Beware of cyclic voltammetry! Measurement artefact in accelerated stress test of fuel cell cathode revealed by operando X-ray diffraction
Source abstract
Abstract
Efficient screening of proton exchange membrane fuel cell (PEMFC) cathode catalysts long-term stability at the laboratory scale requires the use of accelerated stress tests (ASTs), mostly consisting in cathode potential cycling in the device operational range. However, AST protocols must be complemented with auxiliary in situ electrochemical characterization techniques, such as cyclic voltammetry, at least at the beginning and at the end of test. Supposedly non-destructive, such techniques are necessary to interpret the AST in terms of catalyst performance stability. Here, by combining operando X-ray diffraction, on-line inductively coupled plasma mass spectrometry (ICP-MS) and ex situ characterization techniques, we provide experimental evidence that the cyclic voltammetry experiment performed at the end of AST controls the increase of the coherent domain size monitored on the aged catalyst. We propose this process originates from coalescence of crystallites during low potential excursions of the cathode far below the operational range of the device. This study reveals a ‘measurement artefact’ in typical AST protocols, where the investigated state of the aged catalyst is largely impacted by the cyclic voltammetry measurement itself, without relevance of fuel cell device practical operation.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Challenges in applying highly active Pt-based nanostructured catalysts for oxygen reduction reactions to fuel cell vehicles10.1038/s41565-020-00824-w ↗
2. Abdel-Baset · 2017
3. Recent advances in catalyst accelerated stress tests for polymer electrolyte membrane fuel cells10.1149/2.0881807jes ↗
4. The impact of potential cycling on PEMFC durability10.1149/2.083308jes ↗
5. Recent developments in catalyst-related PEM fuel cell durability10.1016/j.coelec.2020.02.007 ↗
6. Electrocatalyst durability under simulated automotive drive cycles10.1149/1.2981858 ↗
7. Pourbaix · 1974
8. Towards a comprehensive understanding of platinum dissolution in acidic media10.1039/C3SC52411F ↗
9. Structure dependency of the atomic-scale mechanisms of platinum electro-oxidation and dissolution10.1038/s41929-020-0497-y ↗
10. Eliminating dissolution of platinum-based electrocatalysts at the atomic scale10.1038/s41563-020-0735-3 ↗
11. Particle size effect on platinum dissolution: practical considerations for fuel cells10.1021/acsami.0c02801 ↗
12. Electrochemical on-line ICP-MS in electrocatalysis Research10.1002/tcr.201800162 ↗
13. Evaluating electrocatalysts at relevant currents in a half-cell: the impact of Pt loading on oxygen reduction reaction10.1149/2.0911915jes ↗
14. Scientific aspects of polymer electrolyte fuel cell durability and degradation10.1021/cr050182l ↗
15. Review: durability and degradation issues of PEM fuel cell components10.1002/fuce.200700053 ↗
16. A review of PEM fuel cell durability: materials degradation, local heterogeneities of aging and possible mitigation strategies
17. X-ray transparent proton-exchange membrane fuel cell design for in situ wide and small angle scattering tomography10.1016/j.jpowsour.2019.226906 ↗
18. The effect of size on the oxygen electroreduction activity of mass-selected platinum nanoparticles10.1002/anie.201200586 ↗
19. Direct enumeration of the geometrical characteristics of clusters10.1016/S0965-9773(97)00168-2 ↗
20. Impact of intermittent operation on lifetime and performance of a PEM water electrolyzer10.1149/2.0421908jes ↗
21. Imaging heterogeneous electrocatalyst stability and decoupling degradation mechanisms in operating hydrogen fuel cells10.1021/acsenergylett.1c00718 ↗
22. Impact of accelerated stress tests on the cathodic catalytic layer in a proton exchange membrane (PEM) fuel cell studied by identical location scanning electron microscopy10.1021/acsaem.2c01790 ↗
23. Tracking the catalyst layer depth-dependent electrochemical degradation of a bimodal Pt/C fuel cell catalyst: a combined operando small- and wide-angle X-ray scattering study10.1021/acscatal.1c04365 ↗
24. Decoupling catalyst aggregation, ripening, and coalescence processes inside operating fuel cells10.1016/j.jpowsour.2021.230851 ↗
25. Impact of carbon N-doping and pyridinic-N content on the fuel cell performance and durability of carbon-supported Pt nanoparticle catalysts10.1021/acsami.2c00762 ↗
26. In-situ monitoring of particle growth at PEMFC cathode under accelerated cycling conditions10.1149/2.004206esl ↗
27. Electrochemical strain dynamics in noble metal nanocatalysts10.1021/jacs.1c06780 ↗
28. Particle size effect on platinum dissolution: considerations for accelerated stability testing of fuel cell catalysts10.1021/acscatal.0c00779 ↗
29. Enhancement of surface self-disfusion of platinum atoms by adsorbed hydrogen10.1038/18185 ↗
30. The sintering of supported metal catalysts. II. Comparison of sintering rates of supported Pt, Ir, and Rh catalysts in hydrogen and oxygen10.1016/0021-9517(78)90293-2 ↗
31. Defects do catalysis: CO monolayer oxidation and oxygen reduction reaction on hollow PtNi/C nanoparticles10.1021/acscatal.6b01106 ↗
32. Hydrogen-induced step-edge roughening of platinum electrode surfaces10.1021/acs.jpclett.9b02544 ↗
33. Accelerated stress tests of Pt/HSAC electrocatalysts: an identical-location transmission electron microscopy study on the influence of intermediate characterizations10.1007/s12678-013-0173-y ↗