journal article·2014-12

Electrochemical stability of aluminum current collector in alkyl carbonate electrolytes containing lithium bis(pentafluoroethylsulfonyl)imide for lithium-ion batteries

Seung-Taek Myung, Hitoshi Yashiro

Publisher page

Abstract

Abstract The electrochemical stability of aluminum in anhydrous alkyl carbonate electrolytes containing lithium bis(pentafluoroethylsulfonyl)imide (LiBETI, LiN(SO 2 C 2 F 5 ) 2 ), as compared with LiPF 6 , has been investigated in terms of alloy formation with lithium at lower potentials (∼0 V versus Li/Li + ) and repassivation of scratched surfaces at higher potentials (∼5 V versus Li/Li + ), using cyclic and in situ scratch polarization tests and time-of-flight secondary ion mass spectroscopic (ToF-SIMS) analysis. Li–Al alloy formation at 0 V versus Li/Li + is significantly suppressed in a LiBETI electrolyte though it is common in a LiPF 6 -containing electrolyte. ToF-SIMS analysis indicates that passive films on aluminum, which consist primarily of oxide/hydroxide, are less fluorinated in a LiBETI electrolyte than those formed in a LiPF 6 electrolyte. The less fluorinated oxide/hydroxide layer on aluminum is expected to be an important barrier against alloy formation in a LiBETI electrolyte. In combination with nano-sized SnO 2 powders, aluminum foil is successfully applicable as a current collector without Li–Al alloy formation in the range of 0.25–2 V versus Li/Li + , although graphite electrodes do not operate properly in the same operation range. Thus, the large electrochemical stability of aluminum in LiBETI electrolyte makes it possible to be used as current collectors for both negative and positive electrodes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Kanamura · J. Power Sources · 1995 · 57 · 11910.1016/0378-7753(95)02265-1 ↗
2. Braithwaite · J. Electrochem. Soc. · 1999 · 146 · 44810.1149/1.1391627 ↗
3. Zhang · J. Power Sources · 2002 · 109 · 45810.1016/S0378-7753(02)00110-6 ↗
4. Hyams · J. Electrochem. Soc. · 2007 · 154 · C39010.1149/1.2742321 ↗
5. Myung · Electrochim. Acta · 2009 · 55 · 28810.1016/j.electacta.2009.08.051 ↗
6. Myung · J. Power Sources · 2010 · 195 · 829710.1016/j.jpowsour.2010.07.027 ↗
7. Morita · J. Power Sources · 2003 · 199–121 · 78410.1016/S0378-7753(03)00253-2 ↗
8. Song · Electrochim. Acta · 2004 · 49 · 148310.1016/S0013-4686(03)00930-7 ↗
9. Krause · J. Power Sources · 1997 · 68 · 32010.1016/S0378-7753(97)02517-2 ↗
10. Morita · Electrochim. Acta · 2002 · 47 · 278710.1016/S0013-4686(02)00164-0 ↗
11. Censo · Electrochem. Commun. · 2005 · 7 · 100010.1016/j.elecom.2005.07.005 ↗
12. Myung · Electrochim. Acta · 2009 · 54 · 580410.1016/j.electacta.2009.05.035 ↗
13. Ball · 1974 · 118
14. Wang · Electrochim. Acta · 2000 · 45 · 267710.1016/S0013-4686(99)00429-6 ↗
15. Nakajima · Solid State Sci. · 2002 · 4 · 138510.1016/S1293-2558(02)00026-2 ↗
16. Yang · J. Electrochem. Soc. · 2000 · 147 · 439910.1149/1.1394077 ↗
17. Myung · J. Mater. Chem. · 2011 · 21 · 989110.1039/c0jm04353b ↗