Numerical and experimental characterization of gas permeation through membranes with consideration of mechanical degradation in proton exchange membrane fuel cells
Source abstract
Abstract
Exposed to severe loading condition in fuel cells, the perfluorinated sulfonic-acid (PFSA) membrane degrades over time, which becomes the primary cause of the increasing transmembrane gas permeation during the service. As a result, the hydrogen crossover rate increases with the damage propagation, leading to loss in power and life. However, the effect of mechanical degradation on gas permeability of membrane cannot be quantitatively estimated due to difficulties in damage observation and modeling. This paper first establishes a numerical technique to predict the gas permeation through membrane with consideration of mechanical degradation. Blister test as well as gas permeation test are conducted for the verification of the numerical model. The model shows great prediction accuracy, based on which the uneven distributed damage and its effect on gas permeability are analyzed. Result shows that the gas permeation rate grows with pressure and mechanical degradation has a remarkable contribution, accounting for about 7.3% of total permeation rate at testing pressure of 130 kPa. Finally, the varied membrane shape and gas permeability, which all accelerate the gas permeation, are further analyzed based on the numerical model.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Membrane-based Ion Separation Techniques · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. A review of automotive proton exchange membrane fuel cell degradation under start-stop operating condition10.1016/j.apenergy.2018.04.049 ↗
2. A review of polymer electrolyte membrane fuel cell durability for vehicular applications: degradation modes and experimental techniques10.1016/j.enconman.2019.112022 ↗
3. Boosting the output power of PEM fuel cells by identifying best-operating conditions10.1016/j.enconman.2022.116205 ↗
4. Fabrication and characterization of self-assembled Nafion–SiO2–ePTFE composite membrane of PEM fuel cell10.1016/j.memsci.2007.12.025 ↗
5. Fuel cell membranes – pros and cons10.1016/j.energy.2019.01.034 ↗
6. New insights into perfluorinated sulfonic-acid ionomers10.1021/acs.chemrev.6b00159 ↗
7. Chapter 14 - the use of per-fluorinated sulfonic acid (PFSA) membrane as electrolyte in fuel cells
8. Composite short side chain PFSA membranes for PEM water electrolysis10.1016/j.memsci.2018.09.063 ↗
9. Mechanical failure and mitigation strategies for the membrane in a proton exchange membrane fuel cell10.1016/j.rser.2019.109289 ↗
10. Analysis of degradation mechanism in unitized regenerative fuel cell under the cyclic operation10.1016/j.enconman.2022.115210 ↗
11. Nafion degradation mechanisms in proton exchange membrane fuel cell (PEMFC) system: a review10.1016/j.ijhydene.2021.06.032 ↗
12. A degradation study of Nafion proton exchange membrane of PEM fuel cells10.1016/j.jpowsour.2007.03.061 ↗
13. Patrick · 2003 · 623
14. Hydrogen crossover through microporous anion exchange membranes for fuel cells10.1016/j.jpowsour.2022.231143 ↗
15. Hydrogen crossover in proton exchange membrane electrolysers: the effect of current density, pressure, temperature, and compression10.1016/j.electacta.2021.138085 ↗
16. Free volume and permeabilities of O2 and H2 in Nafion membranes for polymer electrolyte fuel cells10.1016/j.polymer.2008.05.003 ↗
17. Gas permeation in a dry Nafion membrane10.1021/ie00083a034 ↗
18. Study on water uptake of proton exchange membrane by using tritiated water sorption method10.1016/j.ijhydene.2005.02.006 ↗
19. The effect of relative humidity on the gas permeability and swelling in PFSI membranes10.1016/j.ijhydene.2011.07.047 ↗
20. Delamination evolution of PEM fuel cell membrane/CL interface under asymmetric RH cycling and CL crack location10.1016/j.apenergy.2022.118551 ↗
21. Accelerated durability testing via reactants relative humidity cycling on PEM fuel cells10.1016/j.apenergy.2011.05.011 ↗
