Abstract Thermo-mechanical fatigue (TMF) behavior of a newly developed ferritic stainless steel (Crofer 22 H) for planar solid oxide fuel cell (pSOFC) interconnect is investigated. TMF tests under various combinations of cyclic mechanical and thermal loadings are conducted in air at a temperature range of 25oC–800 °C. Experimental results show the number of cycles to failure for non-hold-time TMF loading is decreased with an increase in the minimum stress applied at 800 °C. There is very little effect of maximum stress applied at 25 °C on the number of cycles to failure. The non-hold-time TMF life is dominated by a fatigue mechanism involving cyclic high-temperature softening plastic deformation. A hold-time of 100 h for the minimum stress applied at 800 °C causes a significant drop of number of cycles to failure due to a synergistic action of fatigue and creep. Creep and creep–fatigue interaction mechanisms are the two primary contributors to the hold-time TMF damage. The creep damage ratio in the hold-time TMF damage is increased with a decrease in applied stress at 800 °C and an increase in number of cycles to failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Yokokawa · Fuel Cells · 2001 · 1 · 11710.1002/1615-6854(200107)1:2<117::AID-FUCE117>3.0.CO;2-Y ↗
2. Zhu · Mater. Sci. Eng. A · 2003 · 348 · 22710.1016/S0921-5093(02)00736-0 ↗
3. Weber · J. Power Sources · 2004 · 127 · 27310.1016/j.jpowsour.2003.09.024 ↗
4. Antepara · J. Power Sources · 2005 · 151 · 10310.1016/j.jpowsour.2005.02.084 ↗
5. Fergus · Mater. Sci. Eng. A · 2005 · 397 · 27110.1016/j.msea.2005.02.047 ↗
6. Huang · Solid State Ionics · 2000 · 129 · 23710.1016/S0167-2738(99)00329-X ↗
7. Lin · J. Power Sources · 2007 · 164 · 23810.1016/j.jpowsour.2006.10.089 ↗
8. Lin · J. Power Sources · 2009 · 192 · 51510.1016/j.jpowsour.2009.03.010 ↗
9. Apfel · J. Power Sources · 2006 · 154 · 37010.1016/j.jpowsour.2005.10.052 ↗
10. Shankar · J. Nucl. Mater. · 2012 · 420 · 2310.1016/j.jnucmat.2011.08.048 ↗
11. Chyou · J. Power Sources · 2005 · 139 · 12610.1016/j.jpowsour.2004.07.001 ↗
12. Kurokawa · Solid State Ionics · 2004 · 168 · 1310.1016/j.ssi.2004.02.008 ↗
13. Yang · Int. J. Hydrogen Energy · 2007 · 32 · 377010.1016/j.ijhydene.2006.08.056 ↗
14. Geng · Solid State Ionics · 2006 · 177 · 55910.1016/j.ssi.2005.12.004 ↗
15. Gannon · Surf. Coat. Technol. · 2004 · 188-189 · 5510.1016/j.surfcoat.2004.08.067 ↗
16. Fontana · J. Power Sources · 2007 · 171 · 65210.1016/j.jpowsour.2007.06.255 ↗
17. Chiu · J. Power Sources · 2011 · 196 · 200510.1016/j.jpowsour.2010.09.083 ↗
18. Chiu · J. Power Sources · 2012 · 198 · 14910.1016/j.jpowsour.2011.09.056 ↗
19. Froitzheim · J. Power Sources · 2008 · 178 · 16310.1016/j.jpowsour.2007.12.028 ↗
20. Kuhn · Mater. Sci. Eng. A · 2011 · 528 · 588810.1016/j.msea.2011.03.112 ↗
21. Chang · J. Power Sources · 2009 · 189 · 109310.1016/j.jpowsour.2008.12.102 ↗
22. Chang · J. Power Sources · 2010 · 195 · 315910.1016/j.jpowsour.2009.12.008 ↗
23. Chang · J. Power Sources · 2011 · 196 · 358310.1016/j.jpowsour.2010.12.035 ↗
24. Lin · J. Power Sources · 2012 · 205 · 30710.1016/j.jpowsour.2012.01.048 ↗
25. Colombo · Int. J. Fatigue · 2008 · 30 · 24110.1016/j.ijfatigue.2007.01.036 ↗
26. Shi · Mater. Sci. Eng. A · 2010 · 528 · 23310.1016/j.msea.2010.08.089 ↗
27. Giroux · Mater. Sci. Eng. A · 2010 · 527 · 398410.1016/j.msea.2010.03.001 ↗
28. Sokolov · J. Nucl. Mater. · 2007 · 367-370 · 21310.1016/j.jnucmat.2007.03.143 ↗