Abstract
Abstract Lithium-ion conductors with a crystal structure classified as Na super ion Conductors (NASICON) exhibit high ionic conductivity at room temperature that may be used in next-generation batteries. This study finds unusual ionic conduction of Li1.3Al0.3Ti1.7(PO4)3 (LATP): hysteresis on temperature and atmosphere dependence. The precise conductivity analyses (a wide frequency range, a wide temperature range, and a narrow temperature interval) reveal that the unusual conductivity is attributed to grain boundary conductivity enhanced by moisture. From the detailed studies on bulk (crystal structure) and grain boundary (microcracks, segregation, and impurities) of LATP pellets, it is concluded that the unusual ionic conduction results from adsorbed water on microcracks of LATP pellets. It is also confirmed that at high humidity, grain boundary resistance is further reduced by condensed water in the microcracks. This study reveals the high moisture sensitivity of conductivity of LATP for the first time, which is explained by the concerted influence of microstructure and humidity on ionic conductivity across grain boundaries. The results point out the importance of atmosphere control in scientific studies and for quality control of this class of solid electrolytes in advanced batteries like all-solid-state batteries, Li-air batteries, and others.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Progress and prospective of solid-state lithium batteries10.1016/j.actamat.2012.10.034 ↗
2. Progress in solid electrolytes toward realizing solid-state lithium batteries10.1016/j.jpowsour.2018.05.003 ↗
3. A solid future for battery development
4. Lithium-metal growth kinetics on LLZO garnet-type solid electrolytes10.1016/j.joule.2019.06.013 ↗
5. High-power all-solid-state batteries using sulfide superionic conductors10.1038/nenergy.2016.30 ↗
6. Synthesis of a new lithium ionic conductor, thio-LISICON-lithium germanium sulfide system10.1016/S0167-2738(00)00277-0 ↗
7. Formation of superionic crystals from mechanically milled Li2S–P2S5 glasses10.1016/S1388-2481(02)00555-6 ↗
8. Superionic glasses and glass–ceramics in the Li2S–P2S5 system for all-solid-state lithium secondary batteries10.1016/j.ssi.2012.03.013 ↗
9. High lithium ion conductivity in the perovskite-type compounds Ln12Li12TiO3(Ln=La,Pr,Nd,Sm)10.1016/0167-2738(94)90310-7 ↗
10. Fast Li+ conducting ceramic electrolytes10.1002/adma.19960080205 ↗
11. Fast lithium ion conduction in garnet-type Li7La3Zr2O1210.1002/anie.200701144 ↗
12. A complex hydride lithium superionic conductor for high-energy-density all-solid-state lithium metal batteries
13. Superionic conductivity in lithium-rich anti-perovskites10.1021/ja305709z ↗
14. Relevance of solid electrolytes for lithium-based batteries: a realistic view10.1007/s10832-017-0091-0 ↗
15. Toward understanding the reactivity of garnet-type solid electrolytes with H2O/CO2 in a glovebox using X-ray photoelectron spectroscopy and electrochemical methods10.1021/acsami.0c09135 ↗
16. The active interface of Ta-doped Li7La3Zr2O12 for Li plating/stripping revealed by acid aqueous etching10.1021/acsaem.9b01193 ↗
17. Grain boundary modification to suppress lithium penetration through garnet-type solid electrolyte10.1016/j.jpowsour.2017.07.088 ↗
18. Ionic conductivity of the lithium titanium phosphate (Li1+XMXTi2−X(PO4)3, M = Al, Sc, Y, and La) systems10.1149/1.2096693 ↗
19. Lithium anode for lithium-air secondary batteries10.1016/j.jpowsour.2008.07.080 ↗
20. Study on lithium/air secondary batteries—stability of NASICON-type lithium ion conducting glass–ceramics with water10.1016/j.jpowsour.2008.08.009 ↗
21. Durability of the Li1+xTi2-xAlx(PO4)3 solid electrolyte in lithium-sulfur batteries10.1021/acsenergylett.6b00481 ↗
22. High-performance lithium-iodine flow battery10.1002/aenm.201300627 ↗
23. Reversible Br2/Br− redox couple in aqueous phase as high- performance catholyte for alkali-ion batteries10.1039/C4EE00407H ↗
24. Rechargeable Li//Br battery: a promising platform for post lithium ion batteries10.1039/C4TA04419C ↗
25. Development of rechargeable lithium–bromine batteries with lithium ion conducting solid electrolyte10.1016/j.jpowsour.2015.02.015 ↗
26. Lithium ion conducting solid electrolytes for aqueous lithium-air batteries10.5796/electrochemistry.82.938 ↗
27. Complex investigation of water impact on Li-ion conductivity of Li1.3Al0.3Ti1.7(PO4)3- electrochemical, chemical, structural, and morphological aspects10.1021/acs.chemmater.9b04419 ↗
28. CeraCharge | TDK Electronics - TDK Europe. https://www.tdk-electronics.tdk.com/en/ceracharge.
29. Powder Tech. & All-Solid State Batteries|Video Library|TAIYO YUDEN CO, LTD, https://www.yuden.co.jp/ut/movie/powder_all_solid.html.
