells via synchrotron X-ray diffraction10.1016/j.jpowsour.2021.230253 ↗
30. Time- and space-resolved in situ X-ray diffraction study of phase transformations and redistribution in Zn–air battery anodes10.1021/acsaem.2c01868 ↗
31. Transformation and migration in secondary zinc–air batteries studied by in situ synchrotron X-ray diffraction and X-ray tomography10.1039/C8TA11554K ↗
32. High-resolution powder di!ractometer HRPT for thermal neutrons at SINQ10.1016/S0921-4526(99)01399-X ↗
33. TOPAS and TOPAS-Academic: an optimization program integrating computer algebra and crystallographic objects written in C++10.1107/S1600576718000183 ↗
34. Aberration corrections for non-Bragg–Brentano diffraction geometries10.1107/S1600576717000085 ↗
35. Evolution of structure and lithium dynamics in LiNi0.8Mn0.1Co0.1 O2 (NMC811) cathodes during electrochemical cycling10.1021/acs.chemmater.9b00140 ↗
36. Lithium intercalation into graphitic carbons revisited: Experimental evidence for twisted bilayer behavior10.1149/2.031305jes ↗
37. Two-dimensional diffraaction using area detectors
38. 2018
39. Experimental methods in chemical engineering: X-ray diffraction spectroscopy—XRD10.1002/cjce.23747 ↗
40. Multiscale multiphase lithiation and delithiation mechanisms in a composite electrode unraveled by simultaneous operando small-angle and wide-angle X-Ray Scattering10.1021/acsnano.9b05055 ↗