Abstract

Nowadays, electrochemistry has a considerable technological impact, involving fuel cells, super capacitors and batteries. These devices are based on complex architectures, which complicates monitoring their evolution in situ under operating conditions to reveal the reasons for reduced lifetime and performances. Here, we present a design of a multipurpose electrochemical cell for grazing incidence small and wide angle X-ray scattering (GISAXS and GIWAXS) where the environment for operating conditions can be recreated. We focus on proton exchange membrane fuel cells (PEMFCs) which operational conditions are simulated by means of potentiodynamic-based accelerated stress tests, applied to a thin film of Pt nanoparticles representing a model system of a benchmark catalyst. Two different upper potentials are used to mimic fuel cell operating conditions: at 1.0 V RHE the catalyst film preserves its initial morphology, while at 1.5 V RHE (simulating fuel cell start-up/shut-down cycles) significant coarsening has been observed. The initial dimension of the Pt particles of 4.0 nm increases to 8.7 nm due to the predominant process of coalescence and final Ostwald ripening. In parallel, the distance between the particles increases, the catalyst film (9 nm thick) becomes thinner at first and exhibit a higher roughness at the end.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Ladewig · 2015
2. Anion-exchange membranes in electrochemical energy systems10.1039/C4EE01303D ↗
3. Progress in metal-supported solid oxide fuel cells: a review10.1016/j.jpowsour.2010.02.035 ↗
4. Towards real-time ion-specific structural sensitivity in nanoporous carbon electrodes using in situ anomalous small-angle X-ray scattering10.1021/acsami.9b14242 ↗
5. Mechanisms for enhanced performance of platinum-based electrocatalysts in proton exchange membrane fuel cells10.1002/cssc.201300823 ↗
6. Supercapacitor and supercapattery as emerging electrochemical energy stores10.1080/09506608.2016.1240914 ↗
7. The Li-ion rechargeable battery: a perspective10.1021/ja3091438 ↗
8. Electrode-electrolyte interface in Li-ion batteries: current understanding and new insights10.1021/acs.jpclett.5b01727 ↗
9. Analysis of degradation in PEMFC caused by cell reversal during air starvation10.1016/j.ijhydene.2008.02.049 ↗
10. Design criteria for stable Pt/C fuel cell catalysts10.3762/bjnano.5.5 ↗
11. Probing degradation by IL-TEM: the influence of stress test conditions on the degradation mechanism10.1149/2.078306jes ↗
12. Impact of alloying and lattice strain on ORR activity of Pt and Pd based ternary alloys with Fe and Co for proton exchange membrane fuel cell applications10.1039/c3ra47021k ↗
13. Scanning tunneling microscopy, voltammetry, and x-ray photoelectron spectroscopy study of the early stages of electrochemical faceting of gold (111) in aqueous sulfuric and perchloric acid10.1021/jp0353542 ↗
14. Correlation of surface site formation to nanoisland growth in the electrochemical roughening of Pt(111)10.1038/s41563-017-0015-z ↗
15. Atomic-scale identification of the electrochemical roughening of platinum10.1021/acscentsci.9b00782 ↗
16. Local resolved investigation of PEMFC performance degradation mechanism during dynamic driving cycle10.1016/j.ijhydene.2016.01.048 ↗
17. Atomic-level observation of electrochemical platinum dissolution and redeposition10.1021/acs.nanolett.9b02382 ↗
18. Stability of platinum particles on a carbon substrate investigated by atomic force microscopy and scanning electron microscopy10.1016/j.jpowsour.2007.06.016 ↗
19. Dissolution of pt at moderately negative potentials during oxygen reduction in water and organic media10.1021/la304694d ↗
20. Effect of halogen ions on platinum dissolution under potential cycling in 0.5 M H2SO4 solution10.1016/j.electacta.2007.06.029 ↗
21. In-situ electrochemical atomic force microscopy study of aging of magnetron sputtered Pt-Co nanoalloy thin films during accelerated degradation test10.1016/j.electacta.2016.06.035 ↗
22. In situ probing of magnetron sputtered Pt-Ni alloy fuel cell catalysts during accelerated durability test using EC-AFM10.1016/j.electacta.2017.05.202 ↗
23. In situ electrochemical AFM monitoring of the potential-dependent deterioration of platinum catalyst during potentiodynamic cycling10.1016/j.ultramic.2018.01.015 ↗
24. The max iv storage ring project10.1107/S1600577514011503 ↗
25. Chenevier · 2018
26. Design status of the ultra-low emittance synchrotron facility PETRA IV10.1063/1.5084565 ↗
27. Kinetics and mechanism of redox processes of Pt/C and Pt3Co/C cathode electrocatalysts in a polymer electrolyte fuel cell during an accelerated durability test10.1021/acs.jpcc.6b04437 ↗
28. Operando 3D visualization of migration and degradation of a platinum cathode catalyst in a polymer electrolyte fuel cell10.1002/ange.201703940 ↗
29. Operando monitoring of the pore dynamics in ordered mesoporous electrode materials by small angle x-ray scattering10.1021/acsnano.5b01378 ↗
