Direct evidences for bis(fluorosulfonyl)imide anion hydrolysis in industrial production: Pathways based on thermodynamics analysis and theoretical simulation
Source abstract
Abstract
LiFSI (lithium bis(fluorosulfonyl)imide) is a promising lithium salt for electrolytes in Li-ion batteries. However, the accumulation of harmful gases and heat during LiFSI hydrolysis could lead to serious safety accidents. Here we systematically investigate LiFSI hydrolysis processes under comprehensive conditions: higher temperature/acidity/basicity and lower water content can accelerate the hydrolysis, whereas the presence of DEC (diethyl carbonate) solvent, and other alkali metals (Na +, K +) can stabilize FSI − . Unexpectedly, under alkaline conditions, temperature/water content could not affect the hydrolysis greatly. By monitoring the hydrolysis intermediates and products using time-dependent ion chromatography, infrared spectra, and nuclear magnetic resonance, the hydrolysis routes are proposed and validated by accelerating rate calorimetry, differential scanning calorimetry measurements, and theoretical calculations. Under neutral/acidic conditions, electrophilic attack on the S–N bond generates FSO 2NH 2 and FSO 3 −, while nucleophilic attack on the S–F bond produces FSO 2NSO 3 2− and SO 3NHSO 3 2− under alkaline conditions. As indicated by DFT calculation, the weaker S–N bond and larger S–N–S angle facilitate the electrophilic attack under acid conditions. Furthermore, very unstable intermediates (FSO 2NH 2 and CH 3CH 2OSO 3H) are determined for the first time. Based on these hydrolysis mechanisms, strategies for inhibiting LiFSI hydrolysis are provided, which is significant for the high-efficiency production and safe storage/transportation of LiFSI.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Suo · Science · 2015 · 350 · 93810.1126/science.aab1595 ↗
2. Cai · J. Power Sources · 2022 · 53510.1016/j.jpowsour.2022.231481 ↗
3. Zhou · Adv. Mater. · 2020 · 32
4. Yu · ACS Mater. Lett. · 2020 · 2 · 142310.1021/acsmaterialslett.0c00339 ↗
5. Zhang · Matter · 2020 · 3 · 50910.1016/j.matt.2020.06.026 ↗
6. Escobar-Hernandez · J. Electrochem. Soc. · 2016 · 163 · A269110.1149/2.0921613jes ↗
7. Francis · J. Electrochem. Soc. · 2018 · 165 · A120410.1149/2.0281807jes ↗
8. Roeder · J. Power Sources · 2014 · 248 · 97810.1016/j.jpowsour.2013.09.146 ↗
9. Chen · Batteries Supercaps · 2019 · 2 · 12810.1002/batt.201800118 ↗
10. Wilken · Solid State Ionics · 2012 · 225 · 60810.1016/j.ssi.2012.02.004 ↗
11. Zhang · J. Power Sources · 2002 · 109 · 45810.1016/S0378-7753(02)00110-6 ↗
12. Elisabeth · J. Electrochem. Soc. · 2013 · 160 · A35610.1149/2.081302jes ↗
13. Zaghib · J. Power Sources · 2004 · 134 · 12410.1016/j.jpowsour.2004.02.020 ↗
14. Zhang · Electrochim. Acta · 2014 · 133 · 52910.1016/j.electacta.2014.04.099 ↗
15. Han · J. Power Sources · 2011 · 196 · 362310.1016/j.jpowsour.2010.12.040 ↗
16. Li · J. Electrochem. Soc. · 2010 · 158 · A7410.1149/1.3514705 ↗
17. Jiang · J. Energy Chem. · 2022 · 72 · 15810.1016/j.jechem.2022.05.005 ↗
18. Xu · Energy Environ. Sci. · 2014 · 7 · 51310.1039/C3EE40795K ↗
19. Philippe · J. Am. Chem. Soc. · 2013 · 135 · 982910.1021/ja403082s ↗
20. Kim · Pat. WO2020099527 · 2020 · A1
21. Okumura · Pat. CN101980955 · 2011 · B
22. Passerini · J. Fluor. Chem. · 2004 · 125 · 24310.1016/j.jfluchem.2003.07.003 ↗
23. Huang · J. Phys. Chem. C · 2010 · 114 · 2184010.1021/jp107740p ↗
24. Kerner · RSC Adv. · 2016 · 6 · 2332710.1039/C5RA25048J ↗
25. Pyschik · Electrochim. Acta · 2014 · 130 · 42610.1016/j.electacta.2014.03.033 ↗
26. David · Electrochim. Acta · 2019 · 321
27. Muzio · J. Electrochem. Soc. · 2021 · 16810.1149/1945-7111/ac2aca ↗
28. Shkrob · J. Phys. Chem. C · 2014 · 118 · 1966110.1021/jp506567p ↗
29. Rajendra · Pat. AU2013309495 · 2016 · B2
30. Budi · J. Phys. Chem. C · 2012 · 116 · 1978910.1021/jp304581g ↗
31. Kubota · Electrochem. Commun. · 2012 · 66 · 320
32. Payne · J. Am. Chem. Soc. · 2002 · 59 · 94710.1021/ja01284a506 ↗
33. Boschin · Electrochim. Acta · 2015 · 175 · 12410.1016/j.electacta.2015.03.228 ↗
34. Álvarez · J. Mol. Struct. · 2003 · 657 · 29110.1016/S0022-2860(03)00407-1 ↗
35. Ko · Electrochem. Commun. · 2020 · 11610.1016/j.elecom.2020.106764 ↗
36. Fujii · J. Phys. Chem. B · 2007 · 111 · 1282910.1021/jp074325e ↗
37. Yoshida · J. Am. Chem. Soc. · 2011 · 133 · 1312110.1021/ja203983r ↗
38. Zak · Z. Kristallogr. Z. Krist-Cryst. Mater. · 1998 · 213 · 21710.1524/zkri.1998.213.4.217 ↗
39. Beran · Polyhedron · 2006 · 25 · 129210.1016/j.poly.2005.09.017 ↗
40. Matsumoto · J. Phys. Chem. C · 2017 · 121 · 920910.1021/acs.jpcc.7b02296 ↗