30. Murata Develops Solid-State Battery with Industry's Highest Energy Density for Wearables Applications, Oxide Ceramic Electrolyte Solution Provides Reliability and Durability | Product News | Murata Manufacturing Co, Ltd, https://www.murata.com/en-us/news/batteries/solid_state/2019/0626.
31. Murata's Oxide-Based Solid-State Batteries for Expanding the Range of Applications for IoT Devices and Supporting More Advanced Wearables | Murata Manufacturing Articles, https://article.murata.com/en-us/article/solid-state-battery-that-supports-wearables-2.
32. Structural factors that enhance lithium mobility in fast-ion Li1+xTi2-xAlx(PO4)3 (0 ≤ x ≤ 0.4) conductors investigated by neutron diffraction in the temperature range 100-500 K10.1021/ic400577v ↗
33. Insights into the reactive sintering and separated specific grain/grain boundary conductivities of Li1.3Al0.3Ti1.7(PO4)310.1016/j.jpowsour.2021.229631 ↗
34. Solution-based synthesis and characterization of lithium-ion conducting phosphate ceramics for lithium metal batteries10.1021/cm202773d ↗
35. Three-dimensional visualization in powder diffraction10.4028/www.scientific.net/SSP.130.15 ↗
36. Neutron Scattering Lengths and Cross Sections, https://www.ncnr.nist.gov/resources/n-lengths/.
37. Rietveld analysis software for J-PARC10.1016/j.nima.2008.11.056 ↗
38. Application of matrix decomposition algorithms for singular matrices to the Pawley method in Z-Rietveld10.1107/S0021889812003998 ↗
39. Effect of microcracking on ionic conductivity in LATP10.1016/j.jpowsour.2012.06.081 ↗
40. Evolution of microstructure and its relation to ionic conductivity in Li1+xAlxTi2−x(PO4)310.1016/j.ssi.2016.01.036 ↗
41. A systematic study of Nasicon-type Li1+xMxTi2−x(PO4)3 (M: Cr, Al, Fe) by neutron diffraction and impedance spectroscopy10.1016/j.ssi.2014.07.018 ↗
42. Lithium diffusion pathway in Li1.3Al0.3Ti1.7(PO4)3(LATP) superionic conductor10.1021/acs.inorgchem.5b02821 ↗
43. Bond softness sensitive bond-valence parameters for crystal structure plausibility tests10.1107/S2052252517010211 ↗
44. SoftBV – a software tool for screening the materials genome of inorganic fast ion conductors10.1107/S2052520618015718 ↗
45. Statistical variances of diffusional properties from ab initio molecular dynamics simulations
46. Ionic conduction in space charge regions10.1016/0079-6786(95)00004-E ↗
47. Local structure and composition change at surface of lithium-ion conducting solid electrolyte10.1016/j.ssi.2015.08.019 ↗
48. An explanation of the microcrack formation in Li1.3Al0.3Ti1.7(PO4)3 ceramics10.1016/j.jeurceramsoc.2016.02.042 ↗
49. A visualized structure-property modeling method for phosphogermanate glass based on XPS10.1016/j.mseb.2020.114775 ↗
50. Raman and X-ray photoelectron spectroscopic studies of lithium phosphotungstate glasses10.1016/0167-2738(92)90308-C ↗
51. The grain boundary impedance of random microstructures: numerical simulations and implications for the analysis of experimental data10.1016/S0167-2738(02)00274-6 ↗
52. Influence of strain on local structure and lithium ionic conduction in garnet-type solid electrolyte10.1016/j.jpowsour.2017.09.076 ↗
53. Microstructural and electrochemical properties of alkaline earth metal-doped Li garnet-type solid electrolytes prepared by solid-state sintering and spark plasma sintering methods10.1021/acsaem.8b01899 ↗
54. Proton conductivity: materials and applications10.1021/cm950192a ↗
55. Correlation for the vapor pressure of heavy water from the triple point to the critical point10.1063/1.1430231 ↗
56. Viscosity of deuterium oxide and water in the range 5 to 125 C
57. Surface tension of heavy water10.1038/136186c0 ↗
58. Adsorption-desorption mediated separation of low concentrated D2O from water with hydrophobic activated carbon fiber10.1016/j.jcis.2017.08.016 ↗
59. Observation of an exotic state of water in the hydrophilic nanospace of porous coordination polymers10.1038/s42004-020-0262-9 ↗
60. Isotope effect in the liquid properties of water confined in 100 nm nanofluidic channels10.1021/acs.jpcb.1c00780 ↗