The capacity fading of Lithium-ion batteries (LIBs) containing polycrystalline cathode materials can be attributed to the degradation of secondary particles caused by inter- and intra-granular fractures occurring during charging and discharging cycles. In this work, a diffusion-induced stress (DIS) analysis method based on the finite-discrete element method (FDEM) is developed for studying the fracture behaviors of polycrystalline cathodes. The analysis of lithiation and delithiation processes shows that C-rate and interfacial fracture toughness have significant effects on inter-granular crack morphologies. Our method enables precise analysis of the competition between intra- and inter-granular cracks and the effect of crack-impeded diffusion on crack morphologies. We compared numerical simulation results for scenarios where fracture toughness changes with the number of cycles, and demonstrated that the decreasing fracture toughness with cycle number is an important factor contributing to the slow crack growth. Additionally, we established the relationship between crack length and capacity loss, which agreed well with experimental results.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrostatic Discharge in Electronics · High voltage insulation and dielectric phenomena · Advancements in Battery Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Thermally modulated lithium iron phosphate batteries for mass-market electric vehicles10.1038/s41560-020-00757-7 ↗
2. The challenges and opportunities of battery-powered flight10.1038/s41586-021-04139-1 ↗
3. The promise of energy-efficient battery-powered urban aircraft10.1073/pnas.2111164118 ↗
4. The Li-ion rechargeable battery: a perspective10.1021/ja3091438 ↗
5. High-voltage charging-induced strain, heterogeneity, and micro-cracks in secondary particles of a nickel-rich layered cathode material10.1002/adfm.201900247 ↗
6. Controllable cathode–electrolyte interface of Li [Ni0.8Co0.1Mn0.1]O2 for lithium ion batteries: a review
7. Connecting particle fracture with electrochemical impedance in LiXMn2O410.1149/2.0941714jes ↗
8. Microstructural changes in LiNi0.8Co0.15Al0.05O2 positive electrode material during the first cycle10.1149/1.3544843 ↗
9. Intergranular cracking as a major cause of long-term capacity fading of layered cathodes10.1021/acs.nanolett.7b00379 ↗
10. Intragranular cracking as a critical barrier for high-voltage usage of layer-structured cathode for lithium-ion batteries10.1038/ncomms14101 ↗
11. A new coating method for alleviating surface degradation of LiNi0.6Co0.2Mn0.2O2 cathode material: nanoscale surface treatment of primary particles10.1021/acs.nanolett.5b00045 ↗
12. Capacity fading of Ni-rich Li[NixMnyCo1-x-y]O2 (0.6≤x≤0.95) cathodes for high-energy-density lithium-ion batteries: bulk or surface degradation?10.1021/acs.chemmater.7b05269 ↗
13. Oxygen release induced chemomechanical breakdown of layered cathode materials10.1021/acs.nanolett.8b01036 ↗
14. Nano-structural changes in Li-ion battery cathodes during cycling revealed by FIB-SEM serial sectioning tomography10.1039/C5TA04151A ↗
15. Watanabe · J. Power Sources · 2014 · 260 · 5010.1016/j.jpowsour.2014.02.103 ↗
16. Partial lithiation strategies for suppressing degradation of silicon composite electrodes10.1016/j.electacta.2018.11.009 ↗
17. A stress-based charging protocol for silicon anode in lithium-ion battery: theoretical and experimental studies10.1016/j.est.2020.101765 ↗
18. Mechanical and structural degradation of LiNixMnyCozO2 cathode in Li-ion batteries: an experimental study10.1149/2.1751713jes ↗
19. Tailoring grain boundary structures and chemistry of Ni-rich layered cathodes for enhanced cycle stability of lithium-ion batteries10.1038/s41560-018-0191-3 ↗
20. High-performance and industrially feasible Ni-rich layered cathode materials by integrating coherent interphase10.1021/acsami.8b05648 ↗
21. Coupling of electrochemically triggered thermal and mechanical effects to aggravate failure in a layered cathode10.1038/s41467-018-04862-w ↗
22. Numerical analysis of the cyclic mechanical damage of Li-ion battery electrode and experimental validation10.1016/j.ijfatigue.2020.105915 ↗
23. Degradation of lithium ion batteries employing graphite negatives and nickel–cobalt–manganese oxide+ spinel manganese oxide positives: Part 2, chemical–mechanical degradation model10.1016/j.jpowsour.2014.07.028 ↗
24. Mechanical-electrochemical modeling of agglomerate particles in lithium-ion battery electrodes10.1149/2.1331614jes ↗
25. Corrosive fracture of electrodes in Li-ion batteries10.1016/j.jmps.2018.07.021 ↗
26. Simulation of crack behavior of secondary particles in Li-ion battery electrodes during lithiation/de-lithiation cycles10.1016/j.ijmecsci.2019.02.042 ↗
27. A chemo-mechanical grain boundary model and its application to understand the damage of Li-ion battery materials10.1016/j.scriptamat.2020.03.027 ↗
28. A chemo-mechanical damage model at large deformation: numerical and experimental studies on polycrystalline energy materials10.1016/j.ijsolstr.2021.111099 ↗
29. Coupled chemo-mechanical modeling of fracture in polycrystalline cathode for lithium-ion battery10.1016/j.ijplas.2019.11.015 ↗
30. Chemo-mechanical modeling of inter-and intra-granular fracture in heterogeneous cathode with polycrystalline particles for lithium-ion battery10.1016/j.jmps.2022.104839 ↗
31. On the fragmentation of active material secondary particles in lithium ion battery cathodes induced by charge cycling
32. Munjiza · 2004
33. A coupled thermo-mechanical model based on the combined finite-discrete element method for simulating thermal cracking of rock10.1016/j.ijrmms.2016.11.023 ↗
34. A new 3D continuous-discontinuous heat conduction model and coupled thermomechanical model for simulating the thermal cracking of brittle materials10.1016/j.ijsolstr.2021.111123 ↗
35. The combined finite–discrete element method for structural failure and collapse10.1016/S0013-7944(03)00044-4 ↗
36. Generalized theory for DISes in a large deformed solid10.1142/S1758825122500247 ↗
37. A comparative study of cohesive law shapes in analytical modeling of interfacial debonding in lithium-ion battery electrodes10.1115/1.4044139 ↗
38. Cycling-induced damage of silicon-based lithium-ion batteries: modeling and experimental validation10.1016/j.ijfatigue.2023.107660 ↗
39. Large-scale 3D random polycrystals for the finite element method: generation, meshing and remeshing
40. Degradation identification of LiNi0.8Co0.1Mn0.1O2/graphite lithium-ion batteries under fast charging conditions10.1016/j.electacta.2021.138979 ↗
41. Simulation of intergranular fracture behavior inside randomly aggregated Li[NixCoyMn1-x-y]O2 polycrystalline particle10.1016/j.engfracmech.2022.108381 ↗
42. Microstructural adjusting crack evolution of polycrystalline NCM particle during charge/discharge cycle10.1149/1945-7111/ac8ee3 ↗
43. Numerical computation of central crack growth in an active particle of electrodes influenced by multiple factors10.1007/s10409-018-0764-1 ↗
44. Persistent state-of-charge heterogeneity in relaxed, partially charged Li1-xNi1/3Co1/3Mn1/3O2 secondary particles10.1002/adma.201601273 ↗
45. Capacity fading of Ni-rich NCA cathodes: effect of microcracking extent10.1021/acsenergylett.9b02302 ↗