22. Biaxial fatigue crack growth in proton exchange membrane of fuel cells based on cyclic cohesive finite element method10.1016/j.ijmecsci.2020.105946 ↗
23. Temperature-dependent fatigue crack growth mechanisms of fuel cell membranes10.1016/j.ijfatigue.2021.106554 ↗
24. Fracture property of Nafion XL composite membrane determined by R-curve method10.1016/j.jpowsour.2018.07.052 ↗
25. Biaxial fatigue crack propagation behavior of perfluorosulfonic-acid membranes10.1016/j.jpowsour.2018.02.002 ↗
26. Exploring the role of reinforcement in controlling fatigue crack propagation behavior of perfluorosulfonic-acid membranes10.1016/j.ijhydene.2018.02.034 ↗
27. Determining the critical plastically dissipated energy for fatigue crack growth in PEM fuel cell membrane and its environmental sensitivity10.1016/j.ijfatigue.2020.105697 ↗
28. Predicting fatigue lifetimes of a reinforced membrane in polymer electrolyte membrane fuel cell using plastic energy10.1016/j.jpowsour.2022.231597 ↗
29. Effect of operating conditions and geometric structure on the gas crossover in PEM fuel cell
30. Numerical and experimental investigation on the reactant gas crossover in a PEM fuel cell10.1016/j.ijheatmasstransfer.2018.07.092 ↗
31. Proton exchange membrane fuel cell degradation under close to open-circuit conditions: Part I: in situ diagnosis10.1016/j.jpowsour.2009.08.095 ↗
32. Durability study of proton exchange membrane fuel cells under dynamic testing conditions with cyclic current profile10.1016/j.jpowsour.2006.07.007 ↗
33. A mechanistic model for pinhole growth in fuel-cell membranes during cyclic loads10.1149/2.036408jes ↗
34. The effect of mechanical fatigue on the lifetimes of membrane electrode assemblies10.1115/1.4000629 ↗
35. Constitutive modeling of the rate, temperature, and hydration dependent deformation response of Nafion to monotonic and cyclic loading10.1016/j.jpowsour.2010.03.047 ↗
36. Positron annihilation lifetime study of high and low free volume glassy polymers: effects of free volume sizes on the permeability and permselectivity10.1021/ma000551+ ↗
37. Void nucleation and disentanglement in glassy amorphous polymers10.1103/PhysRevE.82.011803 ↗
38. Mechanisms of crazing in glassy polymers revealed by molecular dynamics simulations
39. Influence of damage on inhomogeneous deformation behavior of amorphous glassy polymers. Modeling and algorithmic implementation in a finite element setting10.1016/j.engfracmech.2014.01.002 ↗
40. Influence of voids on shear band instabilities under plane strain conditions10.1007/BF00036191 ↗
41. Modelling of the elasto-viscoplastic damage behaviour of glassy polymers10.1016/j.ijplas.2007.08.001 ↗
42. Continuum theory of ductile rupture by void nucleation and growth: Part I—yield criteria and flow rules for porous ductile media10.1115/1.3443401 ↗
43. Void nucleation effects in biaxially stretched sheets10.1115/1.3224807 ↗
44. Sorption, diffusion, and permeability of humid gases and aging of thermally rearranged (TR) polymer membranes from a novel ortho-hydroxypolyimide10.1016/j.memsci.2017.08.009 ↗
45. Chapter 5 - gas permeation in PEM water electrolyzers
46. Influence of polyimide precursor synthesis route and ortho-position functional group on thermally rearranged (TR) polymer properties: pure gas permeability and selectivity10.1016/j.memsci.2014.03.032 ↗
47. Estimating gas permeability and permselectivity of microporous polymers10.1016/j.memsci.2014.06.017 ↗
48. Free-volume hole properties of gas-exposed polycarbonate studied by positron annihilation lifetime spectroscopy10.1021/ma9603544 ↗
49. Modeling the cathode pressure dynamics in the Buckeye Bullet II 540 kW hydrogen PEM fuel cell system10.1016/j.jpowsour.2013.03.103 ↗
50. Investigating the stability and degradation of hydrogen PEM fuel cell10.1016/j.ijhydene.2021.08.183 ↗
51. PEM fuel cell-assisted lithium ion battery electric vehicle integrated with an air-based thermal management system10.1016/j.ijhydene.2022.08.153 ↗
52. Constant pressure primary flow standard for gas flows from 0.01cm3/min to 100cm3/min (0.007–74 μmol/s)10.1016/j.flowmeasinst.2013.12.002 ↗