30. In Operando small-angle X-ray scattering investigation of nanostructured polymer electrolyte for lithium-ion batteries10.1021/acsenergylett.8b00763 ↗
31. Operando SAXS/WAXS on the a-P/C as the anode for Na-ion batteries10.1021/acs.jpcc.7b12825 ↗
32. Disentangling the degradation pathways of highly defective PtNi/C nanostructures - an operando wide and small angle X-ray scattering study10.1021/acscatal.8b02665 ↗
33. Combining SAXS and XAS to study the operando degradation of carbon-supported Pt-nanoparticle fuel cell catalysts10.1021/acscatal.8b01321 ↗
34. Quantification of ion confinement and desolvation in nanoporous carbon supercapacitors with modelling and in situ X-ray scattering10.1038/nenergy.2016.215 ↗
35. Watching mesoporous metal films grow during templated electrodeposition with: in situ SAXS10.1039/C7NR03321D ↗
36. In situ observation of strain development and porosity evolution in nanoporous gold foils10.1002/adfm.201100735 ↗
37. Using GISAXS to detect correlations between the locations of gold particles electrodeposited from an aqueous solution
38. A simple electrochemical cell for in-situ fundamental structural analysis using synchrotron X-ray powder diffraction10.1016/j.jpowsour.2013.03.086 ↗
39. In situ anomalous small-angle X-ray scattering and X-ray absorption near-edge structure investigation of catalyst structures and reactions10.1016/S0022-2860(96)09300-3 ↗
40. Electrochemical in situ reaction cell for X-ray scattering, diffraction and spectroscopy10.1107/S090904950300709X ↗
41. Electrochemical flow-cell setup for in situ X-ray investigations10.1149/2.0201610jes ↗
42. Electrochemical flow-cell setup for in situ X-ray investigations10.1149/2.0211610jes ↗
43. X-ray transparent proton-exchange membrane fuel cell design for in situ wide and small angle scattering tomography10.1016/j.jpowsour.2019.226906 ↗
44. Heterogeneous nanostructural aging of fuel cell ionomer revealed by operando SAXS10.1021/acsaem.8b02004 ↗
45. Synchrotron based operando surface X-ray scattering study towards structure–activity relationships of model electrocatalysts
46. Structural reorganization of Pt(111) electrodes by electrochemical oxidation and reduction10.1021/jacs.7b01039 ↗
47. Evolution of the PtNi bimetallic alloy fuel cell catalyst under simulated operational conditions10.1021/acsami.0c02083 ↗
48. Form 2: Affordable Desktop SLA 3D Printer | Formlabs, (n.d.). https://formlabs.com/3d-printers/form-2/(accessed April 25, 2020).
49. 3D Printing Materials for Professionals | Formlabs, (n.d.). https://formlabs.com/materials/standard/#greyscale (accessed April 25, 2020).
50. Leak-Free Electrodes, (n.d.). https://www.alvatek.co.uk/leak-free-electrodes/(accessed April 25, 2020).
51. First performance assessment of the small-angle X-ray scattering beamline at ELETTRA10.1107/S090904959800137X ↗
52. Porod · 1982
53. Surface-sensitive approach to interpreting supramolecular rearrangements in cellulose by synchrotron grazing incidence small-angle X-ray scattering10.1021/acsmacrolett.5b00306 ↗
54. Analysis of small angle neutron scattering spectra from polydisperse interacting colloids10.1063/1.446055 ↗
55. Study of Schultz distribution to model polydispersity of microemulsion droplets10.1021/j100317a032 ↗
56. The structure factor and the transport properties of dense fluids having molecules with square well potential, a possible generalization10.1016/0378-4371(77)90151-0 ↗
57. Interactions and kinetic arrest in an adhesive hard-sphere colloidal system10.1063/1.1601605 ↗
58. Untersuchungen zur Totalreflexion von Röntgenstrahlen10.1002/andp.19314020607 ↗
59. Baumbach · 2004
60. X-ray reflectivity and diffuse scattering
61. Irena: tool suite for modeling and analysis of small-angle scattering10.1107/S0021889809002222 ↗
62. Glassy carbon as an absolute intensity calibration standard for small-angle scattering10.1007/s11661-009-9950-x ↗
63. Co-refinement of multiple-contrast neutron/X-ray reflectivity data using MOTOFIT10.1107/S0021889806005073 ↗
64. Approximations leading to a unified exponential/power-law approach to small-angle scattering10.1107/S0021889895005292 ↗
65. The effect of the particle size on the kinetics of CO electrooxidation on high surface area Pt catalysts10.1021/ja043602h ↗
66. Accelerated stress test of Pt/C nanoparticles in an interface with an anion-exchange membrane - an identical-location transmission electron microscopy study10.1021/acscatal.7b04055 ↗
67. Wagner · 1961
68. Relating rates of catalyst sintering to the disappearance of individual nanoparticles during Ostwald ripening10.1021/ja208324n ↗
69. Identical location scanning electron microscopy: a case study of electrochemical degradation of PtNi nanoparticles using a new nondestructive method10.1021/jp303831c ↗
70. Pt catalyst degradation in aqueous and fuel cell environments studied via in-operando anomalous small-angle X-ray acattering10.1016/j.electacta.2015.05.032 ↗
71. Anomalous grazing incidence small-angle X-ray scattering of carbon-encapsulated Au and Cu clusters10.1107/S0021889809007316 ↗