Interface and grain boundary degradation in LSM-YSZ composite Solid Oxide Fuel Cell cathodes operated in humidified air
Source abstract
Abstract
Abstract The interfaces between the different phases and the associated triple phase boundaries (TPBs) in solid oxide fuel cell (SOFC) cathodes are critical for the oxygen reduction reaction, and their degradation impacts SOFC performance and durability. This work examines nanostructure degradation of composite LSM/YSZ cathodes induced by electrochemical operation in humidified air. Three commercial button cells operated in humidified air for various durations at 800 °C exhibited more severe performance degradation than the cell operated in dry air. Microscopy imaging reveals nanostructure degradation within the cathode active layer, especially in the regions nearest to the electrolyte. Newly formed Mn-enriched nano-precipitates accompanied by nano-voids initiate at the original TPBs and propagate along the LSM/YSZ interface. The abundance of the nano-precipitates at LSM/YSZ interfaces increases with operation time, and prolonged operation in humidified air further promotes the formation of the Mn-enriched precipitates along YSZ/YSZ grain boundaries. The formation mechanism of those precipitates and their influence on the cathode performance are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Chemical Looping and Thermochemical Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Evolution of the electrochemical interface in high-temperature fuel cells and electrolysers10.1038/nenergy.2015.14 ↗
2. Advanced anodes for high-temperature fuel cells10.1038/nmat1040 ↗
3. Layered oxygen-deficient double perovskite as an efficient and stable anode for direct hydrocarbon solid oxide fuel cells10.1038/nmat4166 ↗
4. Lowering the temperature of solid oxide fuel cells10.1126/science.1204090 ↗
5. Effects of impurities on the degradation and long-term stability for solid oxide fuel cells10.1016/j.jpowsour.2008.10.127 ↗
6. Electrochemically influenced cation inter-diffusion and Co3O4 formation on La0.6Sr0.4CoO3 infiltrated into SOFC cathodes10.1016/j.ssi.2015.05.026 ↗
7. Self-regenerating Co–Fe nanoparticles on perovskite oxides as a hydrocarbon fuel oxidation catalyst in solid oxide fuel cells10.1021/acs.chemmater.7b04569 ↗
8. Enhancing SOFC cathode performance by surface modification through infiltration10.1039/c3ee42926a ↗
9. Microstructure degradation of YSZ in Ni/YSZ anodes of SOFC operated in phosphine-containing fuels10.1016/j.ssi.2012.12.019 ↗
10. Stabilities and electrical conductivities of electrode materials for use in H2S-containing gases10.1007/s100080000142 ↗
11. Effect of humidity in air on performance and long-term durability of SOFCs10.1149/1.3459904 ↗
12. Effects of water on oxygen surface exchange and degradation of mixed conducting perovskites10.1016/j.jpowsour.2011.04.032 ↗
13. Influence of water vapor on long-term performance and accelerated degradation of solid oxide fuel cell cathodes10.1016/j.jpowsour.2010.08.014 ↗
14. YSZ cathode degradation induced by moisture: an impedance spectroscopy study10.1016/j.ssi.2011.02.019 ↗
15. The effect of humidity and oxygen partial pressure on LSM–YSZ cathode10.1002/fuce.201100021 ↗
16. Effect of cathode gas humidification on performance and durability of solid oxide fuel cells10.1016/j.ssi.2010.02.018 ↗
17. Hardy
18. Long-term stability of the oxygen exchange properties of (La,Sr)1-z(Co,Fe)O3-delta in dry and wet atmospheres10.1016/j.ssi.2010.01.006 ↗
19. Performance regeneration in lanthanum strontium manganite cathode during exposure to H2O and CO2 containing ambient air atmospheres10.2109/jcersj2.123.199 ↗
20. Microstructural studies on degradation of interface between LSM–YSZ cathode and YSZ electrolyte in SOFCs10.1016/j.ssi.2009.07.011 ↗
21. Degradation of solid oxide fuel cell cathodes accelerated at a high water vapor concentration10.1115/1.3117608 ↗
22. Influence of water vapor on long-term performance and accelerated degradation of solid oxide fuel cell cathodes10.1016/j.jpowsour.2010.08.014 ↗
23. Characterization of adsorbed water layers on Y2O3-doped ZrO210.1016/S0167-2738(01)00826-8 ↗
24. Water incorporation in tetragonal zirconia10.1111/j.1551-2916.2004.00746.x ↗
25. Correlation between microstructure and degradation in conductivity for cubic Y2O3-doped ZrO210.1016/j.ssi.2006.09.003 ↗
26. The effect of humidity and oxygen partial pressure on LSM–YSZ cathode10.1002/fuce.201100021 ↗
27. Factors governing oxygen reduction in solid oxide fuel cell cathodes10.1021/cr020724o ↗
28. Crystal defects of yttria stabilized zirconia in solid oxide fuel cells and their evolution upon cell operation10.1016/j.ssi.2011.11.008 ↗
29. Microstructural and chemical evolution near anode triple phase boundary in Ni/YSZ solid oxide fuel cells10.1016/j.ssi.2011.10.005 ↗
30. A. Barinov. In-situ study of operating SOFC LSM/YSZ cathodes under polarization by photoelectron microscopy10.1016/j.ssi.2008.02.033 ↗
31. In stability of materials in high temperature water vapor: SOFC applications
32. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗
33. Effect of humidity in air on performance and long-term durability of SOFCs10.1149/1.3459904 ↗
34. Long Term Performance Stability Tests of Ba-Fe-O Infiltrated LSM/YSZ solid oxide fuel cells under high steam and high current10.1149/07801.1003ecst ↗